This paper reports a study into the structural-phase composition of the doping alloy made by processing metallurgical anthropogenic waste involving reduction smelting. This is required for determining the technological parameters that ensure an increase in the level of extraction of target elements during the processing of anthropogenic waste and for the further use of the doping alloy. It was revealed that the phase composition of the doping alloy manifested a solid solution of the doping elements and carbon in α-Fe. Cementite Fe3C and silicides Fe5Si3, FeSi, and FeSi2 were also identified. In this case, the doping elements were more likely to act as substitution atoms. It has been determined that the microstructure of the alloy consisted of several phases of different shapes and contents of the basic doping elements. Sites with an elevated iron level of up to 95.87 % by weight in the composition could be represented by the solid solution phase of the doping elements and carbon in α-Fe. The sites with a relatively high (% by weight) content of carbon (0.83‒2.17) and doping elements ‒ W, up to 39.41; Mo, up to 26.17; V, to 31.42; Cr, to 9.15 ‒ were apparently of a carbide nature. The sites with a silicon content of 0.43‒0.76 % by weight likely included silicide compounds. The alloy's characteristics make it possible to smelt steel grades without strict carbon restrictions, replacing some of the standard ferroalloys. Neither phases nor compounds with a relatively high propensity for sublimation were identified in the material produced. Therefore, there is no need to provide conditions to prevent evaporation and loss in the gas phase of the doping elements. That could increase the degree of extraction of the doping elements
30 October 2024 in Eastern-European Journal of Enterprise Technologies
The object of this study is the structural and phase transformations during the carbon reduction of tungsten high-speed steel slag in order to obtain a resource-saving alloying additive. The problem is the loss of precious elements when obtaining and using alloying material from man-made raw materials. Solving the problem is related to the definition of technological parameters to enable the reduction of losses of the corresponding elements. As a result of increasing the degree of scale reduction from 33 % to 72 % and 85 %, the strengthening of the manifestation of the solid solution of carbon and alloying elements in α-Fe relative to FeWO4, FeO and Fe3O4 was revealed. Fe3C, WC, W2C, FeW3C, Fe3W3C, Fe6W6C, VC, V2C, Cr3C2, Cr7C3 and Cr23C6 also appeared. Along with this, rounded and multifaceted particles with different chemical composition and the formation of a spongy microstructure were found. It was established that the most acceptable degree of recovery is 85 %. But achieving a recovery rate of 72 % is also sufficient. This is explained by the fact that the residual carbon in the carbides provides an increased reducing capacity, which is realized during the further reduction of oxides in the liquid metal during alloying. The spongy microstructure results in faster dissolution in contrast to standard ferroalloys, which provides a reduction in melting time while reducing spent resources. No phases with an increased tendency to sublimation were found in the obtained alloying material. That is, no additional conditions are needed that restrain the loss of alloying elements during evaporation with a gaseous phase, which provides an increase in the degree of extraction of the corresponding elements. The properties of the resulting alloying material make it possible to use it in metallurgical production when smelting alloyed steel grades in an electric arc furnace, the composition of which does not have strict restrictions on the carbon content
31 October 2023 in Eastern-European Journal of Enterprise Technologies
Peculiarities of phase and structural transformations during the carbon-thermal recovery of high-speed steel slag with the production of an alloying additive were investigated. This is necessary to determine the technological indicators that allow reducing the loss of high-value elements during the production and use of the alloying additive. A gradual change in the degree of scale reduction from 32 % to 69 % and 77 % led to an increase in the appearance of the solid solution of alloying elements and carbon in the α-Fe lattice with respect to FeWO4 and Fe3O4. Along with this, Fe3C, FeW3C, WC, VC, V2C, and Cr3C2 were manifested. At the same time, the formation of polyhedral and rounded particles of different chemical composition and the formation of a spongy microstructure was observed. It was determined that the most acceptable degree of recovery is 77 %. At the same time, the degree of reduction of 69 % is also sufficient since due to the residual carbon in the form of carbides, an increased reduction capacity is ensured with additional reduction of the oxide component in the liquid metal during alloying. The spongy microstructure provides relatively fast dissolution compared to standard ferroalloys, which causes a reduction in the total melting time while reducing the resources spent. No phases and compounds characterized by an increased tendency to sublimation were detected in the obtained alloying additive. That is, there is no need to provide additional conditions that prevent the loss of high-value elements during evaporation with the gas phase, which causes an increase in the degree of extraction of alloying elements. The indicators of the obtained alloying additive make it possible to melt alloyed steel in an electric arc furnace with respect to brands whose composition does not have strict restrictions on carbon, while replacing a part of standard ferroalloys.
30 December 2022 in Eastern-European Journal of Enterprise Technologies
This paper reports a study into the features of the structural-phase composition of products from the carbon-thermal reduction of scale of high-speed steels that yields an alloying additive. This is necessary to determine the technological parameters that reduce the loss of target elements in the process of obtaining and using resource-saving alloying material. The study indicates that when the degree of scale reduction changed from 28 % to 67 % and 81 %, an increase in the manifestation of a solid solution of carbon and alloying elements in the α-Fe lattice was observed. At the same time, the intensity of the diffraction maxima of FeO and Fe3O4 decreased. In the reduced products, the presence of Fe3C, FeW3C, Fe3W3C, and WC was traced. With an increase in the degree of scale reduction from 28 % to 67 %, the disordered (of "loose" appearance) microstructure was replaced with the formed particles of round and multifaceted shape with different content of alloying elements. At the reduction stage of 81 %, the microstructure had a finely fibrous structure. Based on the suite of studies, the most acceptable degree of reduction of scale of high-speed steel, followed by the use of the obtained material as an alloying additive, is 81 %. At the same time, ensuring the degree of recovery at the level of 67 % would also suffice. This is due to the fact that residual carbon in the form of carbides provides an increased reducing ability and degree of assimilation of alloying elements with the restoration of the residual oxide component in the liquid metal during doping. Spongy microstructure contributes to faster dissolution, in relation to the corresponding standard ferroalloys. This ensures a reduction in the total smelting time and, as a result, a decrease in the energy consumed