The influence of alkyl acrylate comonomers in the rank of methyl- (MA), butyl- (BA), ethylhexyl- (EGA), and lauryl- (LA) in ternary copolymers based on acrylonitrile, alkyl acrylate and acrylamide (PAN-alkyl acrylate) on their solutions rheological behavior in dimethyl sulfoxide (DMSO), and mechanical properties of the spun fibers have been investigated. To reveal the role of molecular weight, two series of copolymers with molecular weights of ~50 and 150 kg/mol have been studied. It was shown that the nature of the alkyl acrylate does not significantly affect the rheological behavior of their solutions regardless of the length of the alkyl substituent and the content of the alkyl acrylate in copolymers. An exception is the high-molecular PAN-LA, which is characterized by a non-Newtonian behavior at lower concentrations. Two series of fibers were spun from the characterized ranks of low and high-molecular-weight copolymer solutions. For all copolymers, a 2.5–5-fold increase in the strength and elastic modulus of the fiber was found with an increase in Mw. It has been shown that PAN-MA and PAN-LA fibers have a tensile strength of 800 MPa that is 1.5–3 times higher than that of other copolymers spun in the same conditions.
A series of novel functional polycarbonates, specifically poly(solketal glycidyl ether carbonate-co-propylene carbonate)s with varying compositions, were synthesized through the ring-opening copolymerization of solketal glycidyl ether, propylene oxide, and carbon dioxide. The reaction was catalyzed by rac-(salcy)CoIIIX complexes with bis(triphenylphosphine)iminium salts as co-catalysts, achieving high selectivity. The resulting terpolymers exhibited number-average molecular weights ranging from 2 × 104 to 1 × 105 and a narrow, bimodal molecular weight distribution, with dispersities of 1.02–1.07 for each mode. Interestingly, the addition of a small amount of water to the reaction mixture yielded a terpolymer with a unimodal molecular weight distribution and a dispersity of 1.11. Subsequent acidic hydrolysis of the solketal protective groups produced poly(glyceryl glycerol carbonate-co-propylene carbonate). All terpolymers were amorphous, with Tg near or below room temperature. The hydroxyl-functional polycarbonates underwent cyclodepolymerization under milder conditions compared to polycarbonates with protected hydroxyl groups.