27 May 2019 in Applied Physics Letters
High performance gate stacks are critically needed for the development of β-Ga2O3 power transistors. Significant improvement in the performance of β-Ga2O3 gate stacks is demonstrated in this work by using SiO2 as an interlayer dielectric between Al2O3 and β-Ga2O3. The presence of SiO2 results in an 800× reduction in gate leakage current along with a 1.7× increase in the electric breakdown field. Additionally, the capacitance-voltage characteristics show an increase in flat band voltage (from 0.74 V to 3.25 V) that can enable normally off power transistors. The lowest interface trap density (Dit) of 5.1 × 1010 cm−2 eV−1 for the SiO2/β-Ga2O3 interface has been demonstrated through the use of a piranha clean before SiO2 deposition on β-Ga2O3 for the first time. Reduction (8×) in Dit, hysteresis (from 0.17 V to 0.05 V), and border trap density indicate substantial improvement in the quality of the β-Ga2O3/gate dielectric interface for the Al2O3/SiO2 bilayer stack as compared to only Al2O3.
22 December 2021 in Journal of Applied Physics
We demonstrate an metal–insulator–semiconductor (MIS) hetero-junction diode with as the high-k dielectric insulator for more efficient electric field management resulting in enhanced breakdown characteristics compared to a Schottky barrier diode. dielectric films were grown using atomic layer deposition and exhibited a high dielectric constant of 50. The high dielectric constant resulted in a lower electric field at the metal/dielectric interface in the MIS diode compared to the metal/ interface in the Schottky barrier diode. With good electron conduction in forward bias enabled by the negative conduction band offset of with respect to , the MIS design led to a improvement in the reverse blocking voltage with a slight trade-off in the specific on-resistance. Overall, a increase in the power figure of merit was observed (3.25 for the Schottky diode and 10.8 for the MIS diode). A detailed analysis of the energy band line-up and the forward and reverse current transport mechanisms are also presented using analytical modeling and 2D technology computer-aided design simulations.
11 May 2023 in IEEE Transactions on Electron Devices
In situ ${I} - {V}$ and ${C}\!\!-\!\!{V}$ measurements were performed during the 120 MeV Au $^{9+}$ ion irradiation on the Pt/Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 , metal–oxide–semiconductor capacitors (MOSCAPs), to comprehend the swift heavy ion (SHI)-induced effects at the interface and in the device performance. At a maximum fluence of $2\times 10^{{12}}$ ions/cm 2 , the ${I}-\!{V}$ data showed a rise in the reverse leakage current by four orders of magnitude compared to the pristine device. The trap level (below the conduction band of Al 2 O 3) from Poole–Frenkel emission exhibits a variation from $\sim $ 1.1 to 0.91 eV. The conduction band offset ${(\phi }_{B}{) }$ of Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 changes from 1.48 to 1.25 eV as estimated under the Fowler–Nordheim tunneling mechanism. In situ ${C}\!\!-\!\!{V}$ measurements show a significant shift in the flat band voltages and increased oxide in the border and interface due to charge trapping. The X-ray photoelectron spectroscopy (XPS) measurements of Al 2p and O 1s core levels revealed the pre-existing oxygen defects in Al 2 O 3 , which increase with fluence. The deconvoluted peaks of Al 2p at 74.6 eV designated to Al-sub oxide and the O 1s peak variation in the FWHM signifies the increase in the O defects. Cross-sectional transmission electron microscopy (XTEM) measurements on the irradiated device (at $2\times 10^{{12}}$ ions/cm $^{{2}}{)}$ revealed a modulated interface of Al $_{{2}}\text{O}_{{3}}/\beta $ -Ga 2 O 3 and the formation of an interlayer of $\sim $ 4 nm Al x Ga y O z . The scanning transmission electron microscope (STEM)-based high-angle annular dark-field imaging (HAADF) energy-dispersive X-ray spectroscopy (EDS) mapping revelation and the depth profiles of XPS data confirm the formation of an Al x Ga y O z interlayer.
26 October 2020 in Applied Physics Letters
β-Ga2O3 based enhancement mode transistor designs are critical for the realization of low loss, high efficiency next generation power devices with rudimentary driving circuits. A large positive flatband voltage (Vfb) of 10.6 V in β-Ga2O3 metal-oxide-semiconductor capacitors, with the ability to fine-tune it between 3.5 V and 10.6 V, using a polycrystalline AlN charge trap layer has been demonstrated. This can enable enhancement mode operation over a wide doping range. An excellent Vfb retention of 97% for 104 s at 55 °C was exhibited by the gate stacks after charge trapping, hence reducing the requirement of frequent charge injection cycles. In addition, low gate leakage current density (Jg) for high negative gate voltages (Vg −60 V) indicates the potential of this gate stack to enable superior breakdown characteristics in enhancement mode transistors.
20 February 2019 in IEEE Transactions on Electron Devices
Fin field-effect transistor (FinFET) scaling beyond the 10-nm node requires formation of a junction isolation region between the source and the drain to suppress sub-fin leakage current. In this paper, heavy species such as Sb and As were implanted at room temperature to form a punch-through stop (PTS) layer in n-Ge substrates. The impact of PTS implants on channel doping and defects, as well as junction leakage, was investigated for bulk Ge p-FinFET applications. We report retrograde doping profiles with a low surface (channel) dopant concentration of 4-5 × 10 16 cm -3 for Sb PTS implants post 550 °C and 650 °C activation anneals. Besides achieving low effective channel doping, the 650 °C high-temperature activation anneal post PTS implant also helps in the reduction of channel defect density. Furthermore, low junction leakage currents are also demonstrated for Sb and As PTS implants with 550 °C and 650 °C activation anneals. To avoid damaging the FinFET channel layer due to PTS ion implantation, Ge homoepitaxy was also studied post Sb PTS implants. However, Sb PTS implants activated at 650 °C without Ge epitaxy exhibit the best results in terms of low channel dopant and defect concentrations, besides junction leakage.
1 February 2021 in Journal of Applied Physics
Ternary dielectrics with varying composition formed by alloying two binary oxides can enable tunable optical and electrical properties for advanced technological applications. Atomic layer deposition (ALD) gives precise control over ternary dielectric composition through the ability to finely tune the precursor pulsing ratio. This work presents ALD development of Si-rich SixTi1−xO2 dielectrics with varying composition (x), along with spectroscopic and electrical characterization of their properties. Stoichiometry of the SixTi1−xO2 films was determined using X-ray photoelectron spectroscopy. Their composition-dependent refractive index, energy bandgap, and reflectance show promise for diverse optical applications ranging from anti-reflective coatings in photovoltaics to optical waveguides. This work also reports a first comparative study of SixTi1−xO2 films prepared by thermal (T-) and plasma-enhanced (PE-) ALD with varying Si composition and deposition temperatures. Deposition rates of 0.67–0.92 Å/cycle were obtained for SixTi1−xO2 films with x = 0.5–0.91 deposited using PE-ALD at 250 °C, which were higher than that of T-ALD at 200 °C (0.42–0.05 Å/cycle). PE-ALD also exhibited a high deposition rate of 0.81 Å/cycle for SixTi1−xO2 film with x = 0.91 at a low growth temperature of 150 °C. The PE-ALD Si-rich silica–titania films show substantially lower (100×) leakage current densities than the thermally deposited films, along with higher breakdown fields for decreasing deposition temperature. A dielectric constant as low as ∼5 was achieved for PE-ALD SixTi1−xO2 films with high Si (x = 0.91) content.