Lead was recovered through a direct smelting reduction route from a lead concentrate by using mixtures of Na2CO3 and SiC to 1000 °C. The lead concentrate was obtained from the mining State of Zacatecas, México by traditional mineral processing and froth flotation. The experimental trials showed that 86 wt.% of lead with a purity up to 97% can be recovered from the lead concentrate by a single step reduction process when 40 wt.% Na2CO3 and 0.4 g SiC were used in the initial charge. The process was modeled in the thermodynamic software FactSage 7.3 to evaluate the effect of adding different amounts of Na2CO3 on the lead recovery rates while holding constant the SiC amount and temperature. The stability phase diagram obtained showed that an addition of 34 wt.% Na2CO3 was enough to reach the highest lead recovery. It was observed that the interaction of Na2CO3 and SiC at a high temperature promotes the formation of C and Na2O, and SiO2, respectively, where the Na2O partially bonds with silica and sulfur forming Na2S and sodium silicates which may decrease the SO2 emissions and increase the weather degradation of the slag. The PbS was mainly reduced by the produced C and CO formed by the interaction between Na2CO3 and SiC at 1000 °C. The predicted results reasonably match with those obtained experimentally in the lead recovery rates and compounds formation.
1 January 2023 in Journal of Mining and Metallurgy, Section B: Metallurgy
In the present work, the effect of low aluminum additions and the hot forging process on the microstructure and non-metallic inclusions of high manganese steels is analyzed. Four high-manganese steels (HMnS) were prepared by adding low aluminum contents of 1.1 and 1.5 wt. % to four carbon austenitic steels with medium carbon content (0.3 - 0.4 wt% C) and manganese contents of 17 and 22 wt. Samples of the as-cast steels were hot forged to 1100?C to obtain an overall reduction of 70 %. Microstructural evolution was studied using microscopy techniques (OM, and SEM-EDS) and X-ray diffraction measurements for the as-cast and hot forged steels. A typical grain columnar zone formed during solidification of a cast ingot was obtained in the as-cast condition, where the microstructure consisted of nonmetallic inclusions in a fully austenitic matrix. The non-metallic inclusions were identified as Al2O3 and MnS particles. Thermomechanical treatment allows the formation of an austenitic microstructure characterized by twins in steels with high manganese content, while an austenitic-martensitic duplex microstructure was obtained in HMnS, which contained the lowest manganese contents. The highest tensile strength values were obtained for 17Mn-1Al steel, which had the smallest grain size and higher content of non-metallic inclusions. The hardness values were similar to those obtained in the as-cast condition.
Closed-cell A356 aluminum alloy foams refined and modified were successfully fabricated by using barite and calcium carbonate as thickening and foaming agents, respectively. A melt treatment consisting of adding master alloys of Al-5Ti-1B and Al-10Sr for refining the dendritic microstructure and modifying the primary eutectic silicon, respectively, were included in the foaming process. The microstructure and mechanical properties of the foams manufactured were analyzed and compared with foams produced without the refining and modifying treatments. The secondary dendritic arm spacing (SDAS) was determined by optical measurements. Lower SDAS values were obtained in foam regions closer to the mold walls due to the high solidification rate imposed during the cooling step and a decrease in the SDAS values for the foams produced with the addition of the Al-5Ti-1B master alloy was evident. Additionally, the addition of the Al-10Sr master alloy caused the formation of solid solution dendrites and a fine irregular fibrous form of silicon. Foams produced with the melt treatment exhibit a good combination of structure and mechanical properties. Therefore, the melt route established is a feasible way to improve foam performance where the lowest SDAS and the highest mechanical properties were obtained for the closed-cell foams produced.
A previously pyrometallurgical process, developed to obtain a Pb-Ag alloy and a slag rich in sulfur from the recycling of a mixture of industrial wastes of jarosite and lead paste, was thermodynamically assessed at 1200 °C. The industrial jarosite sourced from a Mexican zinc hydrometallurgical plant corresponded to an ammonium jarosite with a measurable silver content. The specific heat capacity (Cp) of the ammonium jarosite was obtained from TGA and DSC measurements, as well as the thermodynamic functions of enthalpy, entropy, and Gibbs free energy. The Cp was successfully modeled using polynomial regression, with a second-degree polynomial employed to describe the low-temperature behavior. The thermodynamic data generated were input into the thermodynamic software FactSage 8.2 for modeling of the lead paste–ammonium jarosite-Na2CO3-SiC system and represented by stability phase diagrams. The thermodynamic assessment of the pyrometallurgical process predicted compounds formed at high temperatures, showing that a Pb-Ag alloy and a slag rich in Na, S, and Fe (NaFeS2 and NaFeO2) were obtained. The compounds formed evidence of the effective sulfur retention in the slag, which is crucial for mitigating SO2 emissions during high-temperature treatments. The experimental compounds, after solidification, were determined by X-ray diffraction measurements to be Na2Fe(SO4)2 and Na2(SO4), which reasonably match the thermodynamic assessment. The heat capacity of the ammonium jarosite provides essential thermodynamic insights into the compositional complexities of industrial waste, which are particularly relevant for thermodynamic modeling and process optimization in pyrometallurgical systems aimed at metal recovery and residue valorization.
Ductile iron (DI) can acquire various properties with the addition of alloying elements and through heat treatment. In this work, the effects of vanadium and molybdenum on the microstructure and corrosion resistance of DI and austempered ductile iron (ADI) were studied. Corrosion resistance was evaluated by potentiodynamic polarization techniques in 0.5 M H2SO4, 0.5 M NaCl, and 05 M NaOH as electrolyte. The ADI alloyed with vanadium presented anupper ausferritic microstructure consisting of broad ferrite needles, while the combination of vanadium and molybdenum allows obtaining a fine microstructure composed of ausferrite and thin needles of ferrite; this microstructure improves the corrosion resistance in NaCI and NaOH. The DI’s showed corrosion due to the galvanic pair between the graphite nodule and the ferrite; however, a high amount of carbide increases the corrosion resistance in H2SO4.
A silver-rich lead alloy was obtained through the recycling of two metallurgical wastes: these are lead paste obtained from spent lead–acid batteries and a jarosite residue obtained from the hydrometallurgical production of zinc. Mixtures of both wastes were pyrometallurgically treated with sodium carbonate in a silicon carbide crucible at 1200 °C. The alloy and slag produced were analyzed by atomic absorption spectrometry, X-ray diffraction, and scanning electron microscopy with energy-dispersive spectra. High silver recovery was obtained in a Pb-Ag alloy for a mixture ratio of 30% Na2CO3–40% lead paste–30% jarosite, reaching a silver grade of 126 ppm. The slags produced for the highest jarosite content allow the compound formation of Na2(SO4) and Na2Fe(SO4)2, which have high sulfur-fixing, avoiding SO2 release and contributing to the minimization of atmospheric pollution. The novel pyrometallurgical route addresses not only the valorization of precious metals such as silver and lead but also the reduction in accumulated industrial waste.