Micro/nano structuring of KrF Excimer laser-irradiated Aluminum (Al) has been correlated with laser-produced structural and mechanical changes. The effect of non-reactive Argon (Ar) and reactive Oxygen (O2) environments on the surface, structural and mechanical characteristics of nano-second pulsed laser-ablated Aluminum (Al) has been revealed. KrF Excimer laser with pulse duration 20 ns, central wavelength of 248 nm and repetition rate of was utilized for this purpose. Exposure of targets has been carried out for 0.86, 1, 1.13 and 1.27 J·cm−2 laser fluences in non-reactive (Ar) and reactive (O2) ambient environments at a pressure of 100 torr. A variety of characteristics of the irradiated targets like the morphology of the surface, chemical composition, crystallinity and nano hardness were investigated by using Scanning Electron Microscopy (SEM), Atomic Force Microscopy (AFM), Energy Dispersive X-ray Spectroscopy (EDS), X-ray Diffractometer (XRD), Raman spectroscopy and Nanohardness tester techniques, respectively. The nature (reactive or non-reactive) and pressure of gas played an important role in modification of materials. In this study, a strong correlation is observed between the surface structuring, chemical composition, residual stress variation and the variation in hardness of Al surface after ablation in both ambient (Ar, O2). In the case of reactive environment (O2), the interplay among the deposition of laser energy and species of plasma of ambient gas enhances chemical reactivity, which causes the formation of oxides of aluminum (AlO, Al2O3) with high mechanical strength. That makes it useful in the field of process and aerospace industry as well as in surface engineering.
The surface, structural, and mechanical properties of zirconium after irradiation with Ti: sapphire laser (800 nm, 30 fs, 1 kHz) have been investigated. The zirconium targets were exposed for a varying number of laser pulses ranging from 500 to 2000 at a fixed fluence of 3.6 J/cm2 corresponding to an intensity of 1.2×1014 W/cm2 in ambient environments of de-ionized water and propanol. A scanning electron microscope (SEM) was employed to investigate the surface morphology of the irradiated zirconium. The SEM analysis shows the formation of various kinds of features including nanoscale laser induced periodic surface structures (LIPSS), sponge like surface structure, flakes, conical structures, droplets, pores, and cavities. The energy dispersive x-ray spectroscopy (EDS) analysis exhibits the variation in chemical composition along with an enhanced diffusion of oxygen under both ambient conditions. The crystal structure and phase analyses of the exposed targets were explored by x-ray diffraction (XRD) and Raman spectroscopy techniques, respectively. The XRD analysis confirms the presence of various phases of zirconium hydride and zirconia after ablation in both de-ionized water and propanol. However, excessive hydrides are formed in the case of propanol. The Raman analysis supports the EDS and XRD results. It also reveals the presence of oxides (zirconia) after irradiation in both de-ionized water and propanol environments. The chemical reactivity of zirconium was significantly improved in the presence of liquids which were accountable for the growth of novel phases and modification in the chemical composition of the irradiated Zr. A nanohardness tester was employed to measure the nanohardness of the laser treated targets. The initial increase and then decrease in nanohardness was observed with an increase in the number of laser pulses in the de-ionized water environment. In the case of propanol, a continuous decrease in hardness was observed.
Liquid-assisted laser ablation (LALA) has gained substantial attention as a method that can achieve desired chemical and physical properties. The fabrication of carbides (CdCO3), oxides (CdO), and hydro-oxides (Cd(OH)2) on Cd surfaces make them more useful in industrial and biomedical applications due to the enhancement of their physical properties. For this purpose, LALA of Cadmium (Cd) is performed using a KrF Excimer laser (248 nm, 20 ns) at varying numbers of pulses from 500 to 2000 at constant fluence (3.6 Jcm−2) in deionized water (DI) and ethanol. A comparison of the ablation behavior of Cd in DI water and alcohol (ethanol) environments is discussed in the present work. The surface structuring and enhancement of mechanical properties are also discussed in correlation with the changes produced in its crystallinity due to the increase in the chemical reactivity of Cd in both ambient environments. The surface features, chemical composition, structural and compositional analysis, and mechanical properties of irradiated targets are evaluated using a Scanning Electron Microscope (SEM), X-ray Diffraction (XRD), Fast Fourier Transform Infrared spectroscopic (FTIR), Energy Dispersive X-ray Spectroscopy (EDS), and a Nano-hardness tester. Pores, cavities, hillocks, wave-like ridges, nanoparticles, flake-like structures, and periodic surface structures are distinguished features on the Cd surface after irradiation. However, the density and size of pores and cavities are higher in water, whereas ethanol is favorable for the growth of craters and ripples. These features are attributable to various thermal and chemical phenomena induced by laser heating at the solid–liquid interface. Ethanol-assisted ablation is more favorable for enhancing the hardness of Cd as compared to DI water-assisted ablation due to the presence of maximum compressive stresses and minimum crystallite size (C.S.) caused by the diffusion of carbon into the target surface.