Carbon-based porous materials (CPM) have recently received attention due to their many applications. In this context, this work focused on the development of a simple synthesis method to produce highly porous carbon materials, by applying commercial sugar as carbon source, pyrolyzed silica (as template) and deionized water. The synthesis of the CPMs consisted of: (i) Gel formation: by mixing the raw materials in a mechanical stirrer, wherein the mass ratio sugar/template (S/T) was evaluated (1.8 and 2.7) as well as the deionized water volume (150 and 250 mL); (ii) Carbonization: the gels were carbonized under N2 inert atmosphere at a heating rate of 10oC min-1 and a temperature of 700oC for 1 h; (iii) Template leaching: the silica was removed by washing with NaOH 2.0 mol L-1 or HF 99.9% solution. In order to evaluate the potential and characteristics of the CPMs, a morphological, textural and chemical characterization was carried out through N2 and CO2 physisorption, Raman spectroscopy, X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FT-IR). The N2 physisorption analyses evidenced the synthesis of a highly porous material after the removal of the template, C1-I (NaOH leaching) showed a specific surface area of 462 m2g-1 and a micropore area of 610 m2g-1 , elevated pore volume (1.04 cm3g-1), wherein micropores (0.21 cm3g-1) and mesopores (0.83 cm3g-1) were identified - most interesting values for the best CPM amongst the studied conditions. An average diameter value of ultramicroporous and supermicroporous (2.9Å) was also identified by CO2 physisorption. The XRD diffractograms and Raman analyses indicated the formation of semi-crystalline structure in the CPM, with large domains of graphite and graphene sheets in a random pattern (turbostratic). By the FT-IR analysis it was possible to determine that the carbonized samples underwent partial oxidation and to identify the presence of bonds and vibrations of the aromatic skeleton (νOHνC-HνC=C). Overall, the characterization of the CPMs, produced from simple raw materials, have demonstrated great potential of this synthesis method for highly porous carbonaceous materials.
The growing demand for environmentally friendly materials has driven extensive research into biopolymer-based nanocomposites with enhanced functional performance. Chitosan, a naturally derived polysaccharide, offers excellent film-forming ability, biodegradability, and antimicrobial potential, making it a promising matrix for sustainable packaging and coating applications. In this study, a distinctive solvent-casting strategy was employed to fabricate chitosan-based nanocomposite films functionalized with dual-action silver/titania (Ag/TiO2) nanoparticles, combining both photocatalytic and metallic antimicrobial mechanisms—an approach that provides broader functionality than conventional single-component fillers. The biodegradable films were systematically characterized for their structural, mechanical, optical, and barrier properties, as well as their antimicrobial performance. The integration of Ag/TiO2 imparted unique synergistic effects, modifying film morphology and color, slightly reducing tensile strength, and enhancing hydrophobicity and structural compactness. The obtained water vapor permeability values (0.013–0.102 g·mm·m−2·h−1·kPa−1) classified the materials as moderate barriers, comparable to or better than many existing chitosan-based systems without nanofiller reinforcement. Notably, films containing 10 wt% Ag/TiO2 achieved a 40.4% reduction in Escherichia coli viability and an 8.2% inhibition of Staphylococcus aureus, demonstrating concentration-dependent antimicrobial activity superior to that of neat chitosan films. Overall, the unique combination of a biodegradable chitosan matrix with multifunctional Ag/TiO2 nanofillers offers clear advantages over traditional biopolymer films, highlighting their potential as advanced materials for active food packaging and antimicrobial surface coatings.
Among the countless routes for renewable hydrogen (H2) production, Biogas Dry Reforming (DR) has been highlighted as one of the most promising for the circular bio-economy sector. However, DR requires high operating temperatures (700 °C–900 °C), and, for greater efficiency, a thermally stable catalyst is necessary, being, above all, resistant to coke formation, sintering, and sulfur poisoning. Mesoporous metallic catalysts, such as nickel (Ni) supported on silica, stand out due to their high catalytic activity concerning such characteristics. In this regard, the presented work evaluated the influences of the nickel addition stage during the synthesis of mesoporous catalyst type Si-MCM-41. Two different catalysts were prepared: catalyst A (Ni/Si-MCM-41_A), synthesized through the in situ addition of the precursor salt of nickel (Ni(Ni(NO3)2·6H2O) before the addition of TEOS (Tetraethyl orthosilicate) and after the addition of the directing agent; and catalyst B (Ni/Si-MCM-41_B), resulting from the addition of the precursor salt after the TEOS, following the conventional methodology, by wet impregnation in situ. The results evidenced that the metal addition stage has a direct influence on the mesoporous structure. However, no significant influence was observed on the efficiency concerning BDR, and the conversions into H2 were 97% and 96% for the Ni/SiMCM-41_A and Ni/Si-MCM-41_B catalysts, respectively.
In this work, graphene quantum dots (GQDs) were synthesized from Moringa oleifera seed biomass doped with phosphorus, using a low-cost, renewable hydrothermal method. The biomass was ground and sieved (30 mesh), and the classified powder was transferred to a Teflon capsule, placed in a stainless-steel reactor (210 ºC, 24 h). Afterwards, 20 mL of distilled water were added to the synthesized GQDs, stirred for 30 min, and filtered through Whatman filter paper. Then they were centrifuged (12000 rpm, 10 min) and filtered through a 0.22 μm membrane. The filtrate was dialyzed in a cellulose dialysis bag, with a cut-off size of 3.5 kDa, for 7 days in absolute ethanol (99.5%), with gentle stirring, and the dialysate was exchanged every 24 h. The dialysate was dried at 105 ºC for 24 h. The GQDs were characterized by X-ray energy dispersive spectroscopy (EDX), Fourier-transform infrared spectroscopy (FTIR), UV-vis electronic absorption, fluorescence emission, X-ray Diffraction and high-resolution transmission electron microscopy (HRTEM). The results show the GQDs with an average size of 18.63 ± 4.24 nm and high fluorescence (bright blue) under ultraviolet light (365 nm). Our GQDs are promising for application in bioimaging and bioanalysis.
Chitosan is a biopolymer with a wide range of applications. It typically requires depolymerization to achieve a desired molecular weight for specific uses. This study investigated the potential for depolymerizing chitosan by thermal shock and grinding to produce nanochitosan. A series of thermal shock cycles combined with grinding were performed to assess the influence of drying temperature, residence time, and number of thermal cycles on the molecular weight, particle size, and crystallinity of chitosan. The thermal shock reduced the molecular weight and particle size of chitosan within the first hour of treatment, with optimal conditions achieved at a drying temperature of 90 °C and residence time inside the oven of 5 min. These conditions resulted in a molecular weight of 15.0 kDa with an average diameter of 136 nm. Thermal shock can be considered an effective method for chitosan depolymerization with grinding serving to standardize the particle size. This optimized process offers promising applications where low-molecular-weight chitosan is required, including biomedical, agricultural, and food industries, as well as the potential for reducing time and energy consumption.
RESUMO A reforma a seco do metano (RS) é um processo catalítico endotérmico que ocorre entre 700 e 900 oC, capaz de converter CH4 e CO2 (biogás) em H2 e CO (gás de síntese). Trabalhos têm sido elaborados visando o desenvolvimento de catalisadores ideais para a RS, buscando resolver os problemas encontrados, como é o caso da desativação do catalisador por formação de coque, que reduz o desempenho da produção do gás de síntese e pode obstruir o leito catalítico. Em trabalhos anteriores do Laboratório de Materiais e Energias Renováveis (LABMATER) da UFPR, foi desenvolvido o catalisador 20Ni/Si-MCM-41 que possui bom desempenho na conversão de CH4 e CO2 e baixa tendência à formação de coque (≈10 mgC.gcat-1.h-1), tratando-se de um material com carga nominal de Ni de 20% (m/m), suportado em uma peneira molecular a base de sílica mesoporosa (Si-MCM-41) de elevada área específica (≈600 m2 g-1). Entretanto, somente ensaios em unidades experimentais utilizando o catalisador em pó haviam sido realizados para testar a eficiência do material. Neste trabalho, foi utilizada uma unidade piloto contendo um reator contínuo de leito fixo, com o objetivo de avaliar a atividade do catalisador granulado e sua estabilidade na RS, de forma a subsidiar a construção futura de um reformador em escala industrial. Realizou-se quatro experimentos prévios com variação da composição reacional de 40-70% CH4:30-60% CO2, 3 g do catalisador 20Ni/Si-MCM-41 no leito catalítico, temperatura de 800 oC e vazão dos produtos de 36 L.h-1 a 1 atm. Os testes envolvendo variações nas composições de entrada com duração de 4 horas indicaram melhores resultados para a mistura 50% CH4:50% CO2. Também foi realizado um ensaio de 17 horas afim de verificar a estabilidade do catalisador, avaliar a formação de coque durante o tempo de reação e o desempenho da unidade piloto.