Mehmet Ünal

Mehmet Ünal

Auto-generated profile, based on publicly available information

Mehmet Ünal

Karabük Üniversitesi

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 July 2022 in Biointerphases
Verified
Journal Article
Closed access
PDF file
LELevent Elen
Levent Elen
YTYunus TUREN4
Yunus TUREN4
HAHayrettin AHLATCI
Hayrettin AHLATCI
MUMehmet Unal
Mehmet Unal
DEDeniz Ergin
Deniz Ergin
In this study, casting, extrusion, biocorrosion, and corrosive wear properties of 0.5 wt. % (Zn, Ca, and Nd) element added Mg—3 wt. % Ag alloys were investigated. According to the test results, it was observed that the grain refinement occurred with the effect of Zn and Ca element additions in the as-cast alloys and thus some mechanical properties of the alloys improved. Similarly, the extrusion process provided grain refinement and improved mechanical properties. As a result of in vitro corrosion tests, similar results were also obtained in the as-cast alloys, while this situation became more apparent in the extruded alloys and exhibited more homogeneous corrosion properties. In the corrosive wear tests, the wear rate of the extruded alloys generally showed a decreasing trend. However, both the as-cast and extruded Mg—3 wt. %Ag—0.5 wt. % Ca alloys exhibited the lowest wear rate.

26 August 2022 in Archives of Metallurgy and Materials
Verified
Journal Article
Closed access
LELevent Elen
Levent Elen
YTYunus TUREN4
Yunus TUREN4
HAHayrettin AHLATCI
Hayrettin AHLATCI
YSYavuz Sun
Yavuz Sun
MUMehmet Unal
Mehmet Unal
In this study, microstructure, mechanical, corrosion and corrosive wear properties of Mg-xAg the as-cast and extruded alloys (x: 1, 3 and 5 wt. % Ag) were investigated. According to the experimental results, as the amount of Ag added in the casting alloys increases, the secondary phases (Mg4Ag, Mg54Ag17) emerging in the structure have become more clarified. Furthermore, it was observed that as the amount of Ag increased, the grain size decreased and thus the mechanical properties of the alloys increased. Similarly, the extrusion process enabled the grains to be refined and the mechanical properties to be increased. As a result of the in vitro tests performed, the Mg-1Ag exhibited very bad corrosion properties compared to other alloys. On the other hand, according to corrosive wear tests results, a high wear rate and friction coefficient were found for Mg-5Ag alloys.

31 December 2022 in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
Verified
Journal Article
Open access
PDF file
MMMeriç Meti̇n
Meriç Meti̇n
MÜMehmet Ünal
Mehmet Ünal
HGHalil Ahmet GÖREN
Halil Ahmet GÖREN
Bu çalışmada C95200 ve C95300 alüminyum bronzlarının mikroyapı ve korozyon özelliklerinin incelenmesi amaçlanmıştır. C95200 ve C95300 alaşımları alüminyum bronz normlarında döküm olarak üretilmiştir. Üretilen alüminyum bronz ingotlarından mikroyapı ve korozyon numuneleri oluşturulmuştur. Optik mikroskop, SEM ve EDS araştırmaları yapıldı. Alaşımlara 72 saat %3,5 NaCl ortamında daldırma korozyon testi ve potansiyodinamik polarizasyon korozyon testi yapılmıştır. Mikroyapı incelemelerinde siyah bölgeler birincil α yapısını, tane sınırlarındaki beyaz bölgeler ikincil fazı (β) temsil etmektedir. Potansiyodinamik polarizasyon korozyon testinde C95200 alaşımının korozyon direncinin C95300 göre daha fazla olduğu tespit edilmiştir. Bu durum daldırma korozyon testinde de gözlemlenmiştir.

31 December 2021 in Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi
Verified
Journal Article
Closed access
PDF file
HGHalil Ahmet GÖREN
Halil Ahmet GÖREN
MÜMehmet Ünal
Mehmet Ünal
YTYunus TUREN4
Yunus TUREN4
HAHayrettin AHLATCI
Hayrettin AHLATCI
Bu çalışmada ZM21 Magnezyum (Mg) alaşımına La ve Ca ilavesinin döküm ve hadde sonrası mikroyapı, mekanik ve korozyon özellikleri incelenmiştir. Mikroyapı sonuçları incelendiğinde haddeleme sonrasında La ilaveli alaşımda taneler incelirken ikincil fazların bir miktar hadde yönünde uzadığı görülmüştür. Bundan farklı olarak Ca ilaveli alaşımda oluşan fazların haddeleme esnasında kırıldığı tespit edilmiştir. XRD sonuçlarına göre alaşımlarda MgZn, MgZn2, MgZn3, C5Zn3, Ca2Mg6Zn3, LaZn2, LaMg3 fazlarının oluştuğu görüldü. Daldırma korozyon özelliğine bakıldığında ZM21 Mg alaşımına kıyasla ZM21+0,5(La) Mg alaşımının hem döküm hem hadde olarak daha az ağırlık kaybı yaşanmıştır. Fakat döküm halinde ZM21+0,5(Ca) alaşımı daha düşük, haddelenmiş olarakta çok daha fazla ağırlık kaybı sergilemiştir.

27 September 2024 in Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science
Verified
Journal Article
Closed access
MMMeriç Metin
Meriç Metin
MÜMehmet Ünal
Mehmet Ünal
HGHalil Ahmet GÖREN
Halil Ahmet GÖREN
In this study, the microstructure, adhesive (dry) wear and corrosive wear properties of cast C95200 and C95300 aluminium bronze alloys were investigated. The most important difference for these two alloys is that C95200 alloy contains 8.67% Al and 2.51% Fe while C95300 alloy contains 10.10% Al and 0.93% Fe. Both alloys contain 0.11% Zn and trace amounts of Sn, Ni, Si, Pb. The equilibrium element that completes 100% of these two alloys is Cu. First, 99.9% pure copper was loaded into the graphite crucible of the induction furnace and the temperature was raised to 1155°C. Then 99.9% pure iron filings were added, waited for 30 min and the molten metal was gently stirred with a graphite propeller shaft. At 1140°C, 99.9% pure aluminium was added. A protective flux containing fluoride and chloride was used to cut off contact with the atmosphere. The melted alloys were poured without waiting into a permanent mould heated to 250°C. Microstructure, SEM (Scanning Electron Microscopes), EDS (Energy-dispersive X-ray spectroscopy), XRF (X-ray fluorescence), corrosive wear, adhesive (dry) wear test samples were prepared from the appropriate regions of these alloys. The corrosive wear test was carried out with a back and forth wear system in a salt water environment containing 3.5% by weight NaCl. In the corrosive wear test, at a distance of 1000 m, alloy C95200 lost 381.48% and 152.27% more weight than alloy C95300 under 10 and 20 N load, respectively, but lost 11.98% less weight under 40 N load. When the SEM and EDS results after corrosive wear were examined, it was observed that there were cracked bright parts on the surface of the C95300 alloy. When the Adhesive dry wear results under 10, 20, 40 N loads at 8000 m distance were examined, C95200 alloy lost 5.91% more weight than C95300 under 10 N load but lost 37.25%, 60.03% less weight under 20, 40 N load respectively.

4 March 2024 in Metallurgical Research & Technology
Verified
Journal Article
Closed access
PDF file
MÜMehmet Ünal
Mehmet Ünal
HGHalil Ahmet GÖREN
Halil Ahmet GÖREN
In this study, the effects of Nd, La, and Ca elements added to ZM21 alloy was investigated in terms of parameters such as microscopic, mechanical, and corrosion properties. The content of each of the elemental constituents was 0.5% by weight. The microstructural and mechanical behaviours of the investigated alloys were examined by XRD, EDX, SEM, OM, hardness surveys, tensile tests, and corrosion experiments. According to the XRD results, Ca5Zn3, Ca2Mg6Zn3, LaZn2, LaMg3, Mg41Nd5, and Mg12Nd phases emerged on the investigated alloys. The grain sizes of the alloys were refined by element addition and rolling process, thus increasing their mechanical properties. Ca increased the hardness of the ZM21 alloys, but this had a negative effect on the rolled specimens. The tensile value of ZM21 alloy as cast decreased by 39.702%, 48.080%, 45.678% with the addition of (0.5% La+0.5% Nd), (0.5% La+0.5% Ca), (0.5% La+0.5% Nd+0.5% Ca), respectively. The tensile value of ZM21 alloy with (0.5% La+0.5% Nd) addition increased by 58.302% as rolled. Tensile test could not be performed because the rolled alloys with 0.5% Ca addition were fragmented during rolling. Ca contributed positively to the corrosion behaviour of the casting ZM21 alloy, but it worsened it in the rolled alloys. White oxide areas on the surface of the rolled alloys indicated an increased degree of corrosion formation.