Optical components based on metasurfaces (metalenses) offer an alternative methodology for microlens arrays. In particular, metalens arrays have the potential of being monolithically integrated with infrared focal plane arrays (IR FPAs) to increase the operating temperature and sensitivity of the latter. In this work, we demonstrate a type of transmissive metalens that focuses the incident light (λ = 3–5 μm) on the detector plane after propagating through the substrate, i.e., solid-immersion type of focusing. The metalens is fabricated by etching the backside of the detector substrate material (GaSb here), making this approach compatible with the architecture of back-illuminated FPAs. In addition, our designs work for all incident polarizations. We fabricate a 10 × 10 metalens array that proves the scalability of this approach for FPAs. In the future, these solid-immersion metalenses arrays will be monolithically integrated with IR FPAs.
The InAs/InAsSb (Gallium-free) type-II strained-layer superlattice (T2SLS) has emerged in the last decade as a viable infrared detector material with a continuously adjustable band gap capable of accommodating detector cutoff wavelengths ranging from 4 to 15 µm and beyond. When coupled with the unipolar barrier infrared detector architecture, the InAs/InAsSb T2SLS mid-wavelength infrared (MWIR) focal plane array (FPA) has demonstrated a significantly higher operating temperature than InSb FPA, a major incumbent technology. In this brief review paper, we describe the emergence of the InAs/InAsSb T2SLS infrared photodetector technology, point out its advantages and disadvantages, and survey its recent development.
We studied long and very long wavelength InAs/InAsSb superlattice barrier infrared detectors that contain p-type absorber layers in order to take advantage of the longer electron diffusion length for quantum efficiency (QE) enhancement. While they can achieve higher QE than devices that use only n-type absorbers, their dark current characteristics are affected by the presence of metallurgical and surface p–n junctions, and are best operated under lower biasing conditions where the tunneling dark currents are less pronounced. Rather than using a p-type absorber only, a barrier infrared detector structure with a combination of p- and n-type absorber sections can benefit from a shallower mesa etch that reduces fabrication demands and also decreases the p-type absorber exposed surface area. We compare four complementary barrier infrared detector structures that use an n-type absorber, a combination of p- and n-type absorbers, or a p-type absorber and briefly report results from a 13.3 μm cutoff focal plane array.
In the past decade, infrared detectors with InAs/InAsSb (Gallium-free) type-II strained layer superlattice absorbers became a technology of interest for many imaging applications. In this work, we study the dependence of minority carrier (hole) transport, absorption coefficient, and quantum efficiency (QE) of a 5.6 μm cutoff wavelength mid-wavelength infrared InAs/InAsSb detector on temperatures and applied bias. We found that the minority carrier lifetime is very long (τ ≈ 5.5 μs) and is temperature independent in the temperature range T = 50–150 K. The back-side illuminated QE without anti-reflection coating increases from ∼30% at T = 50 K to ∼60% at T = 180 K. The minority carrier (hole) diffusion length, Ldh, was found from QE and absorption coefficient. The hole diffusion length at T = 50 K is Ldh = 2.4 μm and increases monotonically to Ldh = 7.2 μm at T = 180 K. The hole mobility, calculated from diffusion length and minority carrier lifetime, is μh = 4.5 cm2/V s at T = 50 K and increases with temperature to reach μh = 7.2 cm2/V s at T = 150 K. In addition, we find that at lower temperatures where the diffusion length is shorter, the stronger QE dependence on applied bias is due to minority carrier collection from the depletion region, whose width increases with applied bias.
We demonstrated high-performance 8.9 μm cutoff wavelength nBn InAs/InAsSb type-II strained-layer superlattice (T2SL). These detectors exhibit a long minority carrier (hole) lifetime of 1.2 μs at 80 K, high quantum efficiency of 40% for back-side illuminated devices without antireflection coating, and low dark current density of 4.6 × 10−6 A/cm2 at 80 K. We measured absorption, minority carrier (hole) lifetime, quantum efficiency, and spectral response as a function of the temperature and applied bias. We investigated the temperature dependence of the hole diffusion length and mobility and found that their values increase with temperature from 1.3 μm and 6.5 cm2/Vs at 30 K to 6.5 μm and 36 cm2/Vs at T = 90 K. We compared the measured diffusion length and mobility of holes in long-wavelength infrared (LWIR) T2SL with these parameters of a high-performance mid-wavelength infrared (MWIR) T2SL. Unexpectedly, hole mobility in LWIR T2SL was found to be higher than in MWIR that is contrary to the theoretical predictions.
The net modal gain, optical loss, and transparency current of high-performance, narrow ridge waveguide interband cascade (IC) lasers have been measured using the Hakki–Paoli technique in the temperature range from T=78 to 270 K. In this temperature range, the optical loss of IC lasers increases from αw≈17 cm−1 at T=78 K to αw≈35 at T=270 K, the transparency current density rises from Itr=10 to 330 A∕cm2, and the differential gain decreases from gd≈2.2 cm∕A to gd≈0.06 cm∕A with a characteristic temperature of T0=130 K. The implications of these observed characteristics for IC lasers are discussed.