The capability of battery materials to deliver not only high lithium storage capacity, but also the ability to operate at high charge/discharge rates is an essential property for development of new batteries. In the present work, the influence on the charge/discharge rate behaviour of substoichiometric concentrations of phosphorus (P) in silicon (Si) nanoparticles was studied. The results revealed an increase in rate capability as a function of the P concentration between 0 and 5.2 at %, particularly during delithiation. The stoichiometry of the nanoparticles was found to strongly affect the formation of the Li 3.5 Si phase during lithiation. Cyclic stability experiments demonstrated an initial increase in capacity for the SiP x materials. Galvanostatic intermittent titration technique and electrochemical impedance spectroscopy demonstrated the increased lithium diffusivity with inclusion of P. Density functional theory and ab initio molecular dynamics were deployed to provide a rationale for the electrochemical behaviour of SiP x .
Lithium‐ion capacitors (LICs) represent promising high‐power energy storage devices, most commonly composed of a lithium‐ion intercalation anode (e. g., graphite or hard carbon), a supercapacitor activated carbon (AC) cathode, and an electrolyte with 1 M LiPF6 in carbonate solvents. LiPF6 is susceptible to hydrolysis, forming HF, which leads to challenges for disassembly and recycling, risks during hazardous events, and extensive energy consumption during production. Here, we report on the feasibility of replacing LiPF6 with the non‐hydrolysing salt LiFSI for use with AC electrodes. Based on voltage hold measurements in a half‐cell setup, good long‐term stability is achieved with an upper cut‐off voltage of 3.95 V vs. Li/Li+, potentially enabling cell voltages of ~3.8 V when combined with graphite or silicon‐based anodes (operating at ~0.1 V vs. Li/Li+) in LIC full cells. The lower cut‐off voltage was determined to be 2.15 V vs. Li/Li+. The systematic comparison of CV, leakage current analysis and capacity retention upon voltage hold highlights the importance of the latter method to provide a realistic assessment of the electrochemical stability window (ESW) of LiFSI on a commercial AC electrode. The morphological and surface‐chemical post‐mortem analysis of AC electrodes used with LiFSI revealed that the oxidation of the FSI anion, as evidenced by the presence of new S 2p and N 1s features in the XPS spectra, and an increasing number of oxygenated species on the AC were the main processes causing capacity fade at positive polarization.
Silicon (Si) materials for use in Lithium ion batteries (LIBs) are of continued interest to battery manufacturers. With an increasing number of commercially available Si materials, evaluating their performance becomes a challenge. Here, we use an empirical fitting function presented earlier to aid in the analysis of galvanostatic charge‐discharge data of commercial Si half‐cells with relatively high loading. We find that the fitting procedure is capable of detecting dynamic changes in the cell, such as reversible capacity fade of the Si electrode. This fading is found to be due to the highly lithiated Li2Si Li3.5Si phase and that the behaviour is strongly dependent on the potential of this phase. EIS reveals that the Si electrode is responsible for the reversible behaviour due to progressive loss of Li+ leading to increasing resistance. SEM/EDX and XPS characterization are also employed to determine the origin of the irreversible resistance growth on the Si electrodes.