The paper shows that the contour of a sheet blank at all stages of superplastic forming can be described by application of the universal equations known as a "superformula" and "superellipse". The work provides information on the ranges of values of the coefficients entering these equations and shows that their magnitudes make it possible to additionally determine the level of superplastic properties of the workpiece metal, the shape of the shell being manufactured, the stage of superplastic forming, and the presence of additional operations to regulate the flow of the deformable metal. The paper has the results of approximation by the proposed equations of shell contours that manufactured by superplastic forming by different methods.
This paper presents the results of experimental studies of load characteristic changes during the upsetting of high billets with the upsetting ratio (height to diameter ratio) from 3.0 to 6.0, which is followed by buckling. Such pass is an effective way of preforming the workpiece for production of forgings with a bended axis or dual forming, and belongs to impression-free (dieless) operation of bulk forming. Based on the experimental data analysis, an engineering method for calculation of workpiece pre-forming load as a maximum buckling force has been developed. The analysis of the obtained data confirmed the possibility of performing of this pre-forming operation on the main forging equipment, since the load of shaping by buckling does not exceed the load of the dieforging.
The article is devoted to superplastic forming of non-uniformly heated sheet blanks from aluminum alloy AMg6M. To create an uneven temperature field over the surface of the blank, coatings made of sublimated substances were used from at temperatures 50…150°C below the superplastic forming temperature (450°C for AMg6M alloy). An aqueous solute of chloride and ammonium iodide having a sublimation temperature at normal pressure and a latent heat of conversion equal to 338 and 404°C, 330 and 355kJ/kg, respectively, was sprayed onto the central zones of the blanks. Superplastic forming of shells was carried out in two modes: 1) with simultaneous sublimation of the coating; 2) with the beginning of the sublimation of the coating upon reaching the height, which is formed by the workpiece, equal to 20-30% of the final shell height. The experiments showed a decrease in the thickness of the shells to be formed up to 4-10% on the working surface of the shells (without taking into account their flange zones) and the savings of sublimate during superplastic forming in the second mode. The optimal subliming coating for AMg6M alloy was ammonium chloride.