In this study, TiC particle-reinforced Cu-based composites were prepared by powder metallurgy and spark plasma sintering (SPS) techniques. The mechanical and electrical properties of TiC/Cu composites were analyzed in conjunction with micro-morphology. The results showed that: TiC was fully diffused in the Cu matrix at a sintering temperature of 900 °C. The micron-sized TiC particles were most uniformly distributed in the Cu matrix and had the best performance. At this time, the densification of 5 wt.% TiC/Cu composites reached 97.19%, and the conductivity, hardness, and compressive yield strength were 11.47 MS·m−1, 112.9 HV, and 162 MPa, respectively. The effect of TiC content on the overall properties of the composites was investigated at a sintering temperature of 900 °C. The TiC content of the composites was also found to have a significant influence on the overall properties of the composites. The best performance of the composites was obtained when the TiC mass fraction was 10%. The average values of density, hardness, yield strength and conductivity of the 10 wt.% TiC/Cu composites were 90.07%, 128.3 HV, 272 MPa and 9.98 MS·m−1, respectively. The yield strength was 272 MPa, and the compressive strain was 38.8%. With the increase in TiC content, although the yield strength increased, the brittleness increased due to more weak interfaces in the composites.
Copper matrix composites (CMCs) synergistically reinforced with rare earth oxides (Re2O3) and TiC were prepared using a powder metallurgy process with vacuum hot-pressing and sintering technology, aiming to explore new ways to optimize the properties of composites. Through this innovative approach, we propose a new solution strategy and idea for the difficult problem of mutual constraints between electrical and mechanical properties faced by traditional dual-phase reinforced Cu-matrix composites. Meanwhile, the modulation mechanism of Re2O3 in CMCs and the electrical and mechanical properties of the composites were investigated. The compressive yield strength was improved from pure Cu (50 MPa) to TiC/Cu (159 MPa). The yield strength of Eu2O3-TiC/Cu obtained after biphasic strengthening is 213 MPa, which is 326% higher than that of pure Cu, and the ultimate compressive strength reaches 790 MPa. The conductivity was enhanced from TiC/Cu (81.4% IACS) to La2O3-TiC/Cu (87.3% IACS).
In situ graphene was grown on the surface of copper particles using highland barley powder, which is rich in sucrose and β-glucan, as a carbon source. The graphene content in the graphene-coated copper (Gr@Cu) composite powder was 4.98 wt.%. A characteristic angle of approximately 14° was observed between the graphene and copper crystal planes, indicating strong interfacial bonding. Raman spectroscopy revealed an ID/IG ratio of 0.96 for the graphene. Owing to the in situ growth of graphene, the mechanical properties of the copper matrix are effectively strengthened. At a graphene content of 0.7 wt.%, the graphene was uniformly dispersed within the copper matrix, resulting in optimized mechanical properties of the composite. This composite exhibited a conductivity of 70% IACS and a compressive yield strength of 175 MPa.