28 February 2024 in Journal of Welding and Joining
This study investigates a green laser welding on a nickel-coated copper-mild steel material used in an electric vehicle battery. The laser power and scan speed were varied, and through optical microscopy, it was demonstrated that excessive heat input led to increased weld penetration depth and bead width. Regarding defects, excessive heat input caused the formation of oxide, spatter on the bead surface, as well as porosity and cracks inside the weld penetration depth. The mechanical properties were evaluated through shear stress and microhardness measurements, indicating that as the heat input increased, the mechanical properties improved for the sample welded under the 2 kW condition. Considering the fire risk (occur at weld penetration depth over 50%) and joining aspects (start at weld penetration depth higher 20%), the optimal conditions were set as 1.6 kW and 300 mm/s. This optimized condition was set as the reference for monitoring. Based on the optimized condition, the results shown that an increase in heat input led to increased plasma and temperature signals, and an increase in scanning speed resulted in an increase in reflected light signal.
29 December 2025 in Science and Technology of Welding and Joining
Electric vehicles are gaining popularity as an effective alternative for reducing carbon dioxide emissions and achieving carbon neutrality. Welding copper (Cu) and aluminum (Al) is applied to electric vehicle batteries due to their high conductivity and lightweight properties. However, welding Cu and Al may lead to the formation of intermetallic compounds (IMCs) within the weld zone, which deteriorates mechanical properties. This study analyses the tendency for cracks to occur and the causes of crack formation by welding Al and Cu materials based on nickel (Ni) coating thicknesses (0, 7, 25, and 50 µm) using a green laser. Observations of cracks in the weld zone and the corresponding Ni content, performed using an optical microscope and an electron probe micro-analyser, revealed that increased Ni coating thickness led to higher Ni content in the weld zone and a corresponding decrease in crack occurrence. In addition, micro-structural analysis of the weld zone using a scanning electron microscope revealed that cracks began to occur with the formation of Cu-Al IMCs and propagated in regions where CuAl and CuAl 2 phases were present. The formation of the NiAl phase, due to the increased Ni content in the weld zone, inhibited the reaction between Cu and Al, thereby suppressing the formation of these brittle IMCs. Consequently, crack initiation and propagation were effectively reduced. A shear test was conducted to evaluate mechanical performance. The results showed that the shear strength of the weld with a Ni coating thickness of 25 µm improved by approximately 203% compared to the weld without Ni coating. The shear strength of the weld with a 50 µm Ni coating thickness decreased compared the 25 µm sample due to the non-uniform formation of equiaxed and columnar grain structures.
31 August 2026 in Journal of Welding and Joining
This study investigates the laser welding characteristics and mechanical properties of the Can-Cap butt joint in 600 mm ultra-large prismatic batteries, which are emerging as next-generation electric vehicle (EV) and energy storage system (ESS) platforms. To overcome the high reflectivity and thermal conductivity of aluminum alloys, a green laser with a wavelength of 515 nm was utilized to weld 0.7 mm thick Al3003-H14 sheets. The effects of welding patterns (straight and wobble) and scanning speeds on the weldability, cross-sectional defects, microstructural hardness, and tensile strength were experimentally evaluated. Precise joint alignment was achieved using the Auto Position Alignment (APA) function of the laser scanner. Optical microscopy of the etched cross-sections revealed that both patterns produced sound, fully penetrated weld beads free of internal porosity and hot cracks. Vickers hardness depth profiles indicated that the fusion zone (WZ) exhibited the highest hardness due to rapid-cooling-induced microstructure refinement, with the straight pattern showing higher hardness than the wobble pattern due to its faster cooling rate. Tensile testing demonstrated that the tensile strengths of the straight and wobble patterns reached 84.1% (138.8 MPa) and 77.1% (127.3 MPa) of the base metal, respectively. The straight pattern exhibited a 9.1% higher tensile strength compared to the wobble pattern, which is attributed to the narrower bead width, reduced heat-affected zone (HAZ), and higher joint hardness of the straight path. These experimental findings provide baseline datasets to validate computational fluid dynamics (CFD) melt pool simulations and advance intelligent laser autonomous manufacturing frameworks.