Rheological and relaxation properties of high-purity nanocrystalline beryllium are obtained at hot rolling temperatures. It is shown that full stress relaxation in nanocrystalline beryllium occurs...
Copper-based composite materials strengthened with nanosized fullerene soot particles were produced by mechanical milling and hot pressing technology with a content of carbon up to 5 wt. %. The microstructure of the composite powders and the compacts prepared using them were examined by light microscopy, SEM, EDS, XRD, and XPS; hardness, heat conductivity, and tribological characteristics were measured. The interesting feature of the observed microstructure was a “marble” pattern formed by a white boundary net. The study shows homogeneous distribution of carbon inside the copper grains and its lower concentration in the grain boundaries. The effect was caused by a reaction of carbon with oxygen adsorbed by the copper particles surface. The maximal hardness of the material is 160 HB for the sample with 0.5 wt. % of fullerene soot; this material has the minimal friction coefficient (0.12) and wear in a dry friction condition. Heat conductivity of the material (Cu-0.5 wt. % C) is 288 W/m*K.
Synthesis of the Nb-Si in-situ composite was attempted by mechanical alloying of element powders in vario-planetary ball mill. The particles size distribution was measured by laser diffraction, microstructures were examined with scanning electronic microscope, and the phase constituent were analyzed by X-ray diffraction. The amorphization of the Si during mechanical alloying, large amount of deformation of Nb crystal structure, and after all – the formation of supersaturated solid solution of Nb was observed. To stabilize microstructure and phase composition, a spark plasma sintering was attempted. After SPS microstructure consist of three main phases – Nbss, Nb5Si3 and Nb3Si.
1 March 2015 in Russian Journal of Applied Chemistry
Electrodeposition of tantalum coatings from molten salts onto nitinol substrates was studied in steady and pulsed modes. The adhesion of the tantalum coatings, their porosity, and the corrosion...
This paper investigated the influence of titanium carbide (TiC) content on the processing, microstructure, mechanical and tribological properties of Inconel 718/TiC composites produced by binder jetting additive manufacturing. It was found that increasing the amount of TiC required an increase of the drying intensity during printing due to a decrease in the thermal conductivity of the powder mixture. The sintering process also depended on the TiC content. The most optimal modes were 1270 °C for 10 h for samples with 0 and 3% TiC and 1280 °C for 5 h for samples with 5 and 10% TiC. The hardness of the materials increased as the proportion of reinforcement increased. The best tensile properties, also at high temperatures, were possessed by samples with 3% TiC, showing high strength and, in addition, satisfactory plasticity. The maximum wear resistance was achieved by the composite material containing 5% TiC.
In this paper, a novel approach to obtain a ferromagnetic material for smart applications was implied. A combination of mechanical alloying (MA) and plasma spheroidization (PS) was applied to produce Ni36Al27Co37 spherical powder. Then its structure was systematically studied. It was shown that homogenization of the structure occurs due to mechanism of layered structure formation. The dependence of the lamella thickness on the energy dose input at MA was defined. It was found that 14.7 W⋅h/g is sufficient to obtain lamella thickness of 1 μm and less. The low-energy mode of a planetary mill with rotation speeds of the main disk/bowl of 150/−300 rpm makes it possible to achieve a uniform element distribution upon a minimal amount of impurity. During MA in an attritor Ni3Al-type intermetallic compounds are formed that result in more intensive degradation in particle size. Plasma spheroidization of the powder after MA allowed obtaining Ni36Al27Co37 spherical powder. The powder had a fine β + γ-structure. The particle size distribution remains almost unchanged compared to the MA stage. Coercivity of the powder is 79 Oe. The powder obtained meets the requirements of selective laser melting technology, but also can be utilized as a functional filler in various magnetic composites.