1 November 2017 in Science and Technology of Welding and Joining
In recent years, interest has been increasing in application of Nickel alloys in the oil industry. For subsea engineering, the possibility to weld high-strength materials in an effective manner is essential. Friction Stir Welding (FSW) is alternative to join several materials retaining their properties or even improving them. This fact is relevant for Corrosion-Resistant Alloys (CRA) used in deep-water exploitation of hydrocarbons. Publications up to now have focused on FSW of Inconel® series as alloy 600, 625, and 718. To provide a solid basis for development, this review discusses the crucial points for FSW. The tool materials are described, as well as the joint microstructure and properties achieved. Furthermore, the basics of the corrosion resistance and the early corrosion studies of FSW joints are presented. It is concluded that FSW is a promising process for Ni alloys, but depends on upcoming research regarding tool technology and corrosion investigations.
1 April 2011 in Engineering Structures
19 September 2013 in Revista Brasileira de Ortopedia
LBLeonardo Carbonera Boschin
Leonardo Carbonera Boschin
RGRamiro Zilles Gonçalves
+1
Objetivo: O presente estudo faz uma análise dimensional dos diferentes acetábulos cimentados e não cimentados, nacionais e importados, disponíveis no mercado nacional para artroplastia total do quadril. Métodos: Foram considerados os acetábulos de 50 mm, destinados às cabeças femorais de 28 mm. As análises dimensionais foram feitas em um equipamento tridimensional robótico de medição por coordenadas. Avaliou-se a menor espessura do polietileno e suas medidas externas (diâmetro do espaço para a cabeça femoral e diâmetro máximo do acetábulo). Resultados: A espessura mínima do polietileno foi garantida em todos os componentes testados. A espessura dos acetábulos cimentados variou de 19,185 mm a 25,358 mm, enquanto a espessura dos acetábulos não cimentados variou de 12,451 mm a 19,232 mm A espessura foi em média 27,96% menor nos acetábulos não cimentados. Em relação à cavidade acetabular do polietileno que recebe a cabeça femoral, todos os diâmetros internos apresentaram pelo menos 28 mm. Em relação ao diâmetro externo máximo do polietileno, apenas um acetábulo cimentado atingiu os 50 mm de diâmetro. Conclusões: Observaram-se grandes diferenças nas medidas entre as marcas e os modelos analisados. Os acetábulos não cimentados têm uma espessura menor. Os diâmetros dos acetábulos não cimentados também foram menores do que os cimentados, à custa de sua necessidade de inserção no metal-back. Objective: This paper performs a dimensional analysis of different total hip arthroplasty polyethylenes, cemented and non-cemented, brazilian made and imported. Methods: It was considered acetabular components with 50 mm for the 28 mm femoral heads. Dimensional analysis were performed on a 3d coordinate Carl-Zeiss robotic device. Polyethylene thickness and its external measurements (maximum diameter and diameter for the femoral head) were measured. Results: The minimum thickness of the polyethylene was guaranteed on all tested components. The thickness of cemented acetabular varied from 19.185 mm to 25.358 mm, while the thickness of the non-cemented acetabular varied from 12.451 mm to 19.232 mm. The thickness was 27.96% lower in non-cemented acetabular components. With respect to the polyethylene acetabular cavity that receives the femoral head, all internal diameters exhibit at least 28 mm. In relation to the maximum outer diameter of the polyethylene, only one cemented acetabular component reached 50 mm in diameter. Conclusions: There are large differences in measurements between brands and models analyzed. Cementless acetabular components have the smaller thickness. The diameters of non-cemented acetabular were also lower than those cemented at the expense of their need to insert into the metal-back.