Denghui Li

Mr. Denghui Li

orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 January 2025 in International Journal of Mechanical Sciences
Verified
Journal Article
Closed access
YLYuhan Li
Yuhan Li
YXYintian Xing
Yintian Xing
LSLinhe Sun
Linhe Sun
DLDenghui Li
Denghui Li
TYTengfei Yin
Tengfei Yin
Suet ToSuet To
Suet To

17 April 2024 in Inorganics
Verified
Journal Article
Open access
PDF file
ZZZhenjie Zhai
Zhenjie Zhai
HDHaitao Dong
Haitao Dong
DLDenghui Li
Denghui Li
ZWZhe Wang
Zhe Wang
CSChangfei Sun
Changfei Sun
CCCong Chen
Cong Chen
In this study, TiC particle-reinforced Cu-based composites were prepared by powder metallurgy and spark plasma sintering (SPS) techniques. The mechanical and electrical properties of TiC/Cu composites were analyzed in conjunction with micro-morphology. The results showed that: TiC was fully diffused in the Cu matrix at a sintering temperature of 900 °C. The micron-sized TiC particles were most uniformly distributed in the Cu matrix and had the best performance. At this time, the densification of 5 wt.% TiC/Cu composites reached 97.19%, and the conductivity, hardness, and compressive yield strength were 11.47 MS·m−1, 112.9 HV, and 162 MPa, respectively. The effect of TiC content on the overall properties of the composites was investigated at a sintering temperature of 900 °C. The TiC content of the composites was also found to have a significant influence on the overall properties of the composites. The best performance of the composites was obtained when the TiC mass fraction was 10%. The average values of density, hardness, yield strength and conductivity of the 10 wt.% TiC/Cu composites were 90.07%, 128.3 HV, 272 MPa and 9.98 MS·m−1, respectively. The yield strength was 272 MPa, and the compressive strain was 38.8%. With the increase in TiC content, although the yield strength increased, the brittleness increased due to more weak interfaces in the composites.

24 February 2024 in Nanomaterials
Verified
Journal Article
Open access
PDF file
CCCong Chen
Cong Chen
ZZZhenjie Zhai
Zhenjie Zhai
CSChangfei Sun
Changfei Sun
ZWZhe Wang
Zhe Wang
DLDenghui Li
Denghui Li
Among the various reinforcement phases available in Cu-based composites, the unique layered structure and easy diffusion of A-layer atoms make MAX phases more suitable for reinforcing a copper matrix than others. In this study, Cu-coated Ti3AlC2 particles (Cu@Ti3AlC2) were prepared through electroless plating, and Cu@Ti3AlC2/Cu composites were fabricated via vacuum hot-press sintering. The phase composition and microstructure of both Cu@Ti3AlC2 powder and composites were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results demonstrate the creation of successful electroless copper plating to obtain a Cu coating on Ti3AlC2 particles. At 850 °C, a small amount of Ti3AlC2 particles decompose to form TiCx, while Al atoms from the A layer of MAX phase diffuse into the Cu matrix to form a solid solution with Cu(Al). The test results reveal that the density of the Cu@Ti3AlC2/Cu composite reaches 98.5%, with a maximum compressive strength of 705 MPa, which is 8.29% higher than that of the Ti3AlC2/Cu composite. Additionally, the compressive strain reaches 37.6%, representing an increase of 12.24% compared to that exhibited by the Ti3AlC2/Cu composite.

9 January 2025 in Nanomaterials
Verified
Journal Article
Open access
PDF file
DLDenghui Li
Denghui Li
CSChangfei Sun
Changfei Sun
ZZZhenjie Zhai
Zhenjie Zhai
ZWZhe Wang
Zhe Wang
CCCong Chen
Cong Chen
Q雷QIAN 前 LEI 雷
QIAN 前 LEI 雷
Copper matrix composites (CMCs) synergistically reinforced with rare earth oxides (Re2O3) and TiC were prepared using a powder metallurgy process with vacuum hot-pressing and sintering technology, aiming to explore new ways to optimize the properties of composites. Through this innovative approach, we propose a new solution strategy and idea for the difficult problem of mutual constraints between electrical and mechanical properties faced by traditional dual-phase reinforced Cu-matrix composites. Meanwhile, the modulation mechanism of Re2O3 in CMCs and the electrical and mechanical properties of the composites were investigated. The compressive yield strength was improved from pure Cu (50 MPa) to TiC/Cu (159 MPa). The yield strength of Eu2O3-TiC/Cu obtained after biphasic strengthening is 213 MPa, which is 326% higher than that of pure Cu, and the ultimate compressive strength reaches 790 MPa. The conductivity was enhanced from TiC/Cu (81.4% IACS) to La2O3-TiC/Cu (87.3% IACS).

9 May 2022 in Nanomaterials
Verified
Journal Article
Open access
PDF file
CCCong Chen
Cong Chen
HDHaitao Dong
Haitao Dong
JWJiayuan Wang
Jiayuan Wang
WCWen Chen
Wen Chen
DLDenghui Li
Denghui Li
KZKun Zhou
Kun Zhou
The magnetic nanochain-like material has been regards as one of the most promising electromagnetic (EM) absorbing material but remains a challenging. Herein, magnetic chain-like ferrite (included Fe3O4, CoFe2O4 and NiFe2O4) are successfully produced through a general solvothermal method, using PVP as the structural-liking agent. Experimental results confirm the ultimate sample possess a 3-dimensional chain-like structure which are constructed by numerous ferrite’s nanoparticles with ~60 nm in diameter. Their electromagnetic parameters can be also manipulated by such a chain structure, especially the dielectric loss, where a sharply increases can be observed on within a lower filling ratio. It greatly benefits to the EM absorbing property. In this article, the electromagnetic absorption layer made with a lower content of ferrite possess the excellent electromagnetic absorption ability, where the optimized effective absorption band was nearly 6.4 GHz under a thickness of 1.8 mm. Moreover, the filling ratio is only 30 wt%. Our method for designing of chain-like magnetic material can be helpful for producing wideband electromagnetic absorption in a low filling ratio.

1 August 2023 in AIP Advances
Verified
Journal Article
Open access
PDF file
CCCong Chen
Cong Chen
DLDenghui Li
Denghui Li
ZZZhenjie Zhai
Zhenjie Zhai
CSChangfei Sun
Changfei Sun
WCWen Chen
Wen Chen
In this paper, Cu-based composites were prepared by the powder metallurgy method with the spark plasma sintering (SPS) sintering technique using WC (tungsten carbide) particles as the reinforcing phase and Cu as the matrix. The effect of sintering temperature on the electrical and mechanical properties of the composites was investigated, and the effect of the variation in the reinforcing phase content on the electrical and mechanical properties of the composites was investigated at the optimum sintering temperature. The microstructure and properties of 5 wt. % WC/Cu composites at different sintering temperatures were investigated, and 850 °C was determined as the optimum sintering temperature. When the SPS temperature was 850 °C, the yield strength, compressive strength, compressive strain, and hardness of 10 wt. % WC/Cu composites were 321 MPa, 743 MPa, 40.42%, and 143.2 HV, respectively, which increased the yield strength and compressive strength by 697.82% and 246.84%, respectively, compared with pure Cu material.