The technological mineralogical characteristics of cesium-containing minerals in tailings were examined by means of chemical analysis, the energy spectrum analysis method, and MLA (mineral liberation analyzer) to determine the element content, phase analysis, associated mineral components, degree of liberation, particle size, etc. The results showed that the samples mainly contained spodumene, quartz, feldspar, mica, and other minerals. Pollucite was the main cesium-containing mineral in the sample, which had a cesium oxide content that was as high as 34.58%. The mineral content of pollucite in the sample was relatively low—only 1.23%. The pollucite monomer content and the amount of rich intergrowth was 85.25%, and the metal distribution of cesium in the +0.074 mm sample was as high as 87.06%. Spodumene was the main mineral associated with pollucite. The beneficiation evaluation of this tailing sample was conducted using a combined process that integrated desliming, magnetic separation, and froth flotation, and a pollucite concentrate containing 4.45% Cs2O was obtained with a 63.71 recovery rate. This indicates that little pollucite was removed by means of desliming and magnetic separation before froth flotation recovery, but during the froth flotation stage in spodumene and feldspar, a large pollucite loss was observed. Therefore, to improve pollucite recovery, a pollucite-specific adsorption reagent should be synthesized.
Thallium (Tl) is an extremely toxic rare metal to the eco-environment. Trace thallium impurity in ammonium perrhenate is harmful to the high-temperature mechanical properties of rhenium metal used for aeroengine single crystal blade. The di(2-ethylhexyl) phosphoric acid (P204) extraction to remove thallium in ammonium perrhenate solution without additive was innovatively proposed. The migration behavior of trace thallium with the concentration of P204, saponification degree and organic/aqueous phase (O/A) ratio, distribution law of thallium in the extraction system of P204, and mechanism of thallium removal were revealed. It was found Tl removal was rapidly increased to 98.5%, at conditions of P204 0.75 mol/L saponified 70% by ammonia, Tl 3.27 mg/L, O/A 1:1, T 298.15 ± 2 K, 250 rpm, and 3 min. McCabe-Thiele Tl extraction equilibrium isotherms indicates Tl concentration of raffinate less than 18.7 μg/L, a theoretical extraction of two stages and a theoretical stripping of two stages are required when both O/A work lines were at 1.0. Therefore, the method of the P204 solvent extraction system can effectively extract Tl in the forms of TlA(org), TlA3(org), TlOHA2(org), and Tl(OH)2A(org). Meanwhile, the new approach can be a promising process for ammonium rhenate refining.
Exploring efficient methods to enhance leaching efficiency is critical for bioleaching technology to deal with sulfide concentrate. In our study, a novel artificial microbial community was established to augment the bioleaching efficiency and recovery of copper (Cu) and zinc (Zn). The optimum parameters in bioleaching experiments were explored according to compare a series of conditions from gradient experiments: the pH value was 1.2, temperature was 45 °C, and rotation speed was 160 r/min, which were different with pure microorganism growth conditions. Under optimal conditions, the result of recovery for Cu and Zn indicated that the average leaching rate reached to 80% and 100% respectively, which almost increased 1.8 times and 1.2 times more than control (aseptic condition) group. Therefore, this method of Cu and Zn recovery using a new-type artificial microbial community is expected to be an environmentally-friendly and efficient bioleaching technology solution, which has the potential of large-field engineering application in the future.