In this paper, titanium–dioxide (TiO2) nanotubes (TNTs) are formed by anodic oxidation with a fluorinated glycerol–water (85% and 15%, respectively) electrolyte to examine the effect of fluoride ion concentration, time, and applied voltage on TNT morphologies and dimensions. For fluoride ion concentration, the surface etching increases when the amount of ammonium fluoride added to the electrolyte solution increases, forming nanotube arrays with a clear pore structure. At a constant voltage of 20 V, TNTs with an average length of ~2 µm are obtained after anodization for 180 min. A prolonged anodization time only results in a marginal length increment. The TNT diameter is voltage dependent and increases from approximately 30 nm at 10 V to 310 nm at 60 V. At 80 V, the structure is destroyed. TNTs formed at 20 V for 180 min are annealed to induce the TiO2 anatase phase in either air or nitrogen. When ethylenediaminetetraacetic acid is added as a hole scavenger, 100% hexavalent chromium removal is obtained after 120 min of sunlight exposure for nitrogen-annealed TNTs.
The length of titania nanotubes formed by anodization of 0.1 mm thick titanium foil was found to be a strong function of the pH of the electrolyte. The longest nanotubes were formed by using an electrolyte consisting of 1 M Na2SO4 plus 5 wt% NH4F with pH 7. At this pH, after 30 min of anodization, 3 mu m length nanotubular titania arrays with top diameters of similar to 50 nm and bottom diameters of 100 nm were produced. No acid was added to this electrolyte. The formation of titania nanotubes in neutral pH systems was therefore successful due to the excess NH4F in the electrolyte which increases the chemical dissolution process at the metal/oxide interface. Since the pH of the electrolyte at the top part of the nanotubes is kept very high, the dissolution of the nanotubes at the surface is minimal. However, the amount is adequate to remove the initial barrier layer, forming a rather well-defined nanoporous structure. All anodized foils were weakly crystalline and the transformation to anatase phase was achieved by heat treatment at temperatures from 200 to 500 degrees C for 1 h in air. Annealing at temperatures above 500 degrees C induce rutile phase formation and annealing at higher temperatures accelerates the diffusion of Ti4+ leading to excessive growth and the nanotubular structure diminishes.