1 October 2020 in IEEE Journal of Emerging and Selected Topics in Power Electronics
In this paper, pressureless sintering of nanosilver paste is proposed to enhance the reliability of wire-bonds with SiC chips by both alleviating thermo-mechanical stresses and enhancing thermal coupling of bonding wires and chips. A multichip 1200-V/300-A SiC hybrid module with six Si IGBTs and twelve SiC Schottky Barrier Diodes (SBDs) is demonstrated. The lifetime of the wire-bonds with the SiC SBD bonded by the pressureless sintered nanosilver is 27.9% longer than that by the high-temperature solder under the power cycling with the constant temperature swing. The lifetime of the wire-bonds with the IGBT also bonded by the pressureless sintered nanosilver is 46.2% longer than that by the high-temperature solder under the power cycling with the constant conduction current. Furthermore, not only the cost of 1700-V SiC SBDs is quite similar with that of 1200-V ones, but also the leakage current of the 1200-V/300-A SiC hybrid module can be reduced greatly using 1700-V SiC SBDs as free-wheeling diodes instead of regular 1200-V ones. Considering the much larger leakage current of a SiC SBD compared to that of a Si PiN diode. It is feasible to use a SiC SBD with the higher blocking voltage to reduce the significant leakage current of the free-wheeling SBD with almost no cost increase.
1 January 2026 in IEEE Journal of Emerging and Selected Topics in Power Electronics