8 January 2020 in IEEE Access
A new single event burnout (SEB) hardened AlGaN/GaN structure with a thin barrier interlayer (IL) is presented in this work. The proposed hardened structure is compared with the simulation results of the conventional structure. The comparative analysis demonstrates that the IL lifts the conduction band energy in buffer layer and a new quantum well is formed. The quantum well limits the electrons induced by heavy ion below the second channel into the first channel. Thus, better SEB performance is achieved compared with the conventional structure. Moreover, the breakdown characteristic of the new structure is significantly improved, while the output characteristic is slightly reduced. Under the condition that the two structures are irradiated vertically by heavy ion having the linear energy transfer (LET) value of 0.6 pC/μm, the SEB threshold voltage of the conventional structure is 280 V, while the hardened structure can achieve 375 V.
24 August 2020 in IEEE Transactions on Electron Devices
In this article, a method of single-event burnout (SEB) hardening at high linear energy transfer (LET) value range is proposed and investigated by the 2-D numerical simulations. The improved MOSFET using this method and the conventional MOSFET are analyzed and compared to evaluate the effectiveness of this method. Simulation results show that, compared with the conventional MOSFET, the improved MOSFET using this method can effectively and quickly reduce the internal high electric field, thereby reducing the temperature. Under the condition of a LET value of 0.5 pC/μm and a drain voltage of 1200 V, the maximum drain current is 0.168 A, and the maximum global device temperature is 1724 K, which is much lower than the melting down temperature of silicon carbide (SiC) (3100 K). The hardening method in this article can be applied to different breakdown voltages by adjusting structure parameters.
5 February 2018 in Applied Physics Letters
Several 0.97PbZrO3–0.03Ba(Mg1/3Nb2/3)O3 (0.97PZ–0.03BMN) ceramics were prepared via the columbite precursor method. Their microstructures and pressure-dependent ferroelectric and depolarization performances were then studied. The X-ray diffraction patterns of ground and fresh samples indicate that a main rhombohedral symmetry crystal structure is present in the bulk and that it sits alongside a trace quantity of an orthorhombic antiferroelectric phase that results from the effect of grinding on the surface. The remanent polarization (Pr) of the 0.97PZ–0.03BMN reached 32.4 μC/cm2 at 4.5 kV/mm and ambient pressure. In an in situ pressure-induced current measurement, more than 91% of the retained Pr of the pre-poled sample was released when the pressure was increased from 194 MPa to 238 MPa. That this pressure-driven depolarization should be attributed to the pressure-induced ferroelectric–antiferroelectric phase transition is supported by the emergence of double P–E loops at high hydrostatic pressures. Moreover, the 0.97PZ-0.03BMN ceramics exhibit no temperature-induced phase transitions and little related polarization loss up to 125 °C, which suggests that Pr has excellent thermal stability. The sharp depolarization behavior at low pressures and excellent temperature stability reveal that our 0.97PZ–0.03BMN ceramics exhibit superior performances in mechanical–electrical energy conversion applications.
31 January 2011 in Acta Materialia
4 July 2022 in IEEE Transactions on Device and Materials Reliability
A single-event burnout (SEB) reliability and hardening method for 1.7-kV 4H-SiC power VDMOSFET under high liner energy transfer (LET) value range is proposed and researched by the 2-D numerical simulation. Compared with the conventional VDMOSFET with N-type multi-buffer layers, the hardened VDMOSFET not only ensures that the forward conduction capability does not deteriorate, but also reduces the peak electric field under breakdown voltage from 3.62 MV/cm to 2.98 MV/cm. The advantage of the hardened structure is providing a hole leakage path and increasing the contact area between the source metal and the N+ source, eliminating the effect of electron-hole pairs generated by heavy ion strike on the device, thus improving the SEB performance significantly. In addition, this fabricating technology is compatible with the current technological processes. This hardened structure provides a great potential in aerospace application.