Additively manufactured Ti6Al4V parts have only seen major application in industries such as the aerospace and medical industries, mainly due to the high cost of production of the feedstock powder. In this article, the feasibility of in situ alloying a powder blend of elemental Ti and an Al–V master alloy to produce the Ti6Al4V alloy through direct metal laser sintering is presented and discussed. In a previous study, single track formation from this powder blend was studied and analyzed to determine the optimum principal process parameters suitable for this powder blend. These process parameters were employed in this study to produce single and double layers where the effects of varied hatch distance and the employment of a rescanning strategy on the surface morphology and alloy homogeneity were investigated. Lastly, in the current study, three-dimensional specimens were produced and analyzed to determine the alloy microstructure, homogeneity, part porosity and mechanical properties. The analyses revealed that a Ti6Al4V alloy with a density of up to 99.9% and corresponding tensile strength and ductility values of up to 942.9 MPa and 17% was produced. Furthermore, a minimum Al evaporation value of 7.2% was recorded. Therefore, in situ alloying can indeed be employed to produce high-quality Ti6Al4V parts from an elemental Ti and an Al–V master alloy powder blend.
The mechanical properties of components manufactured via fused filament fabrication (FFF) are significantly influenced by defects that occur during printing and post-processing conditions. This study thoroughly investigated the effects of post-heat treatment on the internal microstructure and mechanical properties of 3D-printed polylactic acid (PLA) reinforced with short carbon fibers (PLA–CF). Samples were produced using FFF and subsequently annealed at 50 and 120 °C for 2 h. X-ray microscopy (XRM) was employed to assess the internal defects, void distribution, and microstructural changes at both the macro and micro levels resulting from the heat treatment. XRM volume segmentation revealed that voids decreased steadily as the treatment temperature increased. The untreated samples had a solid-to-void ratio of 56.205%. The sample treated at 50 °C had a ratio of 56.72%, and the sample treated at 120 °C had a solid-to-void ratio of 58.922%. Mechanical testing adhered to ASTM D638 standards, and the experimentally determined geometries were used in finite element analysis models to confirm the thermomechanical responses. The findings revealed that annealing improved the tensile strength and ductility by enhancing interlayer bonding and reducing porosity while preserving material toughness. These results highlight the significance of controlled heat treatment in optimizing the performance of FFF-printed PLA–CF composites and demonstrate the value of incorporating XRM-informed geometries into computational models for accurate-performance prediction.