In this study, graphene nanoplatelets (GNPs) and boron carbide (B4C) nano reinforcements were incorporated to the pure magnesium (Mg). Powder metallurgy route was used to fabricate composite samples. Microstructures of specimens were examined and tensile, hardness, wear tests were performed to determine the mechanical and tribological performance of produced samples. The results indicate that the hardness was increased especially with the addition of 2% B4C and 0.5% GNPs reinforcements. A general trend was observed for the enhancements of yield and tensile strengths when nano reinforcements were added to the pure magnesium. The composite samples showed better wear resistance than the unreinforced sample. However, thermal conductivity began to decrease with the addition of B4C reinforcements. It is also observed that the porosity level was also higher for the composite samples.
Magnesium and its alloys have become important structural materials in the last couple of decades due to their exceptional and mechanical properties. In this study, the effects of the introduction Cd, Bi, and Sn alloying elements were introduced into AM60 alloys produced from Mg-Al-Mn triple junction in order to improve the microstructural and mechanical properties. The weight percent of the alloying elements was chosen as 0.5% wt. besides the introduction of the additional alloying elements, the effect of cooling rate on microstructural and mechanical properties of the alloys have been investigated. The results showed that the alloying elements introduced to AM60 resulted in an improvement in the mechanical properties of the alloys, which is attributed to the changes in the microstructure. The higher cooling rate led to the formation of the finer α-Mg master matrix which in turn enhanced the mechanical properties of the alloys. It was observed that the intermetallic phase of β-Mg17Al12 at the grain boundaries became thinner due to the rapid cooling rate and the introduction of the alloying elements, and the continuity decreased and the intergranular distance shortened. The addition of the alloying element increased the tensile strength of the AM60 alloy from 140 MPa to 210 MPa and the elongation values increased from 5% to 22%. The effects of the alloying elements and the cooling rate on the hardness and yields properties of the samples were also studied.
In this study, in vitro/vivo biocompatibility experiments of Mg-Al-Mn alloy were carried out, and AM50 and AM60 alloys were used in the experiments. Immersion and potentiodynamic corrosion have been applied to these alloys in vitro. For biocompatibility, cytotoxicity test was performed. A total of 40 rats were used for the in-vivo experiment. AM series alloys were surgically placed in the femoral condyle as mini screws and monitored radiographically. AM alloys were removed together with the femur at the end of 7 weeks and further examined. After in-vivo application, the biodegradability level was successfully concluded with blood mineral analysis and urinalysis. In this study, the bioprocess of AM series Mg alloys with Al and Mn additions has been completed. As a result, the AM alloys used can be classified as biocompatible and biodegradable materials. Graphical Abstract
In this study, it was aimed to investigate the effects of reinforcements used for improving the thermal properties of AA6061 alloy on wear resistance. For this purpose, composites were produced by pressure infiltration method using ceramic microparticles (TiB2 and B4C) and graphene nanoparticles (GNPs). The produced composites were first characterized by porosity measurement, XRD and SEM analysis. Then, the wear behavior of was examined under three different loads (20-40-60N) with the reciprocating ball on flat method in dry environment. Specific wear rates were calculated according to Archard principle by measuring the depth and width of the traces after tests with a profilometer. Wearing mechanisms were determined with the help of optical and microstructure images. According to the obtained results, it was found that B4C + GNPs reinforced samples were more resistant to abrasion at low loads, but TiB2 + GNPs reinforced samples were higher at higher loads.
26 August 2022 in Archives of Metallurgy and Materials
In this study, microstructure, mechanical, corrosion and corrosive wear properties of Mg-xAg the as-cast and extruded alloys (x: 1, 3 and 5 wt. % Ag) were investigated. According to the experimental results, as the amount of Ag added in the casting alloys increases, the secondary phases (Mg4Ag, Mg54Ag17) emerging in the structure have become more clarified. Furthermore, it was observed that as the amount of Ag increased, the grain size decreased and thus the mechanical properties of the alloys increased. Similarly, the extrusion process enabled the grains to be refined and the mechanical properties to be increased. As a result of the in vitro tests performed, the Mg-1Ag exhibited very bad corrosion properties compared to other alloys. On the other hand, according to corrosive wear tests results, a high wear rate and friction coefficient were found for Mg-5Ag alloys.
14 September 2016 in Science and Engineering of Composite Materials
In this study, the effect of Mg alloying addition (1–4 wt.%) on dry sliding wear behaviour of AA1050 matrix composites was investigated. Composites were produced by the pressure infiltration technique at 800°C and had a B 4 C particle volume fraction of 60%. Reinforcement particles were uniformly distributed in the aluminium matrix. Compared with the AA1050 matrix, the weight loss of the composites decreased with increasing Mg content. The wear rate of the composites increased when the applied load and sliding distance were increased. The results show that when the applied load reaches critical values (30 N), the weight loss increases significantly.