Viacheslav Kurlov

Viacheslav Kurlov

Auto-generated profile, based on publicly available information

Viacheslav Kurlov

Separate Structural Subdivision "Starobilsk Applied College of Volodymyr Dahl East Ukrainian National University

Research Focus & Metrics

Academic Career Length

4Years (2023-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
30 October 2024 in Eastern-European Journal of Enterprise Technologies
Verified
Journal Article
Open access
PDF file
APAnatolii Poliakov
Anatolii Poliakov
VVVadym Volokh
Vadym Volokh
AAAndrey Andreev
Andrey Andreev
VRVictor Rebenko
Victor Rebenko
VKViacheslav Kurlov
Viacheslav Kurlov
IKIryna Kovalenko
Iryna Kovalenko
The object of this study is the structural and phase transformations during the carbon reduction of tungsten high-speed steel slag in order to obtain a resource-saving alloying additive. The problem is the loss of precious elements when obtaining and using alloying material from man-made raw materials. Solving the problem is related to the definition of technological parameters to enable the reduction of losses of the corresponding elements. As a result of increasing the degree of scale reduction from 33 % to 72 % and 85 %, the strengthening of the manifestation of the solid solution of carbon and alloying elements in α-Fe relative to FeWO4, FeO and Fe3O4 was revealed. Fe3C, WC, W2C, FeW3C, Fe3W3C, Fe6W6C, VC, V2C, Cr3C2, Cr7C3 and Cr23C6 also appeared. Along with this, rounded and multifaceted particles with different chemical composition and the formation of a spongy microstructure were found. It was established that the most acceptable degree of recovery is 85 %. But achieving a recovery rate of 72 % is also sufficient. This is explained by the fact that the residual carbon in the carbides provides an increased reducing capacity, which is realized during the further reduction of oxides in the liquid metal during alloying. The spongy microstructure results in faster dissolution in contrast to standard ferroalloys, which provides a reduction in melting time while reducing spent resources. No phases with an increased tendency to sublimation were found in the obtained alloying material. That is, no additional conditions are needed that restrain the loss of alloying elements during evaporation with a gaseous phase, which provides an increase in the degree of extraction of the corresponding elements. The properties of the resulting alloying material make it possible to use it in metallurgical production when smelting alloyed steel grades in an electric arc furnace, the composition of which does not have strict restrictions on the carbon content

31 October 2023 in Eastern-European Journal of Enterprise Technologies
Verified
Journal Article
Open access
PDF file
VVVadym Volokh
Vadym Volokh
APAnatolii Poliakov
Anatolii Poliakov
VRVictor Rebenko
Victor Rebenko
AAAndrey Andreev
Andrey Andreev
MYMykhail Михайлович Yamshinskij
Mykhail Михайлович Yamshinskij
Dmytro Vyktorovych IvanchenkoDmytro Vyktorovych Ivanchenko
Dmytro Vyktorovych Ivanchenko
Peculiarities of phase and structural transformations during the carbon-thermal recovery of high-speed steel slag with the production of an alloying additive were investigated. This is necessary to determine the technological indicators that allow reducing the loss of high-value elements during the production and use of the alloying additive. A gradual change in the degree of scale reduction from 32 % to 69 % and 77 % led to an increase in the appearance of the solid solution of alloying elements and carbon in the α-Fe lattice with respect to FeWO4 and Fe3O4. Along with this, Fe3C, FeW3C, WC, VC, V2C, and Cr3C2 were manifested. At the same time, the formation of polyhedral and rounded particles of different chemical composition and the formation of a spongy microstructure was observed. It was determined that the most acceptable degree of recovery is 77 %. At the same time, the degree of reduction of 69 % is also sufficient since due to the residual carbon in the form of carbides, an increased reduction capacity is ensured with additional reduction of the oxide component in the liquid metal during alloying. The spongy microstructure provides relatively fast dissolution compared to standard ferroalloys, which causes a reduction in the total melting time while reducing the resources spent. No phases and compounds characterized by an increased tendency to sublimation were detected in the obtained alloying additive. That is, there is no need to provide additional conditions that prevent the loss of high-value elements during evaporation with the gas phase, which causes an increase in the degree of extraction of alloying elements. The indicators of the obtained alloying additive make it possible to melt alloyed steel in an electric arc furnace with respect to brands whose composition does not have strict restrictions on carbon, while replacing a part of standard ferroalloys.