The main characteristic of ready mix mortar is to remain workable for up to 72hours after mixing. This greater duration of workability is obtained by use of hydration stabilizing admixtures and air-entrained admixtures. Thus, the behavior of this mortar depends on the compatibility between Portland cement and these two admixtures. Within this context, the objective of this article is to evaluate the influence of Portland cement type and water content on the properties of ready mix mortars in fresh state. Three types of Portland cement and four water/dry material ratios were evaluated. The produced mortars were analyzed with respect to their properties in fresh state: consistency index, specific gravity, air entrained content and rheological behavior by squeeze-flow. The properties were determined for three storage durations (0, 24 and 48 hours). The results show that both types of cement (mainly, the rheological behavior) and water content (mainly, the air entrained content, consistency and rheological behavior) influenced the ready mix mortar properties. Therefore, these two parameters must be evaluated for mortar dosages in order to obtain the required properties in fresh state.
This study evaluated the effect of precursor particle size and calcium hydroxide (CH) incorporation on the microstructure, compressive strength, and rheological properties of clay brick waste (BW)-based geopolymers. Rheological analyses were used to evaluate the fresh state of the geopolymers. XRD, SEM, and EDS analyses were performed to analyze the microstructure. The results showed that the particle size reduction in BW and the incorporation of CH significantly contributed to obtaining better compressive strength in the geopolymers. Furthermore, the particle size reduction decreased the yield stress, plastic viscosity, and hysteresis area of the geopolymers, while the incorporation of CH promoted the opposite effect. Increasing the CH incorporation content accelerated the geopolymerization reactions and reduced the workability of the geopolymers over time. However, since the milling process is costly, milling BW for 2 h was more efficient from a technical–economic point of view. In addition, the incorporation of CH not only promoted the early hardening of the geopolymers when necessary, but also contributed to the improvement of the compressive strength through matrix densification. Therefore, the results of this study show the definition of more efficient material proportions for geopolymers using waste as an aluminosilicate source.
Nanomaterials are potential candidates to improve the mechanical properties and durability of cementitious composites. SiC nanowhiskers (NWs) present exceptional mechanical properties and have already been successfully incorporated into different matrices. In this study, cementitious composites were produced with a superplasticizer (SP) and 0–1.0 wt % SiC NWs. Two different NWs were used: untreated (NT-NW) and thermally treated at 500 °C (500-NW). The rheological properties, cement hydration, mechanical properties, and microstructure were evaluated. The results showed that NWs incorporation statistically increased the yield stress of cement paste (by up to 10%) while it led to marginal effects in viscosity. NWs enhanced the early cement hydration, increasing the main heat flow peak. NWs incorporation increased the compressive strength, tensile strength, and thermal conductivity of composites by up to 56%, 66%, and 80%, respectively, while it did not statistically affect the water absorption. Scanning electron microscopy showed a good bond between NWs and cement matrix in addition to the bridging of cracks. Overall, the thermal treatment increased the specific surface area of NWs enhancing their effects on cement properties, while SP improved the NWs dispersion, increasing their beneficial effects on the hardened properties.
1 August 2018 in Revista IBRACON de Estruturas e Materiais
Quarries have invested in equipment to increase production and improve the quality of their products, such as vertical shaft impact crushers (VSI). This type of crusher works with autogenous comminution of the material to improve the shape of the coarse aggregates. However, there are few studies about the influence of crushers in the shape of fine aggregate grains. In this context, gneiss and granite fine crushed aggregates, produced in cone crushers and VSI were studied. Parameters such as coefficient of volumetric shape, aspect ratio, and circularity were used to compare these aggregates with the river sand. The results showed that there is a difference between the shape of the sand river and the fine crushed aggregates. Among the crushed aggregates, those from the VSI showed improvements in grain shape, compared to aggregates from cone crushers. However, this improvement decreases with the reduction of grain size. Mortars produced with the studied aggregates were also evaluated. It was verified their influence on the consistency, the air content and compressive strength at 28 days. For the study in the mortar, the crushed aggregates were separated in fractions by sieving and composed to obtain the same granulometric distribution for all the aggregates. The mortars made with the crushing aggregates from the VSI showed higher fluidity, lower air content and higher compressive strength when compared to the crushed aggregates produced in the cone crusher.