5 October 2020 in Applied Physics Letters
The electrical device characteristics of Ni/β-Ga2O3 vertical Schottky barrier diodes (SBDs) were measured in situ during the irradiation of 120 MeV Ag7+ swift heavy ions (SHIs). These devices exhibit SHI irradiation-induced degradation with 120 MeV Ag7+ ions in the ion fluence ranges of 1 × 1010 to 1 × 1012 ions/cm2. The height of the Schottky barrier is found to decrease from 1.11 to 0.93 eV, and the ideality factor increases from 1.16 to 2.06. These changes indicate the degradation of the device with SHI irradiation. A significant four orders increase is observed in the leakage current density from 4.04 × 10−8 to 1.98 × 10−4 A/cm2 at −1 V, and the series resistance also increases from 3.38 × 103 to 1.15 × 104 Ω. X-ray photoelectron spectroscopy measurements show that the Ga ions are present in divalent and trivalent states with the spectral features having the binding energies centered at 20.2 eV and 19.9 eV (Ga 3d core-levels) before and after ion irradiation. The O 2s peak shifts to 23.7 eV, and there is an increase in intensity and peak broadening due to the change in the trivalent to divalent state of Ga due to the irradiation. The O(I) peak appears at 530.7 eV in the pristine sample with the Ga–O bonding with the Ga3+ state in pure Ga2O3. Moreover, there is a significant change in the intensity and the peak width of O(II) centered at 533.0 eV after ion irradiation at the fluence of 1 × 1012 ions/cm2. This indicates that there is an increase in the surface adsorbed/lattice oxygen, resulting in GaO.
28 January 2020 in Journal of Nondestructive Evaluation
30 September 2022 in IEEE Transactions on Electron Devices
In situ ${I}$ – ${V}$ and ${C}$ – ${V}$ measurements were performed on Pt/PtOx/ $\beta $ -Ga2O3 vertical Schottky barrier diodes (SBD) during 120 MeV Au9+ swift heavy ion (SHI) irradiation in a fluence range of $1\times 10^{{10}}$ – $2\times 10^{{12}}$ ions/cm2. The reverse leakage current density increased from $1.21\times 10^{-{10}}$ to $1.69\times 10^{-{4}}$ A/cm2 at −1 V. The Schottky barrier height (SBH) remains close to ~1.8 eV up to the fluence of $5\times 10^{{11}}$ ions/cm2, and however, at the fluences of $1\times 10^{{12}}$ and $2\times 10^{{12}}$ ions/cm2, the SBH increased to 1.93 and 2.03 eV, respectively. Also, the ideality factor (IF) increased from 1.07 to 1.38. The in situ ${C}$ – ${V}$ measurements showed a similar trend, as the SBH decreased from 2.04 to ~1.88 eV until $5\times 10^{{11}}$ ions/cm2, but it increased to 2.14 and 2.56 eV at $1\times 10^{{12}}$ and $2\times 10^{{12}}$ ions/cm2, respectively. In addition, the doping concentration decreased from $1.01\times 10^{{16}}$ to $0.27\times 10^{{16}}$ cm $^{-{3}}$ as the defects increased significantly at the fluence of $2\times 10^{{12}}$ ions/cm2. The cathodoluminescence measurements revealed various Ga and O defects produced during SHI irradiation. Cross-sectional transmission electron microscopy measurements confirmed the formation of tracks within $\beta $ -Ga2O3 along the SHI path, and these results are explained with the inelastic thermal spike model.
11 May 2023 in IEEE Transactions on Electron Devices
In situ ${I} - {V}$ and ${C}\!\!-\!\!{V}$ measurements were performed during the 120 MeV Au $^{9+}$ ion irradiation on the Pt/Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 , metal–oxide–semiconductor capacitors (MOSCAPs), to comprehend the swift heavy ion (SHI)-induced effects at the interface and in the device performance. At a maximum fluence of $2\times 10^{{12}}$ ions/cm 2 , the ${I}-\!{V}$ data showed a rise in the reverse leakage current by four orders of magnitude compared to the pristine device. The trap level (below the conduction band of Al 2 O 3) from Poole–Frenkel emission exhibits a variation from $\sim $ 1.1 to 0.91 eV. The conduction band offset ${(\phi }_{B}{) }$ of Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 changes from 1.48 to 1.25 eV as estimated under the Fowler–Nordheim tunneling mechanism. In situ ${C}\!\!-\!\!{V}$ measurements show a significant shift in the flat band voltages and increased oxide in the border and interface due to charge trapping. The X-ray photoelectron spectroscopy (XPS) measurements of Al 2p and O 1s core levels revealed the pre-existing oxygen defects in Al 2 O 3 , which increase with fluence. The deconvoluted peaks of Al 2p at 74.6 eV designated to Al-sub oxide and the O 1s peak variation in the FWHM signifies the increase in the O defects. Cross-sectional transmission electron microscopy (XTEM) measurements on the irradiated device (at $2\times 10^{{12}}$ ions/cm $^{{2}}{)}$ revealed a modulated interface of Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 and the formation of an interlayer of $\sim $ 4 nm Al x Ga y O z . The scanning transmission electron microscope (STEM)-based high-angle annular dark-field imaging (HAADF) energy-dispersive X-ray spectroscopy (EDS) mapping revelation and the depth profiles of XPS data confirm the formation of an Al x Ga y O z interlayer.
20 August 2014 in International Journal of Speech Technology
1 October 2019 in Electronics Letters
In this Letter, the authors propose to apply the harmonic regeneration noise reduction (HRNR)‐based Wiener filter (W‐HRNR) to detect acoustic emission (AE) signal from the noisy environment. HRNR technique can regenerate the harmonics to overcome the distortion which occurs with overestimation of conventional Wiener filter and to preserve the essential signal content for accurate detection of AE signal. W‐HRNR is implemented in short‐time Fourier transform domain. Decision direct method is employed to estimate the spectral gain and signal‐to‐noise ratio (SNR) of the signal in each frame. Evaluation of the algorithm is carried out using peak‐SNR (PSNR) and mean square error (MSE). The performance of the proposed algorithm has been demonstrated using a simulated AE burst signal and AE signals acquired from compression test and drilling test. Results have proven the remarkable performance of W‐HRNR over existing conventional Wiener filter for AE with accurate detection by preserving the useful signal information even under high noise conditions at low frequencies. Moreover, W‐HRNR also achieved a significant improvement in PSNR and MSE over the conventional filter.