6 September 2021 in Metals
Verified
Journal Article
Open access
PDF file
JZJin Zhang
Jin Zhang
WTWenfu Tan
Wenfu Tan
CWCheng Wang
Cheng Wang
CZChunnan Zhu
Chunnan Zhu
YYyouping yi
youping yi
Cryogenic deformation can improve the strength and plasticity of Al–Li alloy, although the underlying mechanism is still not yet well understood. The effects of cryogenic temperature on the tensile properties and microstructure of an Al–Cu–Li alloy were investigated by means of tensile property test, roughness measurement, scanning electron microscope (SEM), optical microscope (OM), electron backscatter diffraction (EBSD), and transmission electron microscope (TEM). The results indicated that the strength and elongation of the as-annealed (O-state) and solution-treated (W-state) alloys increased with the decrease in deformation temperature, where the increasing trend of elongation of the W-state alloy was more significant than that of the O-state alloy. In addition, a temperature range was observed at approximately 178 K that caused the strength of the W-state alloy to slightly decrease. The decrease in temperature inhibited the dynamic recovery of the Al–Cu–Li alloy, which increased the dislocation density and the degree of work hardening, thus improving the strength of the alloy. At cryogenic temperatures, the internal grain structure was more involved in the deformation and the overall deformation was more uniform, which caused the alloy to have higher plasticity. This study provides a theoretical basis for the cryogenic forming of Al–Li alloy.

7 January 2023 in Acta Metallurgica Sinica (English Letters)
Verified
Journal Article
Closed access
PDF file
ZJZhen Jiang
Zhen Jiang
DSDongfeng Shi
Dongfeng Shi
JZJin Zhang
Jin Zhang
Tianming LiTianming Li
Tianming Li
LLLiwei Lu
Liwei Lu

11 August 2022 in Materials
Verified
Journal Article
Open access
PDF file
DSDongfeng Shi
Dongfeng Shi
JZJin Zhang
Jin Zhang
This study investigated the twinning behavior with increasing compressive strain in rolled AZ31 alloy. With that purpose, a polycrystalline structure with an average grain size of 30 μm was utilized to perform the uniaxial compression tests. Microstructure evolution was traced by in situ electron backscattered diffraction (EBSD). Multiple primary twin variants and extension double twins were observed in the same grain. A comprehensive analysis of kernel average misorientation (KAM) and Schmid factor (SF) revealed that the nucleation of twins in one special grain is not only based on the SF criterion, but that it is also strongly influenced by surrounding grains. Moreover, the existing primary twins modified the inner and outer strain distribution close to the twin boundaries. With continued compression, the strain inside the primary twins stimulated the nucleation of double twins, while the strain in the matrixes facilitated twin growth. Therefore, the primary twin growth and the new nucleation of secondary twins could take place simultaneously in the same twinning system to meet the requirements of strain accommodation. Twinning behaviors are controlled by the combined effect of the Schmid factor, strain accommodation between surrounding grains, and variation in the local stress state. The local stress exceeded the critical resolved shear stress (CRSS), implying that twin nucleation is possible. Hence, the twinning process tends to be a response of the local stress rather than the applied stress.

22 January 2019 in Metals
Verified
Journal Article
Open access
PDF file
JZJiuhui Zhao
Jiuhui Zhao
YDYunlai Deng
Yunlai Deng
FXFushun Xu
Fushun Xu
JZJin Zhang
Jin Zhang
Fine-grained (average gain size 3.8 μm) and coarse-grained (average gain size 24.9 μm) Al-Zn-Mg-Cu alloys were subjected to isothermal compression at 10−3 s−1 and temperature ranges from 300 °C to 450 °C. The grain structures after isothermal compression were observed by electron backscatter diffraction (EBSD). The results show that the continuous dynamic recrystallization (CDRX) mechanism dominated to form sub-grains in grain interiors during isothermal compression of coarse-grained materials, and sub-grains were gradually developed in grain interiors as the effective strain increased. Discontinuous dynamic recrystallization (DDRX) was the main recrystallization mechanism during isothermal compression of fine-grained materials, in which finer recrystallized grains were formed at grain boundaries. The temperature of isothermal compression had little influence on the recrystallization when the growth of recrystallized grains was slight, and sub-grains were hardly developed in fine-grain interiors.

22 September 2022 in Materials
Verified
Journal Article
Open access
PDF file
HHHao Huang
Hao Huang
WXWei Xiong
Wei Xiong
ZJZhen Jiang
Zhen Jiang
JZJin Zhang
Jin Zhang
An optimized homogenization process for Al alloy ingots is key to subsequent material manufacturing, as it largely reduces metallurgical defects, such as segregation and secondary phases. However, studies on their exact microstructural evolution at different homogenization temperatures are scarce, especially for complex systems, such as the 2195 Al-Cu-Li alloy. The present work aims to elucidate the microstructural evolution of the 2195 Al-Cu-Li alloy during homogenization, including the dissolution and precipitation behavior of the TB (Al7Cu4Li) phase and S (Al2CuMg) phase at different homogenization temperatures. The results show that there are Cu segregation zones (Cu-SZ) at the dendrite boundaries with θ (Al2Cu) and S eutectic phases. When the temperature rises from 300 °C to 400 °C, fine TB phases precipitate at the Cu-SZ, and the Mg and Ag in the S phases gradually diffuse into the matrix. Upon further increasing the temperature to 450 °C, TB and θ phases at the grain boundaries are coarsened, and an S-θ phase transition is observed. Finally, at 500 °C, all TB and S phases are dissolved, leaving only θ phases at triangular grain boundaries. This work provides guidance for optimizing the homogenization procedure in 2195 alloys.

27 August 2021 in Materials
Verified
Journal Article
Open access
PDF file
CWCheng Wang
Cheng Wang
JZJin Zhang
Jin Zhang
YYyouping yi
youping yi
CZChunnan Zhu
Chunnan Zhu
The mechanical properties of Al-Cu-Li alloys after different pretreatments were investigated through tensile testing at 25 and −196 °C, and the corresponding microstructure characteristics were obtained through optical metallography, scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. An increasing mechanism of both strength and ductility at cryogenic temperatures was revealed. The results show that the hot deformation pretreatment before homogenization promoted the precipitation of Al3Zr particles, improved particle distribution, and inhibited local precipitation-free zones (PFZ). Both hot deformation pretreatment before homogenization and cryogenic temperature were able to improve strength and ductility. The former improved strength by promoting the precipitation of Al3Zr particles while enhancing the strengthening effect of the second-phase particles and reducing the thickness of the coarse-grained layer. Meanwhile, the increase in ductility is attributable to the decrease in thickness of the coarse-grained layer, which reduced the deformation incompatibility between the coarse and fine grains and increased the strain-hardening index. The latter improved the strength by suppressing dynamic recovery during the deformation process, increasing the dislocation density, and enhancing the work hardening effect. Additionally, the increase in ductility is attributable to the suppression of planar slip and strengthening of grain boundaries, which promoted the deformation in grain interiors and made the deformation more uniform.