In this Letter, the robust ferroelectric properties of low-temperature (350 °C) Hf0.5Zr0.5O2 (HZO) films are investigated. We demonstrate that the lower crystallization temperature of HZO films originates from a densified film deposition with an anhydrous H2O2 oxidant in the atomic layer deposition process. As a consequence of this densification, H2O2-based HZO films showed completely crystallinity with fewer defects at a lower annealing temperature of 350 °C. This reduction in the crystallization temperature additionally suppresses the oxidation of TiN electrodes, thereby improving device reliability. The low-temperature crystallization process produces an H2O2-based HZO capacitor with a high remanent polarization (Pr), reduced leakage current, high breakdown voltage, and better endurance. Furthermore, while an O3-based HZO capacitor requires wake-up cycling to achieve stable Pr, the H2O2-based HZO capacitor demonstrates a significantly reduced wake-up nature. Anhydrous H2O2 oxidant enables the fabrication of a more reliable ferroelectric HZO device using a low process thermal budget (350 °C).
16 August 2024 in ACS Applied Electronic Materials
A novel precursor, 1,1,1-tris(dimethylamino)disilane {TADS, [(H3C)2N]3Si2H3}, is used to deposit silicon dioxide (SiO2) films in a temperature range of 115–480 °C by thermal atomic layer deposition (tALD) and plasma-enhanced atomic layer deposition (PEALD) techniques. Compared to tris(dimethylamino)silane (TDMAS), the additional Si-Si bond in TADS is expected to enhance the reactivity of the molecule due to the polarization of the bond. In the tALD process, TADS gives a growth rate of 0.06 nm/cycle, which is approximately 20% higher than that of TDMAS, and an excellent conformality (>95% step coverage) in high aspect ratio nanotrenches (6:1). In the case of the PEALD process, TADS leads to not only a higher or at least comparable growth rates (0.11 nm/cycle), but also a higher bulk film density (∼2.38 g/cm3). As a result, the PEALD SiO2 films of TADS show a wet-etch rate down to 1.6 nm/min in 200:1 HF, which is comparable to that of the thermal oxide. Analyzed with Fourier-Transform Infrared (FTIR), the SiO2 films contain predominant Si−O bonds and a low level of Si−H and O−H bonds, consistent with the observed high wet-etch resistance. Furthermore, the PEALD SiO2 films deposited at 310 °C have at least 75% step coverage in high aspect ratio nanotrenches, suggesting that TADS is applicable for forming high-quality SiO2 films on both planar and patterned surfaces.