1 September 2020 in Journal of Manufacturing Processes
24 February 2023 in The International Journal of Advanced Manufacturing Technology
This work presents the evaluation of the interlayer temperature (IT) with travel speed (TS) combined effect for a given wire feed speed (WFS) on operational, geometrical, and metallurgical features of thin walls with the same width deposited by wire arc additive manufacturing (WAAM) with a low alloy steel, using or not active cooling. A preliminary experimental design was carried out to define a range of IT that could prevent the molten pool from running down and, then, be used in the main experimental design. The main tests were planned and performed to find different IT and TS combinations for a given WFS capable of depositing walls with the same target effective wall width. After selecting the parameters, six walls were deposited, three under natural cooling (NC) and three under near immersion active cooling (NIAC). A more significant temperature variability along the layer length (ΔT/ΔLL) is observed in increasing IT-TS combination and under NIAC. Regardless of the cooling approach, a worse surface aspect was observed with lower IT and TS. However, NC or NIAC do not affect the wall width (effective or external) or the layer height. On the other hand, they are affected by the IT with TS combination. A shorter production time was obtained on the walls with NIAC and higher IT-TS. No marked microstructural differences were observed comparing the walls, regardless of the cooling approach. However, microstructure tempering (hardness reduction) was observed in the walls deposited with NC using higher IT levels.
1 January 2021 in CIRP Journal of Manufacturing Science and Technology
12 September 2020 in The International Journal of Advanced Manufacturing Technology
Derivative welding processes are in many cases capable of altering phenomena that determine fundamental aspects of weld bead formation. Some of these evolutions act over the wire feed dynamics. However, in this scenario, the effects of the wire feed pulsation on the weld bead formation governing factors have not been fully explored yet. Therefore, this work aimed at examining how a wire feed pulsation approach affects the droplet transfer in gas metal arc welding and how its interaction with the molten pool defines the weld bead penetration. Bead-on-plate weldments were produced by varying the wire feed pulsation frequency, yet keeping the same levels of arc energy and wire feed speed, with the power source operating in constant voltage and current modes. To assess the droplet transfer behavior, high-speed imaging was used. The geometry of the weld beads was compared in terms of fusion penetration. The results showed that an increase in the wire feed pulsation frequency intensifies the detachment frequency of the droplets, being possible to accomplish a stable metal transfer with them straightly projected toward the weld pool, which contributed to a centralized-increased penetration profile. Based on a descriptive model, it was demonstrated that the increase in droplet momentum or kinetic energy, due to the wire feed pulsation, was not enough to justify the penetration enhancement. It was concluded that the wire feed dynamics can also stimulate surface tension variations in the weld pool and therefore disrupt the behavior of its mass and heat convection, supporting fusion penetration.
1 February 2021 in Journal of Manufacturing Processes