The technological mineralogical characteristics of cesium-containing minerals in tailings were examined by means of chemical analysis, the energy spectrum analysis method, and MLA (mineral liberation analyzer) to determine the element content, phase analysis, associated mineral components, degree of liberation, particle size, etc. The results showed that the samples mainly contained spodumene, quartz, feldspar, mica, and other minerals. Pollucite was the main cesium-containing mineral in the sample, which had a cesium oxide content that was as high as 34.58%. The mineral content of pollucite in the sample was relatively low—only 1.23%. The pollucite monomer content and the amount of rich intergrowth was 85.25%, and the metal distribution of cesium in the +0.074 mm sample was as high as 87.06%. Spodumene was the main mineral associated with pollucite. The beneficiation evaluation of this tailing sample was conducted using a combined process that integrated desliming, magnetic separation, and froth flotation, and a pollucite concentrate containing 4.45% Cs2O was obtained with a 63.71 recovery rate. This indicates that little pollucite was removed by means of desliming and magnetic separation before froth flotation recovery, but during the froth flotation stage in spodumene and feldspar, a large pollucite loss was observed. Therefore, to improve pollucite recovery, a pollucite-specific adsorption reagent should be synthesized.
In this work, bio-hydrometallurgy technology was employed and a novel two-stage method based on successive chemical and bio treatments was proposed to collaboratively utilize manganese–silver ore and silver-bearing pyrite. In the optimization research of the chemical leaching stage, the sensitive factors for the Mn leaching efficiency were screened by Plackett–Burman design, and central compound design was performed to settle the optimized parameters. A mixed strain of bacteria containing Sulfobacillus thermosulfidooxidans, At. caldus and Leptospirillum ferrooxidans was applied in the bioleaching stage. A conventional cyanidation process carried out with the Mn leaching residuals suggested an efficient recovery of Ag. Applying a two-stage method with the optimum conditions, the leaching efficiency of 95.3% (Mn) and 96.3% (Ag) were obtained with 284.94 kg/t silver-bearing pyrite addition and 277.44 kg/t sulfuric acid consumption with a temperature at 77.73 °C and stirring speed at 287.76 rpm. Mineral behaviors were investigated with XRD and SEM/EDS analysis, and it was revealed that the oxidation of sulfur is the crux in reducing the usage of reagents, and the presence of leaching bacteria enhanced the oxidation efficiently. Through optimization and mechanism study, this paper provides an opportunity to co-leach the manganese–silver ore and silver-bearing pyrite process in a more economical and environmental way.
Metal sulfides in waste rocks and tailings are susceptible to serious soil and water contamination due to the generation of acid mine drainage (AMD) during stockpiling. The hydrometallurgical process is one of the most essential heavy metal remediation technologies through harmless disposal and resource utilization of the waste sulfides. However, atmospheric hydrometallurgy of sulfides still faces great challenges due to low leaching efficiency and high cost. In this work, we proposed a cooperative leaching system (Fe2(SO4)3-O3) and investigated the oxidative dissolution process of sphalerite (ZnS). Under the optimal conditions, the extracted zinc reached 97.8%. Reactive oxygen species (ROS) (·OH, 1O2 and ·O2−) were identified in the radical quenching experiments. The dissolution of sphalerite did not show passivation due to the ozone’s capability to oxidize the sulfur in sphalerite to sulfate. In addition, stirring rate, O3 inlet concentration, and Fe2(SO4)3 concentration had a significant effect on the dissolution of sphalerite. Meanwhile, the apparent activation energy was 24.11 kJ/mol based on kinetic fitting, which indicated that the controlling step of the reaction was mainly a diffusion process. This work demonstrated the cooperative effect of sphalerite leaching in the O3-Fe2(SO4)3 system and provided a theoretical reference for efficient and atmospheric dissolution of sphalerite.