Since bacteria remain in the dentin following caries removal, restorative materials with antibacterial properties are desirable to help maintaining the residual microorganisms inactive. The adhesive system Clearfil Protect Bond (PB) contains the antibacterial monomer 12-methacryloyloxydodecylpyridinium bromide (MDPB) in its primer, which has shown antimicrobial activity. However, its bactericidal effect against biofilm on the dentin has been little investigated. The aim of this study was to analyze by confocal laser scanning microscopy (CLSM) and viable bacteria counting (CFU) the MDPB bactericidal effect against S. mutans biofilm on the dentin surface. Bovine dentin surfaces were obtained and subjected to S. mutans biofilm formation in BHI broth supplemented with 1% (w/v) sucrose for 18 h. Samples were divided into three groups, according to the primer application (n=3): Clearfil Protect Bond (PB), Clearfil SE Bond, which does not contain MDPB, (SE) and saline (control group). After the biofilm formation, Live/ Dead stain was applied directly to the surface of each sample. Next, 10 µL of each primer were applied on the samples during 590 s for the real-time CLSM analysis. The experiment was conducted in triplicate. The primers and saline were also applied on the other dentin samples during 20, 90, 300 and 590 s (n=9 for each group and period evaluated) and the CFU were assessed by colonies counting. The results of the CLSM showed that with the Se application, although non-viable bacteria were detected at 20 s, there was no increase in their count during 590 s. In contrast, after the PB application there was a gradual increase of non-viable bacteria over 590 s. The quantitative analysis demonstrated a significant decrease of S. mutans CFU at 90 s PB exposure and only after 300 s of Se application. Protect Bond showed an earlier antibacterial effect than Se Bond.
The aim of this study was to assess the effect of different remineralizing agents on enamel microhardness (KHN) and surface topography after an erosive challenge. Forty-eight human enamel specimens (4 × 4 mm) were randomly assigned to 4 groups: control (no treatment), fluoride varnish, calcium nanophosphate paste and casein phosphopeptide-amorphous calcium phosphate paste (CPP-ACP). Both pastes were applied for 5 minutes, and fluoride varnish, for 24 h. Four daily erosive cycles of 5 minutes of immersion in a cola drink and 2 h in artificial saliva were conducted for 5 days. KHN readings were performed at baseline and after 5 days. The percentage of enamel hardness change (%KHN) was obtained after erosion. The surface topography was evaluated by atomic force microscopy (AFM). The data were tested using ANOVA, Tukey's and paired-T tests (p < 0.05). After an erosive challenge, there was no statistically significant difference between the control (96.8 ± 11.4 KHN / 72.4 ± 3.0 %KHN) and the varnish (91.7 ± 14.1 KHN / 73.4 ± 5.5 %KHN) groups. The nanophosphate group showed lower enamel hardness loss (187.2 ± 27.9 / 49.0 ± 7.9 %KHN), compared with the CPP-ACP group (141.8 ± 16.5 / 60.6 ± 4.0 %KHN), and both were statistically different from the varnish and the control groups. AFM images showed a rough surface for the control and the varnish groups, a non-homogeneous layer with globular irregularities for CPP-ACP, and a thick homogeneous layer for the nanophosphate group. None of the agents provided protection against the development of erosion; however, nanophosphate paste was able to reduce enamel surface softening after the erosive challenge
1 August 2019 in Journal of the Mechanical Behavior of Biomedical Materials