In this study, TiC particle-reinforced Cu-based composites were prepared by powder metallurgy and spark plasma sintering (SPS) techniques. The mechanical and electrical properties of TiC/Cu composites were analyzed in conjunction with micro-morphology. The results showed that: TiC was fully diffused in the Cu matrix at a sintering temperature of 900 °C. The micron-sized TiC particles were most uniformly distributed in the Cu matrix and had the best performance. At this time, the densification of 5 wt.% TiC/Cu composites reached 97.19%, and the conductivity, hardness, and compressive yield strength were 11.47 MS·m−1, 112.9 HV, and 162 MPa, respectively. The effect of TiC content on the overall properties of the composites was investigated at a sintering temperature of 900 °C. The TiC content of the composites was also found to have a significant influence on the overall properties of the composites. The best performance of the composites was obtained when the TiC mass fraction was 10%. The average values of density, hardness, yield strength and conductivity of the 10 wt.% TiC/Cu composites were 90.07%, 128.3 HV, 272 MPa and 9.98 MS·m−1, respectively. The yield strength was 272 MPa, and the compressive strain was 38.8%. With the increase in TiC content, although the yield strength increased, the brittleness increased due to more weak interfaces in the composites.
23 October 2022 in Journal of Alloys and Compounds
Design of interface-controllable magnetic composite towards the wideband microwave absorber is greatly significance, however, it still remains challenging. Herein, we designed a spherical-like hybrids, using the Co3O4 and amorphous carbon as the core and shell, respectively. Then, the existed Co3O4 core could be totally reduced by the carbon shell, thus in CoxOy core (composed by Co and Co3O4). Of particular note, the ratios of Co and Co3O4 can be linearly tuned, suggesting the controlled interfaces, which greatly influences the interface loss behavior and electromagnetic absorption performance. The results revealed that the minimum reflection loss value (RLmin) of −39.4 dB could be achieved for the optimal CoxOy@C sample under a thin thickness of 1.4 mm. More importantly, the frequency region with RL < −10 dB was estimated to be 4.3 GHz, ranging from 13.7 to 18.0 GHz. The superior wideband microwave absorption performance was primarily attributed to the multiple interfacial polarization and matched impedance matching ability.
Among the various reinforcement phases available in Cu-based composites, the unique layered structure and easy diffusion of A-layer atoms make MAX phases more suitable for reinforcing a copper matrix than others. In this study, Cu-coated Ti3AlC2 particles (Cu@Ti3AlC2) were prepared through electroless plating, and Cu@Ti3AlC2/Cu composites were fabricated via vacuum hot-press sintering. The phase composition and microstructure of both Cu@Ti3AlC2 powder and composites were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results demonstrate the creation of successful electroless copper plating to obtain a Cu coating on Ti3AlC2 particles. At 850 °C, a small amount of Ti3AlC2 particles decompose to form TiCx, while Al atoms from the A layer of MAX phase diffuse into the Cu matrix to form a solid solution with Cu(Al). The test results reveal that the density of the Cu@Ti3AlC2/Cu composite reaches 98.5%, with a maximum compressive strength of 705 MPa, which is 8.29% higher than that of the Ti3AlC2/Cu composite. Additionally, the compressive strain reaches 37.6%, representing an increase of 12.24% compared to that exhibited by the Ti3AlC2/Cu composite.
Copper matrix composites (CMCs) synergistically reinforced with rare earth oxides (Re2O3) and TiC were prepared using a powder metallurgy process with vacuum hot-pressing and sintering technology, aiming to explore new ways to optimize the properties of composites. Through this innovative approach, we propose a new solution strategy and idea for the difficult problem of mutual constraints between electrical and mechanical properties faced by traditional dual-phase reinforced Cu-matrix composites. Meanwhile, the modulation mechanism of Re2O3 in CMCs and the electrical and mechanical properties of the composites were investigated. The compressive yield strength was improved from pure Cu (50 MPa) to TiC/Cu (159 MPa). The yield strength of Eu2O3-TiC/Cu obtained after biphasic strengthening is 213 MPa, which is 326% higher than that of pure Cu, and the ultimate compressive strength reaches 790 MPa. The conductivity was enhanced from TiC/Cu (81.4% IACS) to La2O3-TiC/Cu (87.3% IACS).
Magnetic carbon-based composites have been attractive candidates for electromagnetic (EM) absorption due to their dual magnetic and dielectric loss ability.