Cementitious–glass composite bricks (CGCBs) with 3D-printed reinforcement structures made of PET-G could be an innovative production method that relies on recycling glass waste (78%) and PET-G (8%). These bricks offer a promising solution for the construction industry, which has a significant impact on climate change due to its greenhouse gas emissions and extensive use of natural aggregates. The approach presented in this article serves as an alternative to using conventional building materials that are not only costlier but also less environmentally friendly. The conducted research included mechanical tests using digital image correlation (DIC), utilized for measuring deformations in specimens subjected to three-point bending and compression tests, as well as thermal investigations covering measurements of their thermal conductivity, thermal diffusivity, and specific heat. The results highlighted the superior thermal properties of the CGCBs with PET-G reinforcements compared to traditional cementitious–glass mortar (CGM). The CGCBs exhibited a 12% lower thermal conductivity and a 17% lower specific heat. Additionally, the use of specially designed reinforcement substantially enhanced the mechanical properties of the bricks. There was a remarkable 72% increase in flexural strength in the vertical direction and a 32% increase in the horizontal direction.
This study investigates an eco-friendly rapid-setting concrete developed for emergency repair and accelerated post-disaster reconstruction. The proposed material concept combines a low-emission multicomponent cement, CEM V/A (S-V) 42.5 N-LH/HSR/NA, with a hybrid aggregate skeleton composed of crushed granite and waste soda–lime glass, as well as a waste-derived silicate additive system based on aqueous sodium silicate, glass dust and glass powder. One reference mixture (R) and five modified mixtures (M1–M5) were designed to assess the effects of partial replacement of natural aggregate by glass aggregate and of the dosage of the silicate-based additive system on concrete performance. The experimental programme included setting time, compressive strength, splitting tensile strength, water absorption, freeze–thaw resistance and microstructural observations. Among the modified concretes, the mixture containing 5 vol.% glass aggregate (M1) showed the most favourable mechanical performance after 28 days, reaching a compressive strength of 95.1 ± 2.4 MPa and a splitting tensile strength of 4.82 ± 0.29 MPa, compared with 45.5 ± 0.8 MPa and 2.18 ± 0.11 MPa, respectively, for the reference concrete. Higher glass contents reduced strength relative to M1, but the modified mixtures still maintained satisfactory performance. The silicate-based system significantly affected setting behaviour; in mixture M5, the initial and final setting times were reduced from 380 ± 5 min and 497 ± 5 min to 213 ± 5 min and 307 ± 5 min, respectively. The results show that the combined use of CEM V cement, waste glass and silicate-based waste-derived additives can produce concretes with rapid-setting, high strength and satisfactory durability-related properties. The developed material may therefore be considered a promising solution for selected rapid-repair and reconstruction applications, particularly in lightly reinforced or unreinforced concrete elements requiring fast restoration of functionality.
This study evaluated the potential use of waste mineral wool recovered from heating pipe insulation as a functional additive in cement concrete. The research aimed to determine the effect of this fibrous recycled material on the mechanical, physical, durability, thermal, and microstructural properties of concrete. One reference mix and three modified mixes were prepared, incorporating waste mineral wool at 12%, 16%, and 20% by cement mass. All mixes were prepared using CEM I 32.5R cement, 0/2 mm basalt aggregate, 2/8 mm granite aggregate, and a superplasticizer. After 28 days of sample curing, compressive strength, splitting tensile strength, density, water absorption, frost resistance, and thermal parameters were determined. Microstructural observations were also performed on concrete fracture surfaces. The results showed that the addition of mineral wool reduced the compressive strength from 84.9 MPa for the reference concrete to 63.8–53.3 MPa for the modified concretes. At the same time, moderate dosing improved the splitting tensile strength, reaching a maximum of 3.93 MPa with a 16% addition. The most favorable thermal effect was achieved with a 12% addition, for which the thermal conductivity coefficient decreased from 1.3461 to 1.1988 W/(m·K). The results indicate that waste mineral wool can be used in concretes with limited structural function; however, its dosage requires optimization due to increased water absorption and decreased compressive strength.