In this study, the possibility of using adhesives of natural origin for the manufacture of wood fiber-based lightweight panels was investigated. The boards, of a density ranging from 150 to 250 kg/m3, were glued together using commercial urea–formaldehyde resin (control board), solutions of rye flour and potato starch and two types of starch: oxidized and gelatinized. The density and density profile, compressive strength, modulus of elasticity, acoustic properties and thermal conductivity were determined in the produced boards. These studies show that when food components are used as binding agents in the manufacture of lightweight wood fiberboards, the properties obtained can be comparable with those of commercial boards manufactured using synthetic agents.
The aim of this study was to determine the mechanical properties of laminated beams containing selected wood species in the tension zone using a four-point bending test. Three beam types were manufactured with respect to the timber used in the tension zone, i.e., beams containing oak or beech timber of I and II quality class and pine timber with no defects (as defects had been removed). The manufactured beams were assessed with respect to bending strength and the modulus of elasticity. The obtained results were compared with the performance of BSH (Industrial beams GL made in Germany—Brettschichtholz) industrial beams. We concluded that beams made from pine timber are an appropriate alternative to spruce beams. The static bending strength of the beams made with hardwood faces was 70% higher than that of beams made with pine wood. All types of beams manufactured in the laboratory met the requirements of at least the GL24c class.
1 August 2024 in European Journal of Wood and Wood Products
This study investigated the effect of pine particle polyesterification with the mixture of sorbitol and citric acid (SCA) on the properties of particleboard bonded with the PF/pMDI hybrid resin. The use of SCA with a concentration of 35% contributed to improvement in the internal bond of the particleboards, their water resistance and dimensional stability. However, lowering the concentration to 25% resulted in a deterioration of the properties of produced materials. The effect of different loadings of pMDI in the PF/pMDI resin (0%, 5%, 15%, 25%) was also investigated and the outcomes showed a positive effect of the share of 15% and 25%. Furthermore, boards made of treated particles were characterized by slightly better flammable properties (lower mass loss, flashing point temperature and delayed ignition), and the visibility of the effect increased with the increase in the concentration of the impregnate. The results also indicate that the introduction of pMDI may also influence the ignition of the board.
The aim of this study was to assess the static bending strength of pine glulam manufactured when obtaining the main yield, i.e., structural timber or timber to be used in the production of structural glulam. Analyses were conducted on pine timber harvested from three different locations in Poland. Two beam variants were manufactured, differing in the timber arrangement, horizontal vs. vertical. It was shown that the static bending strength of beams manufactured in the vertical timber arrangement variant is slightly higher than that of beams produced from horizontally arranged layers, with the latter beams characterised by a smaller confidence interval for this strength. Moreover, it was found that the difference in the value of the 5th percentile for both beam types is slight and both beam types are considered to exhibit a high bending strength of over 40 N/mm2.
Numerous studies have shown that the geometry of micro-joints significantly affects the strength of the so joined timber element. The bending strength increases by creating a larger bonding area by increasing the length of the wedge joint. Although this type of joint has been successfully used for many years, it can still be troublesome to make. For these reasons, the present study investigated an easy-to-fabricate wedge joint, which we folded during the beams’ formation and glued with the same adhesive as the individual lamellas. Although the research has not fully answered all the questions relevant to both scientific and technological curiosity, it indicates the great potential of this solution. Following the principle adopted in the ongoing wood optimisation work, we concluded that the beams of the target cross-section should be produced, and it should only be possible to cut them to a certain length. In this approach, we only removed defects at critical points for the beam structure and, in this way, up to 30% of the timber processed could be saved or better utilised.
This study aimed to evaluate the mechanical properties determined in a 4-point bending test of beams made of lumber from which knots had been locally removed and the resulting loss replaced with sound wood. Three sets of beams were prepared, which differed in the number of layers/lamellas and the position of the lamellas from which edge knots were removed. All the lamellas used in the tests were subjected to a modulus of elasticity assessment. In addition to the distribution of defects, it determined the position of a given piece in the beam structure. The tests showed that high mechanical properties could characterise the beams produced in this way, i.e., a modulus of elasticity close to 12 kN/mm2 and a strength above 40 N/mm2, if the lamellas without knots were located below the outer tension lamella. Significantly better results were obtained when PUR glue was used in the inserts rather than MUF. In this case, beams with an improved outer lamella in the tension zone using semi-circular inserts glued with PUR glue had an average strength of 34.6 N/mm2.