In this research, the production of carbon fiber composite (CFC) with epoxy resin was carried out for biomedical application. The surface of the carbon fibers was previously oxidized with concentrated nitric acid at a temperature of 100 °C for 30–120 min to create a rough surface impression on the carbon fibers to enhance interfacial bonding in the composite, increase surface area, and reduce surface tension. The carbon fiber/epoxy composite was fabricated using the vacuum assisted resin infusion method. Characterization of the oxidized carbon fibers and the composite products was performed using a digital microscope, scanning electron microscope, and Fourier Transform Infrared (FTIR) analysis. FTIR analysis results indicated that the carbon fiber oxidation process introduced new chemical functional groups, such as –CN and –CO groups. Mechanical characterizations included tensile testing of non-oxidized and oxidized carbon fiber and tensile testing of carbon fiber/epoxy composite. The results showed that the composite formed from oxidized carbon fibers/epoxy resin exhibited higher tensile strength compared to non-oxidized CFC. The longer the carbon fiber oxidation process, the higher the tensile strength values obtained.
Non-asbestos materials are developed to replace asbestos as brake pad due to the dangers to human health. Therefore, this study aimed to explore the development of hybrid reinforced polyester composites using natural fibers such as teak wood and water hyacinth for brake pad application. Natural fibers were prepared by drying, cutting, and filtering through a 30-mesh sieve. The quantity of polyester/catalyst resin was fixed at 30 g, while teak wood and water hyacinth fibers were varied (15, 10, and 5 g). Fillers and composites were investigated using Fourier transform infrared (FTIR) and composites were further analyzed through scanning electron microscopy-energy dispersive spectroscopy (SEM-EDS), thermogravimetric analysis-differential scanning calorimetry (TGA-DSC), hardness, and wear resistance testing. The results of FTIR spectra showed that a 5TW-15WH sample had the lowest lignin content, while surface morphology of composites was inhomogeneous with few voids and cracks. Based on EDS investigation, carbon (C) and oxygen (O) were the two most abundant elements, indicating lignin, cellulose, and hemicellulose as the main components in composites. TGA measurement showed that 15TW-5WH sample had lower weight loss compared to others. Increasing water hyacinth caused a significant improvement in material performance, with 5 g teak wood-15 g water hyacinth in the composite, showing the highest hardness at 71.2 Shore D and lowest wear rate of 5.373 × 10-6 mm2/kg.