Dominik Steckermeier

Dominik Steckermeier

Auto-generated profile, based on publicly available information

Dominik Steckermeier

TU Braunschweig

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 June 2022 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
Julian MayerJulian Mayer
Julian Mayer
FHFabienne Huttner
Fabienne Huttner
CHCarina A. Heck
Carina A. Heck
DSDominik Steckermeier
Dominik Steckermeier
MHMax-Wolfram von Horstig
Max-Wolfram von Horstig
Arno KwadeArno Kwade
Arno Kwade
For batteries with high energy density and good fast-charge capability, NCM cathode active materials with ≥80 mol% nickel are promising due to their high specific capacities. Unfortunately, the increase in nickel content is accompanied by a high susceptibility to moisture. Therefore, nickel-rich NCM is coated or doped by the manufacturers to increase its stability. However, it is unclear if special requirements regarding ambient humidity must still be met during the whole production chain, or only after post-drying and during cell assembly. Therefore, the structure and properties of three different nickel-rich NCM active materials (one doped monocrystalline, two coated polycrystalline materials) processed at ambient atmosphere were investigated. At every process step, moisture content and microstructure were examined. Prior to cell assembly, two different post-drying procedures were applied and investigated. As validation, electrochemical tests were performed. Both polycrystalline cathodes demonstrated good physical and electrochemical properties, despite the ambient process atmosphere. Higher moisture reduction led to improved electrochemical performances at higher C-rates. Finally, a comparison between dry and normal atmosphere of the best performing material indicates that a production of high-quality nickel-rich electrodes at ambient atmosphere is possible if their exposure to moisture is short and well-designed post-drying techniques are applied.

1 April 2024 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
HFHans Fenske
Hans Fenske
TLTeo Lombardo
Teo Lombardo
JGJessica Gerstenberg
Jessica Gerstenberg
CKChristine Kern
Christine Kern
DSDominik Steckermeier
Dominik Steckermeier
Arno KwadeArno Kwade
Arno Kwade
Prelithiation is widely recognized as a promising technology to enable the use of high capacity anode active materials such as silicon. Numerous prelithiation techniques have been proposed over the years, with a handful successfully undergoing pilot scale testing. Nevertheless, new challenges arise when moving from optimizing single processes to integrating them into the process chain. A major concern is the stability of prelithiated electrodes against moisture. In this study, we investigate the influence of industrially-relevant moisture levels on the electrochemical performance of prelithiated graphite/SiOx composite anodes in 3-electrode half- and full-cells. We identify several indicators of electrode degradation such as an increase in open circuit potential, a decrease in graphite lithiation potential, and changes in specific charge/discharge capacity. The underlying degradation mechanisms are examined using electrochemical impedance spectroscopy, X-ray photoelectron spectroscopy, and time-of-flight secondary ion mass spectrometry, which show increased solid electrolyte interphase (SEI)-related interfacial resistances but no clear evidence of SEI degradation. Based on the experimental results, we define a process window for the stability of the investigated electrodes as a function of dew point and exposure time. Our results indicate an encouragingly high stability at dew points up to −40 °C for a realistic exposure time of 1 h.

22 December 2023 in ECS Meeting Abstracts
Verified
Journal Article
Closed access
DSDominik Steckermeier
Dominik Steckermeier
JGJessica Gerstenberg
Jessica Gerstenberg
EHElisa Hartmann
Elisa Hartmann
PMPeter Michalowski
Peter Michalowski
Arno KwadeArno Kwade
Arno Kwade
Among next-generation batteries, all-solid-state batteries (ASSB) promise increased energy densities, fast charging properties, and higher safety compared to traditional liquid-based systems. To achieve the demanded high energy densities high mass loadings of the composite cathodes are necessary. These consist of active material (AM), solid electrolyte (SE), and conductive additive as well as binder. Volume changes of intercalation AM and insufficient ionic percolation at low SE contents lead to an increased interfacial resistance and capacity loss. In order to promote cathode AM utilization the particle size ratio of the AM and the SE within the composite cathode needs to be optimized. Theoretical calculations have shown that for high AM utilization at high AM loadings particle size ratio is a crucial parameter [1, 2]. Experimentally, the influence of particle size ratio has so far only been studied at laboratory scale. However, scalable process routes have not considered this important aspect. In this work, we present a solvent-based process route for the preparation of sulfide-based solid-state composite cathodes with NCM622 as AM, starting from the adjustment of the particle size of a commercially available Li6PS5Cl SE by planetary ball mill. Further process steps include the dispersion of SE with AM and conductive additive and doctor blade coating of cathode films. We analyzed the composite cathodes with regard to their internal resistance as well as their microstructure and conducted electrochemical tests in lab-scale test cells. Optimization of the particle size ratio results in an increase of AM utilization by a factor of 5 as well as an enhanced AM-SE-particle contact area and lower porosity. References [1] Shi T, Tu Q, Tian Y, et al. High Active Material Loading in All‐Solid‐State Battery Electrode via Particle Size Optimization. Adv. Energy Mater. 2020; 10(1): 1902881 [https://doi.org/10.1002/aenm.201902881] [2] Bielefeld A, Weber DA, Janek J. Microstructural Modeling of Composite Cathodes for All-Solid-State Batteries. J. Phys. Chem. C 2019; 123(3): 1626–34 [https://doi.org/10.1021/acs.jpcc.8b11043]

22 December 2023 in ECS Meeting Abstracts
Verified
Journal Article
Closed access
HFHans Fenske
Hans Fenske
TLTeo Lombardo
Teo Lombardo
JGJessica Gerstenberg
Jessica Gerstenberg
DSDominik Steckermeier
Dominik Steckermeier
CKChristine Kern
Christine Kern
Arno KwadeArno Kwade
Arno Kwade
Prelithiation of Si containing anodes has commonly been acknowledged as a potential solution to the challenge of the high irreversible lithium losses that still hinder the widespread adoption of this next-generation anode active material. However, upscaling and implementation in the process chain remain major hurdles for most proposed prelithiation processes. A significant part of this comes down to the high reactivity of prelithiation agents and prelithiated electrodes towards moisture. In industrial scale electrode production, dry rooms with dew point controlled atmospheres are already in use, but are a significant cost factor. Therefore, the compatibility of prelithiated electrodes with dry room conditions is a major factor for the implementation of prelithiation into existing production lines. In this work C/SiOx composite anodes are electrochemically prelithiated and subsequently subjected to industry relevant moisture levels. The influence of dew point and exposure time is examined. After exposure, the anodes are assembled into half-cells and their electrochemical performance during the first lithiation/delithiation cycle is analysed using a 3-electrode setup. The evaluation of the specific capacities and the potential curves provides information about the extent of the damage to the electrode. The results indicate a promising stability window for dew points of up to -40° C and realistic exposure times of up to one hour. Additional aging investigations in full cells against NMC622-based cathodes confirm these findings. Furthermore, electrochemical impedance spectroscopy, XPS and ToF-SIMS measurements are performed to elucidate the effect of moisture exposure on the solid electrolyte interface (SEI) composition. The results suggest the development of a double-layered SEI structure, where the first layer forms during prelithiation and is altered by moisture exposure, while the second layer forms on top of the first layer during formation. Figure 1