Cerium (Ce)-doped Ni0.5Cd0.5CexFe2−xO4 (0.0 ≤ x ≤ 0.20) was synthesized using the sol–gel auto-combustion method. X-ray diffraction (XRD) analysis revealed that all the samples retained spinel cubic crystal structure with space group Fd3m at 800 °C. Crystal structure parameters, such as lattice constant, average crystallite size, and X-ray density were estimated from the major XRD (311) peak. Bulk density and porosity were also calculated. The average crystallite size was estimated to be in the range of 20–24 nm. SEM images displayed agglomerated particles with a porous morphology. The dielectric constant () increased and the dielectric loss tangent (tan) decreased with rising Ce concentration. The hysteresis loop (M–H loop) was measured at room temperature using a vibrating-sample magnetometer (VSM), which showed a nonlinear decrease in magnetization and coercivity with increasing Ce concentration.
Nanoparticles where holmium was substituted with nickel-cadmium Ni0.5Cd0.5HoxFe2-xO4 (X = 0, 0.02, and 0.04) ferrites were synthesized through a sol-gel auto-combustion process to reveal their structural and physical properties. The synthesized nanoparticles were characterized using X-ray diffraction (XRD), a scanning electron microscope (SEM), Fourier transform infrared ray (FTIR) spectroscopy, and impedance spectroscopy techniques. XRD revealed the formation of the cubic crystal structure had a preferential orientation along (311). By including holmium, the lattice constant was reduced, while the average crystallite size was increased. SEM analysis revealed that the nanoparticles exhibited regular shapes, and the average grain size increased with the holmium content. FTIR spectroscopy determined that all the organic and inorganic materials had an absorption range of 400 to 4000 cm−1. The dielectric properties were measured between the frequency ranges of 1 kHz and 2 MHz. This shows that the tangent loss and the dielectric constant were raised when the concentration of holmium was increased.