The amount of solid waste generated annually is increasing around the world. Although the waste has a high calorific value, one major obstacle that may prevent it from becoming a feedstock for power applications is the existence of polyvinyl chloride (PVC), which causes corrosion and emission issues after combustion due to its high chlorine content. Torrefaction is known to release hydrochloric acid; thus, it has been applied in this study for the reduction of chlorine from potential waste feedstocks. Fiber-plastic (60–40%) waste blends, with different chlorine content levels, as well as PVC were used in the current study. Torrefaction was conducted at 400 °C. Chlorine and heat content were measured. Experimental results showed that organically bonded chlorine was reduced during torrefaction as a function of mass loss. The chlorine removal efficiency was only dependent on temperature and residence time, not chlorine level. The heat content of the sample increased with mass loss up to a maximum of ~34 MJ/kg at ~45% mass loss. It was also observed that at ~30% mass loss, the organic chlorine content per unit heat content reduced by ~90%, while the heat content was ~32 MJ/kg, and ~90% energy was retained.
Plastic waste accumulation has been growing due to the increase in plastic generation and the lack of infrastructure for recycling. One of the approaches is to treat the mixed plastic waste (MPW) through thermal processes to produce feedstocks for other applications. However, the presence of polyvinyl chloride (PVC) in MPW would produce HCl during processing and has negative impacts (emission, catalyst poisoning, etc.). In addition, due to the high heterogeneity of MPW, it is difficult to generate consistent experimental data. In this study, MPW was homogenized through double compounding–extrusion and then formed into a sheet to be treated at 400 °C. The solid products at various mass losses were characterized by heat and chlorine content, Fourier-transform infrared (FTIR) spectroscopy, and elemental composition analysis. It was found that the thermal degradation of MPW started at ~260 °C. The chlorine removal efficiency increased with mass loss and reached an asymptotic value of ~84% at ~28% mass loss, and the remaining chlorine can be attributed to inorganic sources. A PVC de-chlorination model was developed for MPW using TGA data for PVC and MPW to determine organic chlorine removal efficiency. These results show that PVC de-chlorination was not affected by other plastics at this temperature. As the mass loss increases, the heat content first increases and then decreases. It was found that mass loss is a universal parameter for organic chlorine removal efficiency and heat content. The elemental composition analysis and FTIR spectroscopy also shed more light into the chemical changes during MPW thermal degradation.