Intan Fadhlina Mohamed

Intan Fadhlina Mohamed

Auto-generated profile, based on publicly available information

Intan Fadhlina Mohamed

Department of Mechanical and Manufacturing Engineering, Faculty of Engineering and Built Environment, Universiti Kebangsaan Malaysia, Bangi, Malaysia

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
30 July 2022 in Progress in Additive Manufacturing
Verified
Journal Article
Open access
PDF file
MBMinhalina Ahmad Buhairi
Minhalina Ahmad Buhairi
Farhana  Mohd FoudziFarhana Mohd Foudzi
Farhana Mohd Foudzi
FJFathin Iliana Jamhari
Fathin Iliana Jamhari
ASAbu Bakar Sulong
Abu Bakar Sulong
NRNabilah Afiqah Mohd radzuan
Nabilah Afiqah Mohd radzuan
M.S.H. Al-FurjanM.S.H. Al-Furjan
M.S.H. Al-Furjan
Various laser powder bed fusion (LPBF) process parameters must be considered as they can independently affect the properties of end-product. However, many studies simply examine one or two LPBF process parameters. Laser power, scan speed, scan spacing, and layer height are the four primary LPBF process parameters that contribute to volumetric energy density (VED) used in LPBF. VED is often used as an optimization metric for LPBF process parameters, because it takes all four major parameters into consideration. Thus, this paper focuses on the effect of VED on the morphology and properties of part, and also discusses on the interrelationship between all four parameters. Common range used for each parameter is 70–400 W for laser power, 70–1800 mm/s for scan speed, 50–140 µm for scan spacing, and 20–50 µm for layer height. It can be seen as the VED increased, the microstructure of as-built titanium alloy Ti6Al4V components exhibited smaller α’ martensite size and larger columnar β grain. High VED can also reduce porosity and defect formation, which will help in increasing part density. The lowest surface roughness reported for LPBF Ti6Al4V is 4.91 µm. Meanwhile, the maximum microhardness obtained is 443 HV and the highest tensile strength achieved is 1400 MPa. The VED used for studies that obtained these results are in the range of 55–65 J/mm3. Thus, it can be concluded that the most suitable VED for LPBF printing of Ti6Al4V is around 55–65 J/mm3.

17 November 2022 in Metals
Verified
Journal Article
Open access
PDF file
MAMOHAMMAD AZLAN ARIPIN
MOHAMMAD AZLAN ARIPIN
ZSZainuddin Sajuri
Zainuddin Sajuri
Nashrah Hani JamadonNashrah Hani Jamadon
Nashrah Hani Jamadon
ABAmir Hossein Baghdadi
Amir Hossein Baghdadi
JSJunaidi Syarif
Junaidi Syarif
AAAhmad Muhammad Aziz
Ahmad Muhammad Aziz
In this study, the effect of phase, microstructure, and porosity in Selective Laser Melting (SLM) on hardness, tensile, and fracture behavior of 17-4 PH was investigated. The increasing interest in SLM in producing complex parts has encouraged the industry to produce performance parts, such as martensitic 17-4 PH stainless steel. However, the microstructure and mechanical behavior of SLM 17-4PH is not fully understood by researchers. Understanding the microstructure profile is complex because it is driven by thermal history and porosity. Both elements vary, based on the build directions, further hindering researchers from fully understanding the mechanical properties. To fabricate specimens in three different building orientations (0°, 45°, and 90°), 17-4 powder was used. Two phases, namely, austenite and martensite, with 90° build direction, retained more austenite, due to the reheating process on a smaller base area. The optical microstructure revealed several elements that were distinct for SLM processing, including circular, columnar lath, wave melt pool, and porosity. Columnar lath was found to grow continuously across different melt pools. Hardness was found to be higher for 0° than for 90°, due to higher martensite content. Tensile strength was highest for 0°, at 958 MPa, higher than at 45° and 90° at 743 and 614 MPa, respectively. Porosity analysis validated that 90° had all three types of porosities and, specifically, the crescent type, which held un-melted powders. All types of porosities were found in fractography analysis.

27 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
DEDawod Mohamed Elabar
Dawod Mohamed Elabar
OIOsama Irfan
Osama Irfan
Improving the engineering properties of Al–7Si cast alloys (300 series) provides an attractive alternative to automotive and aircraft engine industries. The solubility limit of silicon (Si) in Al contributes to the precipitation of flake-shaped Si particles with sharp edges, which function as a stress riser and promote crack propagation during the eutectic phase while also weakening the protective layer’s durability. In this study, the impact of microstructure refinement of Al–7Si alloys by using cooling slope, thixoforming and the T6 heat treatment process on hardness and corrosion resistance behavior was investigated. Results showed that the microstructures of the as-cast alloy had a very coarse dendritic shape, whereas the dendritic transferred to the globular α-Al phase, and the Si particles were replaced into a lamellar- or acicular-like shape after the cooling slope and thixoforming process, respectively. The as-cast, cooling slope and thixoformed samples were subjected to the T6 heat treatment process, which enhanced the hardness to 79, 99 and 104 HV, respectively, due to Si particle refinement. The potentiodynamic test revealed that the corrosion rate dropped to 0.00790 and 0.00736 mmpy−1 in the heat-treated cooling slope and thixoforming samples. This finding can be attributed to the substantially refined Si particles and reduced eutectic phase area due to the smaller cathodic to anodic area ratio.

8 March 2019 in Metals
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
As-cast and semisolid casting using a cooling slope A356 alloy were processed by equal channel angular pressing (ECAP) for Si and grain refinement. The ECAP was conducted at room temperature in a mold, with a channel angle of 120°, and this resulted in a significant size reduction of grain and Si particles from 170.5 and 4.22 to 23.12 and 0.71 µm, respectively, after six passes of heat-treated cooling slope casting, using the ECAP process. The hardness increased with ECAP processing, from 61 HV, for the as-cast alloy, to 134 Hv, after six passes of heat-treated cooling slope casting. The corrosion resistance of the alloy improved, from 0.042 to 0.0012 mmy−1, after the ECAP process. In this work both the strength and corrosion resistance of the ECAPed A356 alloys were improved with the application of the cooling slope process than without (i.e., from the as-cast condition).

17 May 2022 in Metals
Verified
Journal Article
Open access
PDF file
MGMohamed Gebril
Mohamed Gebril
MOMohd Zaidi Omar
Mohd Zaidi Omar
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NONorinsan Kamil Othman
Norinsan Kamil Othman
OIOsama Irfan
Osama Irfan
A356 aluminium alloy is subjected to heat treatment and high-pressure torsion (HPT) processing to investigate the impact of the combined treatments on the alloy’s microstructure refinement, corrosion resistance and hardness. The high-pressure torsion process was performed at room temperature for 0.75 and 5 turns. Subjecting the A356 Al alloy to a heat treatment and subsequent HPT processing produced a more refined microstructure, which has the effect of enhancing the alloy hardness and corrosion resistance under fragmentation and the homogenous redistribution of the intermetallic compounds and the Si particles. The results of the treatment show that there is a marked increase in hardness when imposing a strain from 61 HV to 198 HV on the A356 Al alloy, which has been HPTed and heat-treated for five turns. The polarisation curves show that there is a considerable improvement in the corrosion resistance rate of the alloy from 0.043 mm·year−1 for the A356 Al alloy sample to 0.003 mm·year−1 after five turns of HPT. In this work, the microstructure refinement resulted in the improvement of both the mechanical strength and corrosion resistance of the aluminium 356 alloy after heat treatment in comparison to the untreated alloy.

30 September 2022 in Materials
Verified
Journal Article
Open access
PDF file
AAAfifah Md Ali
Afifah Md Ali
MOMohd Zaidi Omar
Mohd Zaidi Omar
MSMohd Shukor Salleh
Mohd Shukor Salleh
HHHanizam Hashim
Hanizam Hashim
IMIntan Fadhlina Mohamed
Intan Fadhlina Mohamed
NANur Farah Bazilah Wakhi Anuar
Nur Farah Bazilah Wakhi Anuar
Thixoforming is a promising method that offers several advantages over both liquid and solid processing. This process utilizes semi-solid behaviour and reduces macrosegregation, porosity and forming forces during the shaping process. Microstructural and mechanical characterization of 0.3, 0.5 and 1.0 wt% graphene nanoplatelet (GNP) reinforced A356 aluminium alloy composite fabricated by thixoforming was investigated. Stir casting was employed to fabricate feedstocks before they were thixoformed at 50% liquid. The microstructure was characterized and evaluated by field emission scanning electron microscopy with an energy dispersive X-ray detector and X-ray diffraction. Mechanical testing, such as microhardness and tensile testing, was also performed to estimate the mechanical properties of the composites. The incorporation of 0.3 wt.% GNPs in Al alloy increased by about 27% in ultimate tensile strength and 29% in hardness. The enhancement in tensile strength is primarily attributed to load transfer strengthening due to the uniform dispersion of these GNPs within the Al matrix, which promotes effective load transfer during tensile deformation, and GNPs’ wrinkled surface structure. Simultaneously, the addition of GNPs enhances the grain refinement effect of the Al alloy matrix, resulting in a grain size strengthening mechanism of the GNPs/Al composites. The results reveal that thixoformed composite microstructure consists of uniformly distributed GNPs, α-Al globules and fine fibrous Si particles. The composites’ grains were refined and equiaxed, and the mechanical properties were improved significantly. This study creates a new method for incorporating GNPs into Al alloy for high-performance composites.