The paper presents the results of studies on the effects of heat treatment and cold-work parameters on the mechanical properties and microstructure of the tungsten heavy alloy (WHA) with the composition W91-6Ni-3Co. Tungsten heavy alloy (WHA) is used in conditions where strength, high density, and weight are required. The material for testing as rod-shaped samples was produced by the method of powder metallurgy and sintering with the participation of the liquid phase and then subjected to heat treatment and cold swaging. The study compares the effect of degree deformation on the strength, hardness, microhardness, and microstructure of WHA rods. The conducted tests showed that heat treatment and cold-work allowed to gradually increase the strength parameters, i.e., tensile strength , yield strength , elongation ε, hardness, and microhardness. These processes made it possible to increase the tensile strength by over 800 MPa (from the initial 600 MPa after sintering to the final value of over 1470 MPa after heat treatment with cold swaging deformation with reduction of 30%) and the hardness from 32 to 46 HRC.
This study shows the results of Ni replacement with Co in a W-Ni-Co-type tungsten heavy alloy (WHA) in terms of the structure and mechanical properties. Five alloys containing 92 wt. % of tungsten plus Ni and Co changing in the proportions (Co:Ni) of 1:9, 2:8, 3:7, 4:6, and 5:5 were prepared using liquid phase sintering (LPS). The specimens were studied directly after sintering and after solution heat treatment. The tensile strength, yield strength, and elongation were evaluated. The results of tensile tests were supplemented with microhardness measurements of tungsten grains and matrix. Light microscopy was used for the microstructure, and a scanning electron microscope (SEM) equipped with an EDS attachment was applied for the assessment of the fracture mode and chemical microanalysis. It was concluded that the replacement of Ni with Co led to a tensile property increase that was accompanied by a gradual decrease in elongation that started to be critical for a Co:Ni ratio higher than 4:6.
Experimental and finite element studies of the rotary friction welding (RFW) process of tungsten heavy alloy (THA) with aluminium alloy 5XXX series are presented. A 2.5D torsion simulation model including the circumferential effects was developed in this study. The temperature distributions, effective stress, flash dimensions and axial shortening were calculated on un-rotated friction welding aluminium parts. The peak temperatures were measured both in the axis and at the half-radius of the specimen. The maximum interface temperature of 581 °C for the friction weld was below the melting temperature of the aluminium alloy. The experimental and numerical results of the temperature and final weld geometries show good agreement between them. The results indicate very small deviations of 4.45%, 2.96%, and 2.34% on the flash width, flash height and axial shortening of friction welds.
The results of structure and mechanical property investigations of tungsten heavy alloy (THA) with small additions of rhenium powder are presented. The material for the study was prepared using liquid phase sintering (LPS) of mixed and compacted powders in a hydrogen atmosphere. From the specimens, the samples for mechanical testing and structure investigations were prepared. It follows from the results of the microstructure observations and mechanical studies, that the addition of rhenium led to tungsten grain size decreasing and influencing the mechanical properties of W-Ni-Fe-Co base heavy alloy.
1 June 2020 in Advances in Science and Technology Research Journal
Main factors in Electro Discharge Machining (EDM) are material removal rate and the relative electrode-tool wear. Material removal rate and the relative electrode-tool wear depends on many parameters in particular parameter of electrical discharge and properties of electrode materials. The...
11 July 2023 in Continuum Mechanics and Thermodynamics
Depleted uranium (DU) and tungsten heavy alloys (WHA) are commonly used as kinetic energy projectiles penetrators due to their excellent properties such as remarkably high density and strength which significantly affect their armor penetration capabilities. This article presents the results of laboratory and field tests of the new WHA sinter which summarize the results of a development project intended to increase the strength of the above-mentioned sinters used in the production of kinetic ammunition. The alloy with the composition W91–6Ni–3Co was used for the tests. The obtained alloy was subjected to cold swaging deformation with reduction of 25%. The parameters of individual technological processes were determined based on previous research. These studies concerned the impact of the degree of cold swaging deformation on the mechanical properties of the 91W–6Ni–3Co alloy. The above-mentioned work presents the results of UTS test, Charpy impact strength measurement, hardness and microhardness measurement, and the results of WHA microscopic observations in two states: after heat treatment and the final state after cold swaging deformation with reduction of: 25%. The next purpose of the research was to check the strength and functioning of the new WHA rods used in 120 mm sub-caliber projectiles. This examination was crucial for the completion of this research project, and its results enabled a synthesis of laboratory results and experimental tests.