Various researchers are developing efforts to integrate waste and by-products as alternative materials in road construction and maintenance, reducing environmental impacts and promoting a circular economy. Among the alternative materials that several authors have studied regarding their use as partial or total substitutes for natural aggregates in the asphalt paving industry, the steel slag aggregate (SSA) and recycled concrete aggregate (RCA) from construction demolition waste (CDW) stand out. This paper reviews and discusses the characteristics and performance of these materials when used as aggregates in asphalt mixtures. Based on the various studies analyzed, it was possible to conclude that incorporating SSA or RCA in asphalt mixtures for road pavements has functional, mechanical, and environmental advantages. However, it is essential to consider some possible drawbacks of these aggregates that are discussed in this paper, to define the acceptable uses of SSA and RCA as sustainable feedstocks for road paving works.
Steel slag is a byproduct generated as waste during the steelmaking process and can be considered a cost-effective and environmentally acceptable alternative to replace natural aggregates. Using steel slag aggregates (SSA) to produce asphalt mixtures promotes sustainability and circular economy principles by using an industrial byproduct as a raw material. Thus, this work mainly aims to design more sustainable asphalt mixtures with high amounts of SSA that fit the circular economy expectations. This work developed two asphalt mixtures with SSA for surface (AC 14 surf) and binder/base (AC 20 bin/base) courses. Initially, the excellent wearing and polishing resistance of SSA and their good affinity with bitumen demonstrated the potential of this byproduct to be used in asphalt mixtures. Then, when analyzing the influence of using two different SSA incorporation rates (50% and a percentage close to 100%) in both asphalt mixtures, it was concluded that the use of SSA should be limited to 75% to avoid excessive air void contents and durability problems. The importance of considering the different particle densities of SSA and natural aggregates was highlighted during the mix design by defining a relationship between an effective and equivalent binder content. Finally, the mechanical performance of AC 14 and AC 20 with 75% SSA incorporation was compared to identical conventional mixtures produced with natural granite aggregates. The results obtained showed that the asphalt mixtures with 75% SSA have some workability problems due to the rough and porous surface of SSA. However, they present an excellent water sensitivity and permanent deformation resistance, surpassing the performance of the conventional asphalt mixtures.
Using aggregates from alternative sources has been considerably encouraged in recent decades. Reducing the consumption of natural aggregates from quarries (which have a substantial economic, visual, and environmental impact) is increasingly a concern. These needs have led to the broader use of more sustainable aggregates, increasing the incorporation percentages and extending their use to more demanding pavement layers (e.g., surface). In order to prove the efficiency of recycled concrete aggregates (RCAs) under such conditions, the “CirMat” project was developed. Among other works and tests, an asphalt concrete (AC) incorporating 52.3% RCA was characterized mechanically and environmentally. Empirical properties were evaluated, including the Marshall test (S = 20.2 kN; F = 2.9 mm) and resistance to permanent deformation (WTS = 0.10 mm/103 cycles), as well as a life cycle assessment (LCA), which confirmed that nine indicators were improved (from 1% to 93%). The test samples were taken from mixtures produced in the laboratory and at a plant (after which they were applied on a construction site). Comparing the results with those obtained in a reference AC (with natural aggregates), it was possible to conclude that the performance of the AC with RCAs was very similar. Therefore, the use of these aggregates, at high rates, does not represent additional risks for asphalt mixtures and has lower environmental impacts in most categories.
The protection of the environment must be a priority in our society, and the construction sector can contribute significantly to this goal. Construction, being one of the industrial sectors that is more demanding in terms of raw materials, must reinforce its effort to implement, in a more profound and systematic way, the paradigm of the circular economy. In this sense, in recent years several studies have been trying to contribute solutions aimed at reintroducing industrial by-products or residues in new products for the construction industry. It should be noted that nowadays it is increasingly important to introduce a higher percentage of recycled materials in concrete. In this context, the present work addresses the appropriateness of a design procedure proposed to maximize the content of electric arc furnace slag (EAFS) and include recycled tire steel fibers (RTSF) in the production of more sustainable structural concretes. For this, the properties of various concrete mixtures at the fresh and hardened state, obtained by the substantial substitution of coarse and fine natural aggregates by EAFS and fly ash (FA), were investigated. The design of EAFS mixtures was based on two conventional reference mixtures (REF1 and REF2), and by using the modified Andreasen and Andersen particle packing model, these were optimized to achieve maximum packing density. Compressive strength, modulus of elasticity behavior, and fresh and physical properties were assessed in order to define the best mix proportions with respect to the predefined requirements of ordinary mixtures. Untreated recycled tire steel fibers (RTSF) were included in the developed sustainable concrete to perform a comparison of the physical properties with unreinforced concretes developed with natural aggregates (REF2) and with EAFS aggregates (EAFS8D1). This incorporation was intended to improve the physical behavior of unreinforced concretes with EAFS aggregates. Mixtures with high percentages of waste aggregates up to 70% (in weight), and 10% (in weight) of FA were obtained, showing competitive mechanical behavior compared to REF1 and REF2. These concrete compositions showed minimum and maximum compressive strengths between 9 MPa and 37 MPa, respectively. This study coverd the two major classes of concrete used as structural material, namely structural concrete and fiber reinforced concrete.