Energy transfer between Tm3+ and Tb3+ dependent on the power density of pump laser was investigated in NaYF4: Tb3+,Tm3+,Yb3+ microcrystals. Under the excitation of a 976-nm near-infrared laser at various power densities, Tb3+-Tm3+-Yb3+ doped samples exhibited intense visible emissions with tunable color between green and blue. The ratio of blue and green emission were determined by energy transfer between Tm3+ and Tb3+. When the power density of pump laser was low, the energy transfer process from Tm3+ (3F4) to Tb3+ (7F0) occurred efficiently. Upconversion processes in Tm3+ were inhibited, only visible emissions from Tb3+ with green color were observed. When the power density increased, energy transfer from the 3F4 (Tm3+) to 7F0 level (Tb3+) was restrained and population on high energy levels of Tm3+ was increased. Contribution of upconversion emissions from Tm3+ gradually became dominant. The emission color was tuned from green to blue with increasing the power density. Energy transfer processes between low-lying levels of activators, such as Tm3+ will greatly reduce the population on certain levels for further high-order upconversion processes. The Tb3+-Tm3+-Yb3+ doped phosphors are promising materials for detecting the condition of power density of the invisible near-infrared laser.
Ultraviolet upconversion emissions from high energy levels (5D1, 5L8, 5L9,5G5, and 5L10) of Tb3+ were observed in the NaYF4:Tb3+, Yb3+ microcrystals under excitation of a 976 nm laser diode at room temperature. These energy levels were populated by energy transfer and excited state absorption processes. Power dependence measurements confirmed it was caused by a three-photon upconversion process. Concentration quenching did not strongly affect the population of these levels.
1 June 2017 in IEEE Journal of Quantum Electronics
The evolution Raman effect in a single-mode tellurite fiber (SMTF) was investigated by pumping a nanosecond laser operated at ~1545 nm. With the increase of the average pump power, inverse Raman scattering (IRS) effect was first observed in a 2.5-m-long SMTF, which induced a steadily growing second-order Raman Stokes that finally exceeded the first-order Raman Stokes. When the length of the SMTF was reduced to 0.5 m, no IRS effect was obtained due to the lower Raman gain.