In this study, TiC particle-reinforced Cu-based composites were prepared by powder metallurgy and spark plasma sintering (SPS) techniques. The mechanical and electrical properties of TiC/Cu composites were analyzed in conjunction with micro-morphology. The results showed that: TiC was fully diffused in the Cu matrix at a sintering temperature of 900 °C. The micron-sized TiC particles were most uniformly distributed in the Cu matrix and had the best performance. At this time, the densification of 5 wt.% TiC/Cu composites reached 97.19%, and the conductivity, hardness, and compressive yield strength were 11.47 MS·m−1, 112.9 HV, and 162 MPa, respectively. The effect of TiC content on the overall properties of the composites was investigated at a sintering temperature of 900 °C. The TiC content of the composites was also found to have a significant influence on the overall properties of the composites. The best performance of the composites was obtained when the TiC mass fraction was 10%. The average values of density, hardness, yield strength and conductivity of the 10 wt.% TiC/Cu composites were 90.07%, 128.3 HV, 272 MPa and 9.98 MS·m−1, respectively. The yield strength was 272 MPa, and the compressive strain was 38.8%. With the increase in TiC content, although the yield strength increased, the brittleness increased due to more weak interfaces in the composites.
Among the various reinforcement phases available in Cu-based composites, the unique layered structure and easy diffusion of A-layer atoms make MAX phases more suitable for reinforcing a copper matrix than others. In this study, Cu-coated Ti3AlC2 particles (Cu@Ti3AlC2) were prepared through electroless plating, and Cu@Ti3AlC2/Cu composites were fabricated via vacuum hot-press sintering. The phase composition and microstructure of both Cu@Ti3AlC2 powder and composites were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results demonstrate the creation of successful electroless copper plating to obtain a Cu coating on Ti3AlC2 particles. At 850 °C, a small amount of Ti3AlC2 particles decompose to form TiCx, while Al atoms from the A layer of MAX phase diffuse into the Cu matrix to form a solid solution with Cu(Al). The test results reveal that the density of the Cu@Ti3AlC2/Cu composite reaches 98.5%, with a maximum compressive strength of 705 MPa, which is 8.29% higher than that of the Ti3AlC2/Cu composite. Additionally, the compressive strain reaches 37.6%, representing an increase of 12.24% compared to that exhibited by the Ti3AlC2/Cu composite.
Composite photocatalyst materials have potential application value in the field of environmental protection, especially in the degradation of water pollutants. In this paper, Ag-BiOI composite photocatalyst materials were prepared by deposition method on BiOI flower-like microspheres prepared by microwave solvothermal method. BiOI flower balls are stacked by interlaced nanosheets, and Ag nanoparticles are attached to the surface of BiOI microspheres. This paper explores the effect of Ag loading on the photocatalytic performance of composite materials through variable control. The research results show that as the Ag content increases, the degradation rate of RhodamineB (RhB) and Ciprofloxacin (CIP) of the sample under visible light irradiation increases. The 4% Ag/BiOI composite photocatalyst exhibits the best degradation performance for Rhodamine B solution (RhB, 20 mg/L) and Ciprofloxacin solution (CIP, 10 mg/L), achieving degradation rates of 80.4% and 80.0%, respectively, which is five times higher than that of BiOI before loading. This significantly improves the treatment efficiency of organic pollutants.In addition, excessive Ag particle compounding will reduce the light absorption performance of the sample, thereby reducing the catalytic degradation characteristics of the material. Furthermore, the recyclability of the 4% Ag-BiOI composite was evaluated, and it was found that after five cycles of use, the photocatalytic activity remained stable, indicating excellent reusability of the material. Finally, this article discusses the catalytic degradation mechanism of Ag composite catalyst materials based on experimental results, and provides a design strategy for loading heavy metals to improve the catalytic performance of materials.
Copper matrix composites (CMCs) synergistically reinforced with rare earth oxides (Re2O3) and TiC were prepared using a powder metallurgy process with vacuum hot-pressing and sintering technology, aiming to explore new ways to optimize the properties of composites. Through this innovative approach, we propose a new solution strategy and idea for the difficult problem of mutual constraints between electrical and mechanical properties faced by traditional dual-phase reinforced Cu-matrix composites. Meanwhile, the modulation mechanism of Re2O3 in CMCs and the electrical and mechanical properties of the composites were investigated. The compressive yield strength was improved from pure Cu (50 MPa) to TiC/Cu (159 MPa). The yield strength of Eu2O3-TiC/Cu obtained after biphasic strengthening is 213 MPa, which is 326% higher than that of pure Cu, and the ultimate compressive strength reaches 790 MPa. The conductivity was enhanced from TiC/Cu (81.4% IACS) to La2O3-TiC/Cu (87.3% IACS).
In this paper, Cu-based composites were prepared by the powder metallurgy method with the spark plasma sintering (SPS) sintering technique using WC (tungsten carbide) particles as the reinforcing phase and Cu as the matrix. The effect of sintering temperature on the electrical and mechanical properties of the composites was investigated, and the effect of the variation in the reinforcing phase content on the electrical and mechanical properties of the composites was investigated at the optimum sintering temperature. The microstructure and properties of 5 wt. % WC/Cu composites at different sintering temperatures were investigated, and 850 °C was determined as the optimum sintering temperature. When the SPS temperature was 850 °C, the yield strength, compressive strength, compressive strain, and hardness of 10 wt. % WC/Cu composites were 321 MPa, 743 MPa, 40.42%, and 143.2 HV, respectively, which increased the yield strength and compressive strength by 697.82% and 246.84%, respectively, compared with pure Cu material.