The relationship between local microstructure and superconducting properties of commercially prepared YBa 2 Cu 3 O
7−
δ single-grain bulk superconductor was investigated. The small samples for magnetization measurements were taken from the beginning and end of the a -growth sector and the c -growth sector as well as from the beginning and end of a / a -growth sector boundary. The field dependence of the magnetic moment was measured at temperatures starting from liquid helium (4.2 K) to liquid nitrogen (77 K) using the commercial Magnetic Property Measurement System with a magnetic field of up to 7 and 18 T. The microstructure was analysed using polarised light optical microscopy and scanning electron microscopy. The quantitative microstructural data were determined using an image processing software package. Microstructure analysis was focused on the size and volume fraction of Y 2 BaCuO 5 particles as well as on the characterisation of subgrain structure. These measurements showed that not only inhomogeneous distribution of Y 2 BaCuO 5 particles had influence on the critical current density but it can also be significantly affected by the subgrain structure within the bulk or by local contamination of YBa 2 Cu 3 O
7−
δ from the seed during fabrication process. It was observed that the critical current density along the a / a -growth sector boundary could be substantially higher in comparison to the other parts of the bulk and this behaviour can be related to the subgrain structure in the sample.
1 February 2018 in IEEE Transactions on Applied Superconductivity
Several studies showed that the SmBa$_{2}$Cu$_{3}$O$_{7-\delta}$ (Sm123, SmBCO) achieve higher critical current density (J$_{c}$) and critical transition temperature (T$_{c}$) in comparison to the YBa$_{2}$Cu$_{3}$O$_{7-\delta}$. On the other hand, the high sensitivity of Sm/Ba substitution at the solidification on the temperature of solidification is caused by changes of Sm solubility in the Sm123, what can be an obstacle to fabrication of SmBCO single grains with homogenous superconducting properties. We prepared Sm123 single grain bulk superconductors with addition of 1 wt. % CeO$_{2}$ and BaO$_{2}$, fabricated via the top-seeded melt growth (TSMG) process in air applying the slow cooling time-temperature profile. Evaluation of a substitution effect was based on an analysis of local superconducting properties and also on the results of EDS analysis from different sample location.
9 November 2018 in IEEE Transactions on Applied Superconductivity
We prepared ${\mathrm{GdBa}}_{2}{\mathrm{Cu}}_{3}{\mathrm{O}}_{7-\delta}$ (Gd123, GdBCO) single-grain bulk with Ag addition via the top-seeded melt growth (TSMG) method. Peritectic temperatures of precursor powder mixture and pure Gd123 powder were tested by differential thermal analysis (DTA). The dependence of the volume fraction and the size of ${\mathrm{Gd}}_2{\mathrm{BaCuO}}_5$ (Gd211) particles on the distance from the seed was determined with the help of image processing of the micrographs taken by scanning electron microscope (SEM) from the polished a/c-section of the sample. The morphology of Ag particles was evaluated by the SEM image analysis. The substitution of Ag in Gd123 was characterized by the wavelength-dispersive spectrometry (WDS). The magnetic measurements of superconducting properties (critical current density $J_c$ at 77 K and critical temperature $T_c$ ) were carried out using a vibrating sample magnetometer. Magnetization measurements were per-formed on the specimens taken from several different locations of the same crystal plane and the value of the maximum middle critical temperature ( $T_{c,m}$ ) was determined as 92.6 K.
The thermal and oxidation resistance of elements found in the combustion boilers of power generation plants are some of the most important factors deciding their effectiveness. This paper shows the experimental results of the influence of NiCr-based material composition on the microstructure and phase changes occurring during the oxidation and corrosion process. NiCr alloy was modified by the addition of rhenium and aluminum oxide. Materials were densified using the spark plasma sintering method at a sintering temperature of 1050 °C. Oxidation tests conducted up to 1100 °C under synthetic airflow revealed the formation of a thin Cr2O3 layer protecting the material against in-depth oxidation. Results of electrochemical corrosion in a 0.5 M NaCl solution indicated a positive role of Re and Al2O3 addition, confirmed by low corrosion current density values in comparison to the other reference materials. According to the provided positive preliminary test results, we can conclude that a NiCr-Re-Al2O3 system in coating form was successfully obtained by the plasma spraying method.