The study of new metallic biomaterials for application in bone tissue repair has improved due to the increase in life expectancy and the aging of the world population. Titanium alloys are one of the main groups of biomaterials for these applications, and beta-type titanium alloys are more suitable for long-term bone implants. The objective of this work was to process and characterize a new Ti10Mo8Nb6Zr beta alloy. Alloy processing involves arc melting, heat treatment, and cold forging. The characterization techniques used in this study were X-ray fluorescence spectroscopy, X-ray diffraction, differential scanning calorimetry, optical microscopy, microhardness measurements, and pulse excitation technique. In vitro studies using adipose-derived stem cells (ADSC) were performed to evaluate the cytotoxicity and cell viability after 1, 4, and 7 days. The results showed that the main phase during the processing route was the beta phase. At the end of processing, the alloy showed beta phase, equiaxed grains with an average size of 228.7 µm, and low Young’s modulus (83 GPa). In vitro studies revealed non-cytotoxicity and superior cell viability compared to CP Ti. The addition of zirconium led to a decrease in the beta-transus temperature and Young’s modulus and improved the biocompatibility of the alloy. Therefore, the Ti10Mo8Nb6Zr alloy is a promising candidate for application in the biomedical field.
The development of titanium-β alloys for biomedical applications is associated with the addition of alloying elements or the use of processing techniques to obtain suitable bulk properties. The Ti25Ta25Nb3Sn alloy has been highlighted for its mechanical properties and biocompatibility. To further enhance the properties of titanium alloys for biomedical applications, equal channel angular pressing (ECAP) was used due to its capability of refining the microstructure of the alloy, leading to improved mechanical properties without significant changes in Young’s modulus. This study aims to evaluate the impact of ECAP on the microstructure of the Ti-25Sn-25Nb-3Nb alloy and investigate the correlation between the microstructure, mechanical properties, and corrosive behavior. Grain refinement was achieved after four ECAP passes, with an average grain diameter of 395 nm and a non-homogeneous structure, and microhardness was slightly increased from 193 to 212 HV after four ECAP passes. The thermomechanical aspects of the ECAP processing have led to the formation of a metastable α″ phase during the first two passes, while after four passes, the structure was composed only of the β phase. The corrosion resistance of the alloy was increased after four passes, presenting the best results in terms of the improvement of passivation corrosion density.
1 March 2022 in International Journal of Advances in Medical Biotechnology - IJAMB
As life expectancy increases, further research is needed to develop new materials for biomedical applications. Titanium and its alloys have great potential to be used for such a purpose due to their excellent bulk properties, such as mechanical strength. However, these properties are influenced by their microstructure which varies according to the processing method. Thus, this research aims to evaluate the influence of heat treatment on phase transformation and mechanical properties of Ti30Ta alloy which has been made in an arc melting furnace. The heat treatment has been carried out at 750ºC, 800º C and 850ºC for 12 hours, followed by water quenching. The β-transus temperature was determined by Differential Scanning Calorimetry and High Temperature X-ray diffraction. The phases and structure have been investigated through optical microscopy, scanning electron microscopy and X-ray diffraction. Microscopy images and X-ray diffraction analysis reveal the presence of martensitic phase α'' for the solution treated sample and both α'' and α' phases for recrystallized samples. Mechanical tests show an increase in mechanical strength for all samples after recrystallization and the highest value was observed for the sample treated at 750ºC, although there was an undesirable increase of 30 GPa in Young Modulus.