In this study, we successfully obtained Al-TiB2 composite materials using self-propagating high-temperature synthesis and preliminary mechanical activation of the initial Al-(Ti + 2B) powder mixture with a high aluminum content (70 wt.%). We investigated the possibility of controlling the structure of synthesis products, in particular, the size and shape of ceramic particles. We examined the effects of the mechanical activation of the initial powder mixture on the structure and particle size of titanium diboride in the synthesis products. We proposed a mechanism of structure formation in the synthesis products obtained by SHS using the method of preliminary mechanical activation of the initial mixture. We found that mechanical activation for 60-180 s led to the formation of isolated TiB2 particles of prolate and irregular shape. The average particle size of TiB2 in the synthesis products was 0.77 (after 60 s of mechanical activation) and 1.5 µm (after 180 s of mechanical activation), respectively. An increase in the duration of mechanical activation to 900 s led to the formation of an island (skeletal) structure, in which there were interconnected aggregates and isolated particles of titanium diboride. The average size of these particles was 4.3 µm.
This article considers issues pertinent to the research of the phase composition, structure and mechanical properties of materials obtained from powders of composite (Ni-Ti)-TiB2, which have prospective applications in aerospace and automotive industry and engine construction. The starting powder materials (Ni-Ti)-TiB2 were obtained by self-propagating high-temperature synthesis (SHS). Research samples were produced using high-temperature vacuum sintering. It was shown that the use of such materials increases the wettability of the particles and allows the production of composites, the density of which is 95% of the theoretical one. Average particle size was 1.54 µm, average microhardness was 8 GPa, which is an order of magnitude higher than the average microhardness of pure nickel-based and titanium-based alloys, and the ultimate strength values were comparable to those of tungsten-based heavy alloys.