Engineering Materials & Structures (eMast) ikhoza, Malaysia-Japan International Institute of Technology (MJIIT), Universiti Teknologi Malaysia, 54100 Kuala Lumpur, Malaysia
Mr. Mohd aidy faizal Johari
Engineering Materials & Structures (eMast) ikhoza, Malaysia-Japan International Institute of Technology (MJIIT), Universiti Teknologi Malaysia, 54100 Kuala Lumpur, Malaysia
The enhancement of fuel economy and the emission of greenhouse gases are the key growing challenges around the globe that drive automobile manufacturers to produce lightweight vehicles. Additionally, the reduction in the weight of the vehicle could contribute to its recyclability and performance (for example crashworthiness and impact resistance). One of the strategies is to develop high-performance lightweight materials by the replacement of conventional materials such as steel and cast iron with lightweight materials. The lightweight composite which is commonly referred to as fiber-reinforced plastics (FRP) composite is one of the lightweight materials to achieve fuel efficiency and the reduction of CO2 emission. However, the damage of FRP composite under impact loading is one of the critical factors which affects its structural application. The bumper beam plays a key role in bearing sudden impact during a collision. Polymer composite materials have been abundantly used in a variety of applications such as transportation industries. The main thrust of the present paper deals with the use of high-strength glass fibers as the reinforcing member in the polymer composite to develop a car bumper beam. The mechanical performance and manufacturing techniques are discussed. Based on the literature studies, glass fiber-reinforced composite (GRP) provides more promise in the automotive industry compared to conventional materials such as car bumper beams.
5 July 2023 in Journal of Materials Research and Technology
This paper presents the effect of the micro-sized particles on the storage modulus and durability characteristics of magnetorheological elastomers (MREs). The initial phase of the investigation is to determine any associations among the microparticles’ weight percent fraction (wt%), structure arrangement, and the storage modulus of MRE samples. In order to carry out this, both isotropic and anisotropic types of MRE samples consisting of the silicone rubber matrix and 50, 60, 70, 75, and 80 wt% microparticles of carbonyl iron fractions are prepared. It is identified from the magneto-rheometer that the increase in storage modulus and decrease in linear viscoelastic region limit are observed in varying consistency depending on wt% and particle arrangement. The consistency of this dependency feature is highlighted by superimposing all of the graphs plotted to create the proposed the samples’ behavior model. In response to increasing magnetic stimulation, a sample of 70 wt% microparticles with an isotropic arrangement is found to be significant and stable. The experimentally defined fraction is then used for the durability test as the second phase of the investigation. During this phase, the durability evaluation is subjected to stress relaxation for an extended period of time. After undergoing durability testing, storage modulus performance is decreased by 0.7–13% at various magnetic stimulation levels. This result directly indicates that the storage modulus characteristics of different forms of MRE are sensitive to the different iron particle fractions’ and microparticles’ alignment. Therefore, important treatments to alter the storage modulus can be undertaken before the practical implementation to accommodate any desired performance of MRE itself and MRE application systems.
Temperature is one of the most influential factors affecting the performance of elastomer matrix in magnetorheological elastomer (MRE). Previous studies have utilized silica as a reinforcing filler in polymer composite and as a coating material in MRE to improve the thermal stability of the base material. However, the usage of silica as an additive in the thermal stability of MRE has not been explored. Thus, in this study, the effect of silica as an additive on the temperature-dependent mechanical and rheological properties of ethylene propylene diene monomer (EPDM)-based MREs was investigated by using 30 wt.% carbonyl iron particles (CIPs) as the main filler, with different contents of silica nanoparticles (0 to 11 wt.%). The microstructure analysis was examined by using field-emission scanning electron microscopy (FESEM), while the thermal characterizations were studied by using a thermogravimetric analyzer and differential scanning calorimetry. The tensile properties were conducted by using Instron Universal Testing Machine in the absence of magnetic field at various temperatures. Meanwhile, the rheological properties were analyzed under oscillatory loadings in the influence of magnetic field, using a rotational rheometer at 25 to 65 °C. The results revealed that the temperature has diminished the interfacial interactions between filler and matrix, thus affecting the properties of MRE, where the tensile properties and MR effect decrease with increasing temperature. However, the presence of silica capable improved the thermal stability of EPDM-based MRE by enhancing the interactions between filler and matrix, thus reducing the interfacial defects when under the influence of temperature. Consequently, the incorporation of silica nanoparticles as an additive in EPDM-based MRE requires more exploration, since it has the potential to sustain the properties of MRE devices in a variety of temperature conditions. Thus, the study on the temperature-dependent mechanical and rheological properties of MRE is necessary, particularly regarding its practical applications.
Engineering rubber composites have been widely used as main components in many fields including vehicle engineering and biomedical applications. However, when a rubber composite surface area is exposed to heat or sunlight and over a long-term accelerated exposure and lifecycle of test, the rubber becomes hard, thus influencing the mechanical and rheological behavior of the materials. Therefore, in this study, the deterioration of rheological characteristics particularly the phase shift angle (δ) of silicone rubber (SR) based magnetorheological elastomer (MRE) is investigated under the effect of thermal aging. SR-MRE with 60 wt% of CIPs is fabricated and subjected to a continuous temperature of 100 °C for 72 h. The characterization of SR-MRE before and after thermal aging related to hardness, micrograph, and rheological properties are characterized using low vacuum scanning electron microscopy (LV-SEM) and a rheometer, respectively. The results demonstrated that the morphological analysis has a rough surface and more voids occurred after the thermal aging. The hardness and the weight of the SR-MRE before and after thermal aging were slightly different. Nonetheless, the thermo-rheological results showed that the stress–strain behavior have changed the phase-shift angle (δ) of SR-MRE particularly at a high strain. Moreover, the complex mechanism of SR-MRE before and after thermal aging can be observed through the changes of the ‘in-rubber structure’ under rheological properties. Finally, the relationship between the phase-shift angle (δ) and the in-rubber structure due to thermal aging are discussed thoroughly which led to a better understanding of the thermo-rheological behavior of SR-MRE.
Magnetorheological elastomer (MRE) materials have the potential to be used in a wide range of applications that require long-term service in hostile environments. These widespread applications will result in the emergence of MRE-specific durability issues, where durability refers to performance under in-service environmental conditions. In response, the outdoor tropical climatic environment, combined with the effects of weathering, will be the primary focus of this paper, specifically the photodegradation of the MRE. In this study, MRE made of silicone rubber (SR) and 70 wt% micron-sized carbonyl iron particles (CIP) were prepared and subjected to mechanical and rheological testing to evaluate the effects under natural weathering. Magnetorheological elastomer samples were exposed to the natural weathering conditions of a tropical climate in Kuala Lumpur, Malaysia, for 30 days. To obtain a comprehensive view of MRE degradation during natural weathering, mechanical testing, rheology, and morphological evaluation were all performed. The mechanical and rheological properties test results revealed that after 30 days of exposure and known meteorological parameters, Young’s modulus and storage modulus increased, while elongation at break decreased. The degradation processes of MRE during weathering, which are responsible for their undesirable change, were given special attention. With the help of morphological evidence, the relationship between these phenomena and the viscoelastic properties of MRE was comprehensively defined and discussed.