Simen Martinussen

Mr. Simen Martinussen

University of Twente
orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
27 September 2024 in Optics Express
Verified
Journal Article
Closed access
SMSimen Martinussen
Simen Martinussen
EBErwin Berenschot
Erwin Berenschot
DBDawson Bonneville
Dawson Bonneville
KWKai Wang
Kai Wang
MDMeindert Dijkstra
Meindert Dijkstra
Roald M. TiggelaarRoald M. Tiggelaar
Roald M. Tiggelaar
Low-stress stoichiometric silicon nitride (Si3N4) waveguides with an unprecedented thickness of up to 1350 nm and a width in the range of 2.2 - 2.7 µm are fabricated using a single LPCVD step on sapphire substrates (SiNOS). Optical characterization of proof-of-concept ∼1.35 µm thick waveguides show propagation losses in the order of 0.30 ± 0.01 dB/cm at 1600 nm. The proposed process offers a simple route to high confinement Si3N4 waveguides, enabling applications in nonlinear and mid-IR integrated photonics.

15 July 2019 in Optical Materials Express
Verified
Journal Article
Closed access
SMSimen Martinussen
Simen Martinussen
RFRaimond N. Frentrop
Raimond N. Frentrop
MDMeindert Dijkstra
Meindert Dijkstra
FSFrans Segerink
Frans Segerink
VTVictoria Tormo-Márquez
Victoria Tormo-Márquez
Sonia BlancoSonia Blanco
Sonia Blanco

24 November 2020 in Micromachines
Verified
Journal Article
Open access
PDF file
SMSimen Martinussen
Simen Martinussen
RFRaimond N. Frentrop
Raimond N. Frentrop
MDMeindert Dijkstra
Meindert Dijkstra
Sonia BlancoSonia Blanco
Sonia Blanco
KY(WO4)2 is a promising material for on-chip laser sources. Deep etching of small KY(WO4)2 samples in combination with various thin film deposition techniques is desirable for the manufacturing of such devices. There are, however, several difficulties that need to be overcome before deep etching of KY(WO4)2 can be realized in small samples in a reproducible manner. In this paper, we address the problems of (i) edge bead formation when using thick resist on small samples, (ii) sample damage during lithography mask touchdown, (iii) resist reticulation during prolonged argon-based inductively coupled plasma reactive ion etching (ICP-RIE), and (iv) redeposited material on the feature sidewalls. We demonstrate the etching of 6.5 µm deep features and the removal of redeposited material using a wet etch procedure. This process will enable the realization of waveguides both in ion-irradiated KY(WO4)2 as well as thin KY(WO4)2 membranes transferred onto glass substrate by bonding and subsequent polishing.