This paper compares, the mechanical properties of welded joints 6061 T6 and 5083 O aluminium alloys obtained using friction stir welding (FSW) at four rotation speeds namely 450,560,710 and 900 rpm and that by conventional fusion welding. FSW welds were carried out on a milling machine. The performance of FSW and Fusion welded joints were identified using tensile test, hardness test and microstructure. The properties of FSW and fusion welded processes were also compared with each other to understand the advantages and disadvantages of these processes for welding applications for Al alloys. It was seen that the tensile strength obtained with FSW was higher as compared to conventional fusion welding process. The width of the heat affected zone of FSW was narrower than Fusion welded joints. The results showed that FSW improved the mechanical properties of welded joints.
1 December 2015 in Bulletin Of The Polish Academy Of Sciences-Technical Sciences
A methodology was exhibited to create the experimental model for assessing the Ultimate Tensile Strength of AA 5083-O aluminum compound which is broadly utilized as a part of boat building industry by Friction Stir Welding (FSW). FSW process parameters, such as: tool rotational speed, welding speed, and axial force were optimized for better results. FSW was completed considering three-component 3-level Box Behnekn Design. Response surface Methodology (RSM) was implemented to obtain the relationship between the FSW process parameters and ultimate Tensile Strength. Analysis of Variance (ANOVA) procedure was utilized to check the aptness of the created model. The FSW process parameters were additionally streamlined utilizing Response Surface Methodology (RSM) to augment tensile strength. The joint welded at a rotational speed of 1100 rpm, a welding speed of 75 mm/min and a pivotal energy of 2.5 t displays higher tensile strength compared with different joints in comparison with other joints.
Surface composites are viable choices for various applications in the aerospace and automotive industries. Friction Stir Processing (FSP) is a promising method for fabricating surface composites. Aluminum Hybrid Surface Composites (AHSC) are fabricated using the FSP to strengthen a hybrid mixture prepared with equal parts of Boron carbide (B4C), Silicon Carbide (SiC), and Calcium Carbonate (CaCO3) particles. Different hybrid reinforcement weight percentages (reinforcement content of 5% (T1), 10% (T2), and 15% (T3)) were used in fabricating AHSC samples. Furthermore, different mechanical tests were performed on hybrid surface composite samples with different weight percentages of the reinforcements. Dry sliding wear assessments were performed in standard pin-on-disc apparatus as per ASTM G99 guidelines to estimate wear rates. The presence of reinforcement contents and dislocation behavior was investigated using Scanning Electron Microscopy (SEM) and Transmission Electron Microscopy (TEM) studies. The results indicated that the Ultimate Tensile Strength (UTS) of sample T3 exhibited 62.63% and 15.17% higher than that of samples T1 and T2, respectively, while the Elongation (%) of T3 exhibited 38.46% and 15.38% lower than that of samples T1 and T2, respectively. Moreover, it was found that the hardness of sample T3 increased in the stir zone compared to samples T1 and T2, owing to its higher brittle response. The higher brittle response of sample T3 compared to samples T1 and T2 was confirmed by the higher value of Young’s modulus and the lower value of Elongation (%).
15 February 2023 in Materialwissenschaft und Werkstofftechnik
The present work is focused on synthesizing Copper/Silicon Nitride (Si 3 N 4) Nano Surface Composite (NSC) by friction stir processing. All the four copper plates had a groove width of 0.6, 0.9, and 1.2 respectively. A dual-pass FSP was carried out, the rotational speed of the tool is 1400 rpm, an axial force of 10 k N, and a traverse speed of 15 mm min −1 . The microstructure and the distribution of silicon nitride nanoparticles were studied using a field emission scanning electron microscope (FESEM). The results indicate that the tensile strength of Cu/Si 3 N 4 NSC increased and they exhibit superior micro hardness, corrosion resistance, and wear resistance compared to pure copper.
The present work aims to evaluate the effects of varying the volume fraction of natural fibers reinforced in PLA on the mechanical properties of the resulting composites. The study involved preparing composite filaments by blending polylactic acid (PLA) with different percentages of pineapple and banana fiber particles, followed by 3D printing test samples using a Fused Deposition Modeling (FDM) printer. The results showed that increasing the volume fraction of Banana fibers up to 2% increased the compressive strength by 27.97% and flexural strength by 3.95% of the composite while decreasing its tensile strength by 5.6% compared to the plain PLA. With potential uses in the automotive, aerospace, and biomedical sectors, this study emphasizes the potential of pineapple and banana fiber powder as economical, sustainable reinforcements in 3D printed composites.