Thin copper selenide films were synthesized on polyamide sheets using the successive ionic layer adsorption and reaction (SILAR) method at three different temperatures. It was found that elevating the temperature of the solution led to the creation of copper selenide films with different features. X-ray diffraction characterization revealed that all films crystallized into a cubic Cu2−xSe, but with different crystallinity parameters. With elevating the temperature, grain size increased (6.61–14.33 and 15.81 for 40, 60 and 80 °C, respectively), while dislocation density and the strain decreased. Surface topology was investigated with Scanning Electron Microscopy and Atomic Force Microscopy, which revealed that the grains combined into agglomerates of up to 100 nm (80 °C) to 1 μm (40 °C). The value of the direct band gap of the copper selenide thin films, obtained with UV/VIS spectroscopy, varied in the range of 2.28–1.98 eV. The formation of Cu2−xSe was confirmed by Raman analysis; the most prominent Raman peak is located at 260 cm−1, which is attributed to binary copper selenides. The thin Cu2−xSe films deposited on polyamide showed p-type conductivity, and the electrical resistivity varied in the range of 20–50 Ω. Our results suggest that elevated temperatures prevent large agglomeration, leading to higher resistance behavior.
30 December 2024 in Materials Chemistry and Physics
Advances in additive manufacturing have accelerated the development of 3D-printed dental resin composites. These materials contain a higher proportion of organic matrix and less filler than light-cured representatives, which may affect their behavior in the oral environment. This study aimed to evaluate the biological and chemical properties of 3D-printed dental resin composites before and after artificial aging, and to compare them with the light-cured representative. Specimens from a light-cured composite (Omnichroma—OMCR) and two 3D-printed composites (GT Temp PRINT—GTPR; SprintRay CROWN—SPRY) were subjected to aging treatments: unaged (T0) or thermocycled for 5000 (T1) and 10,000 cycles (T2). Biological evaluation was performed using MTT assay and Live/Dead cell fluorescence microscopy using human gingival fibroblasts, whereas Raman spectroscopy analysed materials’ structural changes. Materials exhibited good biocompatibility (>70% cell viability), with OMCR displaying greater variability. OMCR was more susceptible to chemical degradation under thermal stresses than both 3D-printed materials. Tested 3D-printed composites can provide comparable or even superior biological and chemical properties compared to light-cured representative, likely due to optimized resin formulations and post-curing protocols that improve polymer network organization and reduce residual monomer release. These findings support the potential of tested 3D-printed composites for manufacturing dental restorations.