High thermal conductivity electronic materials are critical components for high-performance electronic and photonic devices as both active functional materials and thermal management materials. We report an isotropic high thermal conductivity exceeding 500 W m−1K−1 at room temperature in high-quality wafer-scale cubic silicon carbide (3C-SiC) crystals, which is the second highest among large crystals (only surpassed by diamond). Furthermore, the corresponding 3C-SiC thin films are found to have record-high in-plane and cross-plane thermal conductivity, even higher than diamond thin films with equivalent thicknesses. Our results resolve a long-standing puzzle that the literature values of thermal conductivity for 3C-SiC are lower than the structurally more complex 6H-SiC. We show that the observed high thermal conductivity in this work arises from the high purity and high crystal quality of 3C-SiC crystals which avoids the exceptionally strong defect-phonon scatterings. Moreover, 3C-SiC is a SiC polytype which can be epitaxially grown on Si. We show that the measured 3C-SiC-Si thermal boundary conductance is among the highest for semiconductor interfaces. These findings provide insights for fundamental phonon transport mechanisms, and suggest that 3C-SiC is an excellent wide-bandgap semiconductor for applications of next-generation power electronics as both active components and substrates.
We attempted to control grain boundary propagation in mono-like Si utilizing functional grain boundaries introduced by multi-seeds with specific configurations, and demonstrated that functional grain boundaries can suppress multi-crystallization during growth. The suppression mechanism was studied on the basis of grain boundary character. The grain boundaries nucleate at the crucible surface, which generally leads to multi-crystallization, interact with the functional grain boundaries, resulting in a change of their character and configuration. This would increase the yield of the mono-like wafers in an ingot and would enable a large reduction of cost per watt of solar cells.
Optical properties of wurtzite ZnO bulk single crystals in which an arbitrary number (typically 109–1010 cm−2) of fresh dislocations were introduced intentionally by the plastic deformation at elevated temperatures (923–1073 K) were examined. Deformed specimens showed excitonic light emission with photon energies of 3.100 and 3.345 eV, as well as their LO phonon replicas at 11 K. The light intensities increased with increasing dislocation density. The activation energy for a thermal quenching of the 3.100 or 3.345 eV emission band, which corresponds to the depth of the localized energy level associated with the emission band, was estimated to be 0.3±0.1 or 0.05±0.01 eV, respectively. The origin of the energy levels was proposed as point defect complexes involving dislocations. The introduction of the dislocations at the elevated temperatures above 923 K did not influence the intensities of the emission bands except the dislocation-related emission bands.