We report on the thickness scaling behavior of ferroelectric Sc0.3Al0.7N (ScAlN) films grown on Mo substrates by molecular beam epitaxy. Switchable ferroelectricity is confirmed in ScAlN films with thicknesses ranging from 100 to 5 nm. An increase in coercive field and a significant diminution of remnant polarization are found when the ferroelectric layer is scaled down to below 20 nm. Notably, a switching voltage of 2–3.8 V and saturated remnant polarization of ∼23 μC/cm2 are measured in 5 nm thick ScAlN. X-ray diffractions and transmission electron microscopy studies indicate that the increase in coercive field and diminishment in switchable polarization can be closely linked to the surface oxidation and strain state in ultrathin ScAlN films. This work sheds light on the fundamental thickness scaling fingerprints of ScAlN thin films and represents an important step for next-generation compact and power-efficient devices and applications based on nitride ferroelectrics.
We report the demonstration of ferroelectric switching in yttrium (Y)-doped nitride semiconductors. In this study, single-crystalline, wurtzite Y0.07Al0.93N films were epitaxially grown on GaN/sapphire templates by plasma-assisted molecular beam epitaxy. The ferroelectric switching process has been investigated by current density–electric field (J-E) and polarization–electric field (P-E) loops as well as positive-up-negative-down measurements, showing a coercive field of ∼6 MV/cm and a switchable polarization of ∼130 μC/cm2. Ferroelectric switching was further confirmed via butterfly shape capacitance–voltage (C-V) loops and polarity-sensitive wet etching. The realization of ferroelectric, Y-doped AlN films further extends the family of nitride ferroelectrics and unravels a wealth of intriguing opportunities in III-nitride based electronic, piezo-electronic, and optoelectronic devices.
In this Letter, we demonstrated fully epitaxial ScAlN/AlGaN/GaN based ferroelectric high electron mobility transistors (HEMTs). Clean and atomically sharp heterostructure interfaces were obtained by utilizing molecular beam epitaxy. The fabricated ferroelectric gate HEMTs showed counterclockwise hysteretic transfer curves with a wide threshold voltage tuning range of 3.8 V, a large ON/OFF ratio of 3 × 107, and reconfigurable output characteristics depending on the poling conditions. The high quality ferroelectric gate stack and effective ferroelectric polarization coupling lead to improved subthreshold performance, with subthreshold swing values approaching 110 and 30 mV/dec under forward and backward gate sweeps, respectively. The results provide fundamental insight into the ferroelectric polarization coupling and threshold tuning processes in ferroelectric nitride heterostructures and are promising for nitride-based nonvolatile, multi-functional, reconfigurable power, and radio frequency devices as well as memory devices and negative capacitance transistors for next-generation electronics.
Significant efforts are being put into the development of efficient micrometer-scale light emitting diodes (LEDs) for future display technologies due to their marked benefits over existing displays. To date, however, the efficiency of microLED devices remains significantly lower than that of conventional broad-area devices. The deterioration in device performance with smaller device size has been linked to the plasma damage induced on mesa sidewalls during device fabrication. Here, we studied bottom-up red-emitting nanowire LEDs with different Mg doping levels in the p-GaN layer. The resulting sub-micron LED devices show a distinct improvement in efficiency with increasing Mg dopant incorporation. Through optimization of the doping, we measured an external quantum efficiency of ∼8.3% and a wall-plug efficiency of ∼4.6%, at a current density of ∼1 A/cm2, for a red-emitting sub-micrometer scale LED operating at >630 nm. This study highlights the importance of p-doping in microLEDs for attaining high efficiency performance in nanostructure-based devices.
Molecular beam epitaxy of single-phase wurtzite N-polar ScxAl1−xN (x ∼ 0.11–0.38) has been demonstrated on sapphire substrates by locking its lattice-polarity to the underlying N-polar GaN buffer. Coherent growth of lattice-matched Sc0.18Al0.82N on GaN has been confirmed by x-ray diffraction reciprocal space mapping of the asymmetric (105) plane, whereas lattice-mismatched, fully relaxed Sc0.11Al0.89N and Sc0.30Al0.70N epilayers exhibit a crack-free surface. The on-axis N-polar crystallographic orientation is unambiguously confirmed by wet chemical etching. High electron mobility transistors using N-polar Sc0.18Al0.82N as a barrier have been grown on sapphire substrates, which present the existence of well confined two-dimensional electron gas. A Hall mobility of ∼564 cm2/V s is measured for a 15-nm-thick Sc0.18Al0.82N barrier sample with a sheet electron concentration of 4.1 × 1013 cm−2, and the corresponding sheet resistance is as low as 271 Ω/sq. The polarity-controlled epitaxy of ScxAl1−xN provides promising opportunities for applications in high-frequency and high-power electronic and ferroelectric devices.